Safety Speed Cut

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Gluing VS Floating Panels

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Gluing VS Floating Panels

10/21/23       
Austin Vicknair Member

What is everyones opionions on gluing vs floating mdf panels. We have been gluing 1/2 mdf panels for 5 piece doors for years and havent run into problems, but it seems most people do not.

10/21/23       #2: Gluing VS Floating Panels ...
Yavuz Member

No need to gamble either wood or painters. Lesson learned long time ago.
10/21/23       #3: Gluing VS Floating Panels ...
Yavuz Member

Custom shaper profile that leaves tiny gap for paint bridging is way to go.
Caulking works or not is a kind of gamble.
No need to gamble either wood or painters. Lesson learned long time ago.

10/22/23       #4: Gluing VS Floating Panels ...
Adam

We've been gluing mdf/plywood panels into 5 piece cabinet doors for 35 years. It makes better doors. The movement is what causes the cracking. We get zero cracking when we glue. It's really that simple. People like to argue about expansion. They do not know what they are talking about. Wood panels need to move. mdf/ply do not.

10/22/23       #5: Gluing VS Floating Panels ...
nicko

I glue my MDF panels. I have not had any problems with it.

10/22/23       #6: Gluing VS Floating Panels ...
Jesse Beaverson Member

Website: https://instagram.com/jessebeaverson

Adam, you’re talking about gluing MDF panels into MDF frames, right? Or have you been gluing MDF panels into wood frames as well? I’ve always wondered if I could do that, it would really solve some problems for me.

10/22/23       #7: Gluing VS Floating Panels ...
Adam

Jesse,

mdf or cabinet ply glued into wood stiles/rails. 35 years. The best 5 piece paint grade raised panel door would be a double refined 5/8" mdf, raise, preprimed on the raised section only. Glued into soft maple or maple stiles rails. No caulk is required. This is just with regular off the shelf Freeborn stile/rail/raised panel cutters. Only use Titebond1. You get no telegraphing or creep at the stile/rail joint. You do not need a ton of glue on the panel. Just a fine bead.

10/22/23       #8: Gluing VS Floating Panels ...
Karl E Brogger

Am I the only one left that does hardwood panels for painted cabinets?

10/24/23       #10: Gluing VS Floating Panels ...
Bruce H

I glue MDF panels into Maple frames for painted doors without issue.

10/27/23       #11: Gluing VS Floating Panels ...
Adam

Karl,

If you consider that I trained under an ornery old master carpenter kinda guy back in early 90's. He had already had the epiphany that a bonded mdf panel is better than a solid wood door. We were a do anything high end Arch millwork shop. Custom solid historically wood interior/exterior m/t pinned(not glued) doors were one of our specialities. But for paint grade cabinet doors or wainscotting. It was bond in mdf. I know just saying mdf leaves a bitter taste in your mouth. You get over it quickly, when you see zero cracking & it saves a ton of time making/finishing panels.

We've likewise made a boatload of shaker style cabinet doors with rather expensive 1/2" veneer plywood in the last three decades that are bonded. You put the glue on the rebated back of the panel. We still do our raised panel clear/stain grade doors with solid wood.

11/1/23       #12: Gluing VS Floating Panels ...
Rodney Member

Karl, no we still do hardwood raised panel doors we are are in Texas, We do some low budget jobs using mdf panel's actually looks better after its painted Imo , but that the first thing everyone says.. I don't want any of that cheap wood mdf or pb , about 90 percent of the door's we do now are either shaker or flat panel door's, we use a mdf core flat panel with a maple veneer I probably wouldn't recommend gluing the panels in the door frames, I know mdf Is supposed to be more stable. But with that said we use 3/4 mdf core maple for cabinet's with slab doors and have had some problems with warpage on larger doors, maybe its the Texas climate and humidity Idk.

11/2/23       #13: Gluing VS Floating Panels ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I've had bigger slab doors twist up on me too. Mdf core, veneer both faces, .5mm banding.

I do agree that mdf can paint up better, but it still moves. Some of it might be ego too, or a selling scheme that we do hardwood on PG raised panels. I like doing them from wood too.

Anybody cutting the profile and the parts free on the cnc? That could be a nice use of time being it'd be a longish program to run.

11/8/23       #14: Gluing VS Floating Panels ...
warren Member

I use ply MDF. MDF is too clinical the plys have some pores depending and look more like wood not so MDF flat perfect. Depends on final finish and what it is.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors

    Become a Sponsor today!