We are a closet parts wholesaler and are now making our standard drawer boxes out of 1/2" pre finished baltic birch ply. We purchase them in 60" lengths and 4" to 10" widths. Volume is picking up. I expect to be in the 300 box a month range soon and growing.

We are currently using a dewalt sliding chop saw with stops.

I would like to optimize and have software to do this. So I am thinking about a tigerstop or equivalent.
Any comment about comparisons welcome.

My questions is, what is the best saw to use to get a nice cut and increase production?

Better Chop Saw, upcut saw, sliding table saw, vertical panel saw with scoring or ??

As all parts are cut in pairs so 2 at a time would be a nice feature.

Thanks for any advice.

9/9/15       #2: Production cutting drawer box lengt ...
Joel

In my opinion having used all above tools, a dialed in radial arm saw with a stop would be the way I would go. You can stack like 6 pcs even with a 10" saw. Make sure you use a quality blade and that your blade is perpendicular to the fence along it's travel or your cuts will be sh*t. Even a minute angle in your carriage will cause a poor cut. I've used tiger stops and by the time you type everything in you could have measured twice.

9/9/15       #3: Production cutting drawer box lengt ...
Bob Member

Thanks Joel
Radial arm not my first choice because of safety issues.
Your reasoning sounds good so it goes on the list.

If I use a stop, data will be optimized and downloaded from our system. Worst case will use mm as it is so much faster on entry. Don't understand why anyone would enter in inches.

Really want to download, But we have the capability to optimize and then print cut list and/or labels.

Just found out TigerStop charges $1300 for download software and there could possibly be extra hardware needs as well.
Price of productivity I guess.

9/15/15       #5: Production cutting drawer box lengt ...
scott

They say production and accuracy is all about automation. No offense but you measure and cut 10 pieces on a radial arm saw and how many would be the same exact length? I would bet money that you would have a few different sizes. I have many hours on a radial arm saw and think they have some amazing applications, but they are also very dangerous if you have a careless operator.
For the application you are describing you need an upcut saw with a push system. They are made by different companies like Tigerstop, Razor and others. Program the sizes and it pushes the material, cuts them all the same, safely and efficiently.
I agree with the old saying that there is more than one way to skin a cat? What works great for one guy is not great for another.

9/24/15       #6: Production cutting drawer box lengt ...
Rich Kuban Member

Website: http://closetexperts.com

As a wholesaler, I would think you would only make so many different sizes of drawers. Would you not have a list of standard lengths to cut? 300 boxes a month is only 15 per day. That is 60 parts, and if cutting 2 at a time, that is only 30 short cuts a day (not including trim cuts). If you can cut two pair at a time, then you are making only 15 cuts per day. I would be inclined to use flip stops and stop blocks first on different saws to figure out the best sizing method for you. I would not be inclined to pursue automation until making 50 - 60 boxes per day, with a proven cutting method.

FWIW, I used a Striebig without scoring with a regular stop and a flip stop to stack cut (up to 4 at a time) vinyl drawer blanks. The flip stop was to cut my shorter standard box sides. Fairly safe, but I learned to cut the short lengths first from my optimization. Downside to the vertical is the shelf is short. If not careful, the blanks could twist and fall off the shelf sometimes. If you used a dedicated machine for this, the operator would learn pretty quick how to avoid doing so.

In order of my preference, I have cut a lot drawer blanks on a Striebig without scoring, a radial arm saw with scoring, and a scoring table saw with a sliding carriage.

9/24/15       #7: Production cutting drawer box lengt ...
Bob

After reading the responses and considering our other needs it looks like we are going to use a Vertical Panel saw.

Rich, I am curious as to why without scoring?

I am looking at Holz Her mainly because I have an awesome tech that I can really trust to check out any machine I am looking at.
But with the cost of moving this type of machine, a lot will depend on what I can find fairly close to me.

9/24/15       #8: Production cutting drawer box lengt ...
Rich Kuban Member

Bought used Striebig without scoring. Was satisfied with climb cutting to score, since you make the stroke anyway. Downside was requirement to change blades more often. At time of purchase did not want the additional cost to add scoring unit (available) and was tired of setting scoring blades on other saws. Striebig rocks when cutting rectangles! Although a good local tech always trumps brand in my book.

9/24/15       #9: Production cutting drawer box lengt ...
Bob

Thanks Rich... and to all who replied.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello