I am doing about 300 to 400 drawer boxes a month and I am about to start offering notching for under mount slides.

Look like I am going to need about an 1 1/4 notch at the from and smaller at the back.

I am thinking about a dedicated cheap shaper with dodo blades to cut set up to cut both front and back notch in one pass through.

I don't want to use the table saw because of having to do 2 passes and the setup time.

Anyone doing it with a shaper?
How is it working?

Any other suggestions?

5/3/16       #2: Cutting Drawer Box notches for unde ...
Bob Member

Dado not Dodo :-)
But I do want to set it up so any Dodo can do it.

5/3/16       #3: Cutting Drawer Box notches for unde ...
Dustin orth

Website: http://customwood@skybeam.com

I do this on a shaper using an insert tip rabbiting cutter with spurs from Amana tools. I do all my boxes in one direction , then flip the cutter over and cut the other. I can do maybe 50 drawers in under an hour, usually less.

5/3/16       #4: Cutting Drawer Box notches for unde ...
D Brown

I cut the drawer box back to sit on top of the bottom , no notch needed , unless I'm missing something .

5/3/16       #5: Cutting Drawer Box notches for unde ...
Bob Member

To start with, they will be dovetailed boxes.
(need to notch after assembly)

Slots need to be front and back.

I just got full specs and front notch needs to be 2 1/8" for front clip to mount to drawer front. Back notch needs to be about 1 1/4". I don't think it will matter if back notch is cut at same width as the front.

5/3/16       #6: Cutting Drawer Box notches for unde ...
Jim Herron

I've got the Amana insert head with spurs mounted in the shaper.
Does a decent job.
For that many boxes on a regular basis you'd probably be better served with a dedicated notcher, ie Penske or similar.
The time saved and safety gain over a shaper with that much head exposed and ready to launch a box would be a no brainer.
I do most of mine with a telephone these days.
I have a 15 spindle dovetailer but can touch them for what I can buy them for.
Still nice to be able to knock out a few boxes or misorder on the fly.

5/3/16       #7: Cutting Drawer Box notches for unde ...
Jim Herron

Missed part of your post.
Dodo using WIDE (think aggressive) dado on shaper equals HUGE medical disaster in the making.

5/3/16       #8: Cutting Drawer Box notches for unde ...
Kevin Jenness

I have installed many a Blum slide on factory built dovetail drawers that were notched only at the back. Why do you need to notch the front of the box? Probably 5% of those boxes were missing pins that got knocked off by careless handling or shipping damage due to short grain at the notch. Do you really want to induce that weakness at the front of the box where it will be all too obvious? Fastening the clips to the finished drawer front is much less forgiving than attaching the front to the installed box.

5/4/16       #9: Cutting Drawer Box notches for unde ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Hello Bob,

There are a couple of very efficient machines on the market for this operation. Penske and Hurst are 2 that come to mind. With 300 drawers per month the machine would probably pay for itself in no time. These machines are designed to plow the notch and bore the pin hole with one pass per side.

Here is some info on one brand.

Hurst Engineering Drawer Notch Machine

5/4/16       #10: Cutting Drawer Box notches for unde ...
Bob Member

Kevin, not my choice. The only under-mount slides I can get that are in 2" increments require the clip be mounted to the drawer front.
We do closets and it would really disrupt our designers to do the 3" increments of Blum or others.

At in and around $10K both those machines are out of my range at this time.

The more I think about the shaper it scares me as well.

I am now thinking about using a small table top CNC and bar codes for calling the program. Maybe a bit slower but a lot safer. I could build 2 for about 1/4 the price of the dedicated notcher and probably be faster.

I am going to experiment with our Biesse to see if this is viable.

5/4/16       #11: Cutting Drawer Box notches for unde ...
Kevin Jenness

Bob,

That makes sense, but it still leaves a weak point at the bottom corners of the drawer. I can"t count the times I looked for those broken pins to glue them back on, failed and installed the drawer gap-toothed because the show had to go on. It might be worth the extra minute to secure those weak corners with a micropinner.

5/4/16       #12: Cutting Drawer Box notches for unde ...
jimherron

Have you considered a custom stagger tooth head mounted in a table saw with a recess machined to allow the arbor nut to be secured? The cutting pressure of a wide cutter is what knocks the weak dovetail socket flying.
I think it would be infinitely safer than the shaper setup, especially with a sled, and would facilitate a blowout board.
How much are you charging to notch and bore the boxes?
How many boxes would you need to do to get back to zero on the 10k machine?
What's a hand worth? What's the worry worth?
Just some considerations.

5/4/16       #13: Cutting Drawer Box notches for unde ...
Bob Member

The safest option appear to be CNC.
That's the rout I am going to pursue.

First I have to prove it will work on a CNC.
We will run some tests on our production router.

I have a need for some flip operations that would tie up the main production router that I would like to do and a couple of other non critical operations, so I may try a cheap slow Chinese 4X8 CNC just for this type so stuff.
I am lucky that I can maintain these types of machines or I would never try one from China. Also having several "non critical uses" is key here.

I really wanted to add making the dovetail drawer boxes on a CNC to help justify the 2nd machine. (This also would have made this problem moot) But, I read there were some issues using this method and no one responded on the CNC forum about making them that way. Anyone know of a successful operation using CNC to cut (semi) dovetail drawer box parts?

5/4/16       #14: Cutting Drawer Box notches for unde ...
Stuart Douglas

No notch in the front, and just cut the whole back short. It allows the bottom of the drawer to be removed for finishing, or replaced when damaged. Secure with a screw (or brads), up into the bottom edge of the drawer back. Done deal. It's a more flexible way of doing these and the only downside is the potential for the bottom dovetail to get "gap toothed." It's at the bottom of the back of the drawer and hardly noticeable.

5/4/16       #15: Cutting Drawer Box notches for unde ...
Bob Member

Stuart: What if my slides require a slot in the front? :-)

5/4/16       #16: Cutting Drawer Box notches for unde ...
Mark Elliott Member

Bob,

Take a look at the KV MUV slides. They come in 2" increments and don't requirer the front notch.

Mark

5/4/16       #17: Cutting Drawer Box notches for unde ...
Bob Member

Everything is a trade off. The KV's are 3 times the price of of the imports I am testing and so far so good. Trying to find that ballance.

5/5/16       #18: Cutting Drawer Box notches for unde ...
KAP

Bob, if you're notching the front and back, IMHO you're over-thinking this...

It comes down to efficiency... for a CNC, you'll have to set-up both the front and back on the table, as well as, programming for notching and with the notching machine above, you're still dealing with four corners (not to mention a costly investment)...

Since you're notching both the front/back, you can simply run the drawers after assembly with the support of the fence and only have to make one more pass to get to 1.25"...

I mean, you're literally talking about 15 seconds on each side per pass... add a hole jig for above the notch in the back with a drill bit and depth stop, and again, we're talking seconds... at 18-20 drawers per day, let's say it takes a TOTAL of an hour to notch and drill the holes (allowing a total of 3 minutes per drawer on average)... it would take a lot longer using a CNC no matter the set-up... and would you really want to tie up a CNC and an operator who most likely makes more for notching?

Even if you're paying a guy $20/hour (most likely less), you're stressing (maybe a bit strong characterization) over $20/day for a service that you're going to charge for I assume (average is around $3 for notching) so at 18-20 drawers per day (300-400/month) you are making more than double your labor cost (considering loaded labor cost) for an add-on service...

Add to it, it allows you to use existing tooling (even if you wanted to dedicate a table saw for it, a lot cheaper equipment purchase), and not to mention dado blades used for this purpose will last a lot longer than bits, so you'll save money on consumables... and the skill level is minimum for the application as laid out...

Just some thoughts... Best of luck... 8^)

5/5/16       #19: Cutting Drawer Box notches for unde ...
B

I set up to dado with a sled prior to assembly. You can notch 10 or more parts per pass by stacking them all together Takes 10 minutes total for 20 boxes. Ive also tried one scoring cut and breaking out the notch with a hard blow from a hammer. Works okay but occasionally breaks higher than I'd like.

5/5/16       #20: Cutting Drawer Box notches for unde ...
Dustin orth

Website: http://customwoodmontrose.com

I will try and do a video of how I do this so you can see exactly how simple it is for me to do large quantities of drawers in a short time period SAFELY. Dustin

5/5/16       #21: Cutting Drawer Box notches for unde ...
jimherron

Anxious to see the video.
Hit it...

5/8/16       #22: Cutting Drawer Box notches for unde ...
dustin orth

Website: http://customwoodmontrose.com

I am attaching 2 videos, one describes how I do this, the second shows how I do it. Sorry if I didn't put the links in the right place. Dustin

https://www.youtube.com/watch?v=6yvrhsIbhP8

https://www.youtube.com/w
atch?v=DOg_jsSMKzk

5/8/16       #23: Cutting Drawer Box notches for unde ...
Jimherron

Thank you for your time to make the video.
Very informative.
I now know that my old Beach Mfg shaper is too slow and lacks reverse.
My shaper now sucks.
I thought my shaper was a bargain at the 300.00 I paid for it.
I was wrong.
My shaper is a Ford Pinto and I am two steps from walking.

5/8/16       #24: Cutting Drawer Box notches for unde ...
Dustin orth

Website: http://customwoodmontrose.com

Sorry for making you see a pinto Jim, it took me many years to get a shaper like that.

5/8/16       #25: Cutting Drawer Box notches for unde ...
Mark V.

Dustin,

Cabinetmaking and model trains....sweet!

Mark

5/11/16       #26: Cutting Drawer Box notches for unde ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Bob, I cut those notches on a small rockwell shaper I picked up years ago on an auction for pennies. I had a set of dado heads cut with a 1" bore, built a weird tall fence for it, and use it for cutting the notch. I'm not producing near the numbers of drawers per month that you are, but I grew tired of doing it on the tablesaw and this works pretty well. I posted this video because I posted a picture of it on facebook and a friend asked WTF is it?

https://www.youtube.com/watch?v=ur8etQ5Q8SY

It's a little scary looking, but if you're doing it correctly your hands are nowhere near the cutters. I also had to get another pulley for the shaper so I could slow it down from ludicrous speeds. I found a calculator somewhere on the google to get the rpm in the correct range.

It works well, it's fast enough. If I had the money and were producing drawers in the quantities that you are I would buy a machine that cuts the notch without having to flip the drawer, and also drills the hole in the back. This shaper setup isn't great, but it's lightyears ahead of doing it on a stupid tablesaw.

Video

6/5/16       #27: Cutting Drawer Box notches for unde ...
Jason

I have actually used a drill press and forestner bit in times past.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello