Medex for raised panels

3/13/18       
Bill

We are starting to make hybrid doors with MDF raised panels. I am being told Medex is one of the better materials to make these with.

Does anyone have experience with this material? I understand it resists moisture better than most MDF. Is it harder on cutters?

Thanks

3/13/18       #2: Medex for raised panels ...
Leo G Member

What are you looking for in the panel? Most people are looking for less prep on the beveled edge.

I've been using double refined MDF by Plum Creek and it reduces the amount of prep needed by a large factor.

If you are looking for water resistant qualities the the Medex is the way to go.

3/14/18       #3: Medex for raised panels ...
David R Sochar Member

Cabinet doors? Passage doors? Exterior doors?

Who is telling you this, the Medex salesman?

First, you will need good carbide tooling and plenty of power to raise the Medex or any MDF for long. You will also need to have excellent dust collection and personal protection since the brown cloud can/will envelop everything as well as your lungs.

I no longer make any panels in MDF. As in "you can't pay me enough to deal with that crap."

3/14/18       #4: Medex for raised panels ...
Bill

A customer prefers Medex, hence the question.
They are cut on a Cnc router with custom made tooling.
Our dust collection is excellent there is no objectionable dust.
They are for paint grade cabinet doors.

3/14/18       #5: Medex for raised panels ...
door shop guy

I never met a piece of medex that did not curl up like a potato chip.
I will use plum creek if the customer wants to buy the cutters. So far no one has. I will not use my cutters on it.

3/14/18       #6: Medex for raised panels ...
Bill

We are early in this and we have tested with Plumb Creek. Medex in the thickness I need is hard to come by around here so I think it is a no go anyway.

I have many customers requesting Hybrid doors, I really don't have much choice. The benefits with painted jobs make it worth it. We will be producing them on a nested router so the labor savings is also significant. Think about that savings.

Hardwood process is:
Rip boards
Cut boards to rough length for a panel
Glue the panel
Scrape glue from the panel
Run through planer
square/size the panel
Profile one side at a time
Sand profile.

With hardwood the parts been handled quite a bit.

MDF process is:
Create nest
Drop full sheet on the router
Push button
Go do other work.
Come back, pencil job number on panel
Sand profile

We have dedicated insert carbide tooling for the MDF. I am not sure how long it will last at this point.

3/14/18       #7: Medex for raised panels ...
David R Sochar Member

"I have many customers requesting Hybrid doors, I really don't have much choice".

For several years around here a mantra was "Sell what you make rather than make what you can sell". The point being one of self-determination vs a flag of the winds, at the mercy of the winds, as another once put it.

Once we learned to sell what wanted to make, we never looked back. The money is a bit better, but we are all happier, we have a far better class of customer, we really find satisfaction on several levels, we are the envy of our peers, and even the scrap is better.

I do not mean to tell you what to do. Enough is written about herd mentality and how lower prices is always a dead end that is hard to reverse. Just my opinion.

3/14/18       #8: Medex for raised panels ...
Bill

I appreciate your input David but it is not like that at all. I sell wholesale and it’s not about price. It’s about the quality of finish and stability of the product.

3/15/18       #9: Medex for raised panels ...
Adam

We've used 5/8" ultra refined mdf for raised panels since they invented the stuff in the mid 2000's. 3/8" mdf flat panels(been using that forever before the good mdf)

Both fully glued into soft maple.

We get zero paint cracking. Wood panels always crack, show, etc.

Never really had any issues with shaper cutters. Not sure why the other guys are complaining.

We don't have any issues around the dishwasher. There is a ton of paint on the raised panel.

3/15/18       #10: Medex for raised panels ...
Brad

I would call Vortex and talk to them. I believe they did a lot of testing on the CNC when they developed this set --->https://www.vortextool.com/index.cfm?fuseaction=category.display&catego
ry_id=65&CFID=34286750&CFTOKEN=7d90ca31563b7ab0-A446365D-F887-C871-A45B83
B3903E3274

4/20/18       #11: Medex for raised panels ...
Tracy Yarborough  Member

If you are going to produce MDF doors of any appreciable quantity, invest in diamond tooling. At least for your main bits. Carbide will work for about a 100 doors or so before it becomes dull and begins to burn. Customers are asking for Medex brand probably because of its moisture resistance properties. A good quality, double refined mdf panel with good coats of bonding primer will last for many, many years without abuse.
I can't get medex in my area, but some guys I know in the northeast use it, and claim that it is a good product for panels and doors.

7/11/22       #12: Medex for raised panels ...
Ian Gunn

Can you stain a door made with Soft maple surround and Medex inserts? Ie will it be possible to get same finish? We have had a custom door made for our house and we requested “paint grade” so they made it with soft maple surround and Medex inserts. They are saying that is the best for dealing with weather issues but our assumption is only if whole door is painted vs staining. If inserts were wood is panel likely to shrink ?


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors
    • CabinetCRUNCHER
      3D Cabinet Design and Construction Software Powered by SketchUp and Excel, Precise Cut List Calculators with Highly Adjustable Construction Options for Cabinetmakers and Woodworkers of All Levels
    • Holz-Her US Inc.
      Custom Edgebanders, Vertical Panel Saws, CNC Beam Saws, Wide Belt Sanders, CNC Point to Point Boring Machines, CNC Routers
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • 360 Degree Machinery
      Specializing in high end American, European, and select Import woodworking machines.
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Original Saw Company
      Industrial Radial Arm Saws
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands

    Become a Sponsor today!