Door Making Process

5/12/18       
Edward Curtis Member

After buying doors for 20 plus years, I am going to start making them again.
I'm investing in new equipment, 3 shapers, straight line rip, 5 head moulder, amoung others.
In the old days of making doors, I would tend to buy stock in the rough, rough cut to length, joint, plane , rip to achieve S4S, do copes, then patterns.
With the new eqipment, I'm thinking order rough stock, straight line Rip, send thru moulder to achieve S4S, run thru sticking Shaper to get pattern, Cut stiles and Rails to length, run copes. Will I get blowout on one end of copes?
What am I missing? What would you do differently, given the same equipment

5/12/18       #2: Door Making Process ...
Paul Miller

Website: http://MCCWOODWORKING.COM

Not knowing what equipment you have now, its hard to make a suggestion. Wide belt sander is a must, a random orbital wide sander is also needed.

I have a Unique 250 door machine. I like this, easier to set up. I also use carbide insert knives, they last a long time.

As for the blow out, that is not a problem, just put a block of wood behind the piece being machined.

Having said all of that, we have all the equipment, but I buy most of our doors. Labor is an issue for me and I think the cost of buying doors is not much more than making them ourselves. We can make more money doing other things.

5/12/18       #3: Door Making Process ...
Bill

If you have a moulder wouldn’t you make the inner profile on the rail stock not just S4S? With a moulder you can also make mitered door rails if you choose.

Don’t forget, glueing panels, squaring/sizing panels, shaping panels raise, sanding the panel profile.

If you are making stain grade panels staining the panel tounge when it’s apart is not a bad idea.

5/13/18       #4: Door Making Process ...
Curious

Why have you decided to bring doors in-house?

5/13/18       #6: Door Making Process ...
Edward Curtis

With a higher volume of doors that we arenow buying, I think we can shift the doormaking in house. Our number of employees have grown, and the overhead burden, per employee has gone down.
When I consider the timing that damaged doors cost us, sometimes the quality of the outsourced doors, I think we can do better, and do it profitably.

5/14/18       #7: Door Making Process ...
David R Sochar Member

Paul has it covered, with one exception. For 40 years I have heard one can run sticking first then tenon/cope. Use of a block of wood, or a coped scrap will back up the rail end work with no blowout.

I have never been able to make that work. We build a lot of passage doors, and we oversize the rails in width. Tenon and cope, then joint or plane to remove 1/8", then profile and plow the rail. We remove the 1/8" to take care of any cope blowout.

Even with cabinet doors, we follow a similar process. We have wood rails on all our coping sleds, but there is still blowout.

If you look at the top cabinet door equipment (Unique comes to mind), you will see cope cutters with two counterrotating spindles. Cope the first half of the width of the rail feeding one way, and the second half feeding into the other cutter. No blowout at all.

This allows you to run stock to pattern on the molder, eliminating a few large steps.

5/14/18       #8: Door Making Process ...
JR Rutter Member

Website: http://harmonicdesignworks.com

I like to cut the S4S stock to length first, flipping/turning as needed to get best face and crown up. Then we cope rails with a simple square backer to minimize blowout (losing maybe a couple pieces on a kitchen if the inserts are getting dull). Then feed the sticking shaper in a continuous flow for each stack. This only takes a bit longer than running sticking full length and simplifies the cope machinery/process requirements.

5/15/18       #9: Door Making Process ...
David R Sochar Member

It is all about quantity - how many doors will you make in a batch? Will you make them every day? or once a week? or once a month?

I also like the rough length, rough width, face and edge method. You can defect better, and get better parts. Great for a few doors. However, there is nothing like a ripsaw and S4S molder or profile molder for making hundreds or thousands of parts.

Congratulations on making your own doors. It is about taking pride in your work, and 'doing the work'. You will produce a better product, with more employee pride and self-respect.

5/15/18       #10: Door Making Process ...
Karl E Brogger

I like to run full lengths for sticking, cut to length then cope.

You should thickness, size, and stick in one pass on the moulder if that's available to you. Saves one step, and should be able to run a higher feed rate than a shaper.

Coping on a shaper is asinine in my opinion. It's how I do it, but it is slow and depends too much on the operator to keep his head out of his posterior. I'd look into a automatic coper. That's the direction I plan on going soon. Tooling costs double with the one I'm looking at since it uses counter rotating heads to eliminate needing a backer block.

You'll need a door clamp. Clamping with pipe clamps can give good results, but it's painfully slow.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • OMEC/Macoser Inc
      Exclusive Importer of European Woodworking Machinery Since 1988
    • Steve H. Wall Lumber Co.
      Quality Hardwoods and Softwoods, Exotic Wood, Furniture Quality Plywood, and Hardwood Flooring
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Denray Machine
      Quality Dust Filtration Systems Provided by an Industry Leader in Wood, Metal, and Many Other Dust Control Applications
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • J&P Machines
      Design and Production of Custom Equipment for the Manufacturing Industry

    Become a Sponsor today!