Looking for advice on the best approach for a client who wants painted slab cabinet doors with a vertical v-groove. We have always built 5 piece doors so this is new territory for me. We use a CNC in the shop and my initial thought is to cut MDF for the doors on the CNC, but I have never produced 100% MDF doors with no rail/stile. We use MDF for our paint grade 5 piece door panels so working with MDF isn't new, but I am worried about the durability of the edges as well as the finish quality. Any advice?


View higher quality, full size image (928 X 1145)


View higher quality, full size image (1682 X 145)

3/3/22       #2: Slab V-Groove Cabinet Door Construc ...
james e mcgrew  Member

Website: mcgrewwoodwork.com
Simple enough, I use Vectrics Aspire yet the lower tier Vcarve pro or any software capable of following a single vector line will do this. you could cut all the doors including the v bit work from full size sheets it you have a cnc
Take a look at Vectric .com vcarve or vcarve pro, no need for aspire unless you intend to make and work 3d (2.5d) files


View higher quality, full size image (1090 X 1004)

3/3/22       #3: Slab V-Groove Cabinet Door Construc ...
Skip Member

Thanks for the response James, but I'm more concerned with the performance of an MDF slab door long term. Machining the doors won't be an issue. Have you made doors like these and seen how they hold up?

3/3/22       #4: Slab V-Groove Cabinet Door Construc ...
Adam B Member

Skip,
What is your definition of "long term performance"? The use of MDF as it pertains to doors has been discussed on this forum many times and there are some that trash the idea and avoid mdf like the plague. Then then there are those that have been using it for quite a while without issue. We have been carving 1 piece mdf doors regularly for about 5 years now. We also supply mdf carved doors to other shops in our area. In my experience, normal everyday use of opening & closing doors/drawers does not result in any noticeable difference between an mdf door or a 5 piece hardwood door. I will 100% agree that if little Johny rolls his tonka truck across the kitchen floor and it were to strike an mdf door, that door will show more damage than a hardwood door would. However in either case a blow of that magnitude would have damaged the paint/enamel/varnish of either door style resulting in the need for some type of repair.

In my world, in our market place/geographical region, MDF doors and drawer fronts are a very acceptable option to use/offer in today's paint crazy mindset.

3/3/22       #5: Slab V-Groove Cabinet Door Construc ...
gary

I am probably opening a can of worms but I think mdf gets a bad wrap on this forum from a handful of people and it unfairly scares a lot of people . We have been making mdf painted doors for long enough that if were a problem it would have shown up by now. I would put them in my own house if I wanted painted cabinets.

The biggest failure of any cabinet door starts when moisture gets under the finish. The finish will always crack at the stile and rail joint from natural wood movement so this is the most common place failure starts. This invites moisture to get in and under the finish. There are no such joints in a one piece mdf door so the most common cause of finish failure does not exist.

We always give our customers the choice of mdf or a 5 piece door. They almost always go with the mdf. We do not push one over the other because we get paid either way.

Some call mdf garbage, and a lot of other names and that working with it is poor craftsmanship. I couldn't disagree more. My guess is they have never used it or given it a fair chance.

I say make them doors out of mdf and don't look back. Even if a door does fail, which it wont, it is very easy to replace.

3/3/22       #6: Slab V-Groove Cabinet Door Construc ...
Nate Cougill  Member

Website: http://www.cougilldiversified.com

If you have any concerns with durability, wrap them in 1/4” hardwood banding, but it’ll work great without if you seal the cut edges with sizing.

3/4/22       #7: Slab V-Groove Cabinet Door Construc ...
Skip Member

Thanks for all the responses. It seems that MDF is the best approach with good care during finishing.

Nate, what did you mean by "sizing"

3/4/22       #8: Slab V-Groove Cabinet Door Construc ...
Nate Cougill  Member

Website: http://www.cougilldiversified.com

Hey Skip, diluted pva wood glue 1:1. Here’s an older forum post: https://woodweb.com/knowledge_base/Prepping_MDF_for_Paint.html

3/5/22       #9: Slab V-Groove Cabinet Door Construc ...
Adam Spees

Sizing mdf with glue is some old school thing from the 80's. They used that bondo, and drywall compound.

Most people have known that you can simply use high quality mdf. Sand it with 240grit. Spray or brush on two coats of a primer/sealer like BIN shellac or a catalyzed one like Clawlock. Sand the primer with 320 and it looks identical to the mdf face.

3/6/22       #10: Slab V-Groove Cabinet Door Construc ...
PKD

Website: http://www.premierekitchensllc.com

we edge band the edges with maple tape.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors

    Become a Sponsor today!