Subject: Re: Fiber Tear Out

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Fiber Tear Out

1/11/16       
Dan Heagle Member

Just purchased my first CNC to get a handle on production back logs. With absolutely no experience using a CNC I'm hoping this site will help a great deal with my learning curve.

I have a Holz-Her Dynestic 4x8 with an 11kw router controlled by Cabinet Vision. I've been using solid carbide 1/2" up/down spiral cutters with suggested spindle speeds and travel according to the manufacturer when cutting 3/4" thick particle board with double sided melamine.

I was unaware of the fibers that pull out of the edges, even when the cutter is new (small but noticeable), and eventually get larger as the blade wears. This all while the melamine is still chip free. With this issue, I have to hand sand the edges prior to edgebanding if I use a PVC tape that is thinner than 0.8mm.

From my limited research I found that to solve this issue I would have to purchase an edgebander that has a pre-miller.

Question: Is purchasing a pre-miller my only option, or is there a better cutter available, or specific operations required when nesting?

Thanks in advance.

1/11/16       #2: Fiber Tear Out ...
Eric Olsen  Member

Website: http://www.erccabinets.com

You could change the way you program your parts by adding a final pass to the part. This has a tendency to not pull out the center of the core because your not trying to route in one pass. The time difference is nominal.
Another option is to switch to a 1mm edgebanding for the short term. the 1mm doesn't radiate the core issues your having.

1/12/16       #3: Fiber Tear Out ...
Paul S

I have found that this varies from mfg to mfg. last job I ran I used panel lam ..... Not happy at all there was a lot of tear out .... Plumcreek I had very little tear out. So I would try different mfg products and see what works best for you

1/12/16       #4: Fiber Tear Out ...
Gerry

Hi Dan,

I came up against the same issue when I started using the router. I think both of the suggestions above are accurate. I found that Panalam hardwood core tends to leave a rough edge. They have a softwood core that leaves a smoother edge. I have found I can get an acceptable edge on the hardwood core by using a double outline pass on all parts with the down side being the extra time and wear on cutters and machine.

I don't think you will ever get as nice an edge as you get off a good panel saw with a sharp blade.

Gerry

1/12/16       #5: Fiber Tear Out ...
Dan Heagle Member

I leave the skin on parts 6" and smaller before cutting through and they too leave the centre core pulled out. The cores with more hardwood left bigger voids in the centre which for me indicates large particles being pull out or just bad quality sheets. The sheets I've tried with more softwood in them didn't leave voids but the rough core is now my only issue.

Would any one know if the upgrade to a pre-mill on an edge bander be the solution to this problem? or is this just another process that will add to my dust collection bins?

1/12/16       #6: Fiber Tear Out ...
Eric Olsen  Member

Website: http://www.erccabinets.com

Yes an edgebander with a premill setup will eliminate this issue. You would either add to the part what the premill takes away or not stress the 32nd of an inch.

1/12/16       #7: Fiber Tear Out ...
Richard

Hi Dan,

When you leave the skin on the small parts do you also offset it away from the edge of the finished part? I usually find this does the trick.

I have also found that 3/8" cutters tend to be less aggressive on the core.

Never used a pre-mill on an edgebander so can't comment on that. Thicker edge tape does help.

Good luck!

Richard

1/12/16       #8: Fiber Tear Out ...
Leland Thomasset  Member

Website: http://www.cnc-cabinetparts.com

I am curious does a climb cut help out with this issue?

http://taghkanicww.com

1/13/16       #9: Fiber Tear Out ...
Dan Heagle Member

I'm leaning towards Eric's answer with the purchase of a new edge bander with the pre-mill. I'd rather use one solution to enable me to keep with a single pass to cut larger parts, pick and chose any sheet manufacture colors and tape thickness.

I've only worked with Holz-hers edge banders in my shop and the shop I learned this trade. I never had any major issues and I did all the service on them. I especially like the glue pucks that take less than 5 min to heat up.

Has anyone had experience with their 1054 Streamer? or any other brand that's similar is size with pre-mill? I'm limited with space and this model has all the options I would need.

I'm supposed to have an estimate by tomorrow for one.

1/16/16       #10: Fiber Tear Out ...
Gerry

Leland,
The climb cut does help but causes other issues, deflection of the cutter being one of them. What we do is a climb cut on the onion skin then a conventional cut on the finish pass. This works for us even using the hardwood core with the larger pieces.

I would be interested to know the pricing on the new bander also if that is allowed in a open forum?

Gerry

1/17/16       #11: Fiber Tear Out ...
Jason Scott

We had the same problem but have found that conventional cutting with a 3/8 3 flute tool gives us a much better edge than the 2 flute tools and you get the bonus of running much faster. We have been running 18,000 RPM and 29-30 Meters/minute on 3/4 melamine.

1/17/16       #12: Fiber Tear Out ...
jerry Member

We use a low helix 3 flute Vortex 1/2 inch bit and get good results.

1/17/16       #13: Fiber Tear Out ...
Gerry

Jerry,

We use Vortex bits also, could you give us a part number for the bit you are using?

Thanks,
Gerry

1/23/16       #14: Fiber Tear Out ...
Dan Heagle Member

In response to Gerry's question. The price came in at $46,800.00 Can. for a Streamer 1054 which has Pre-Milling, Auto Load Glue Cartrige, End Trim, Top/Bottom Trim, Scraper Unit and Buffing. Delivered and Installed.

They will give me 5k for my 1402HF off the price as a trade in.

1/23/16       #15: Fiber Tear Out ...
Gerry

We just completed a job using Stevens textured melamine that has a 1mm matching edge tape and it makes me think that using 1mm tape all the time would be an acceptable solution for me. If of course the tape you need is available in 1mm.

The pre-mill option got me thinking that if the edgebander milling was not perfect you could off size your parts or take them out of square? Not having used a bander with this option I don't know if it is a concern but it gets me thinking after using a router to get all the parts accurately sized I hesitate to introduce a process that would compromise that. I have seen one bander that by all accounts works well with the pre-mill option but the cost on it was closer to $500,000.00 Can. If the pre-mill works well in this price range it would allow you spend a lot less time worrying about edge quality coming off the router.

Thanks for getting back with the quote Dan.

Gerry

6/12/16       #16: Fiber Tear Out ...
Dan Member

I had the new pre-mill bander installed a few weeks ago. Tweaked it a bit after the techs were finished setting it up. Tape to board is near flawless.

I now cut all parts on the CNC to exact sizes (no reduction for tape thickness) and pre-mill the tape thickness on the edge-bander. This now removes all fibres that are protruding the edges and any skin left over by not going deep enough on the cuts. 0.5mm PVC tapes comes out smooth. The only issue left is if there's voids in the core, they show the indents. When exposed edges need to be perfect, I just add 0.5mm to my overall size of board and take off 1mm on the bander.

Very happy with the results.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA