We are just getting started running jobs with our Pratix. Here is a photo of the edge quality in pre-finished maple. You may not be able to see in the photo, but the the edge is not straight, there is a slight step. Terrible! Test pieces run in melamine were near perfect. Speed, feed rate, tooling? Any input as to what we need to change would be appreciated.


View higher quality, full size image (2108 X 902)

1/19/16       #2: Edge Quality on Plywood ...
Gavin S

Website: http://soraghanwoodworking.net

What are you using for tooling ?

A 3/8" compression but should deliver great results , much cleaner than your picture . Feeding @ 450 IPM (a lot of production guys run faster ) @18,000 rpm
Even a 3 flute down cut should yeild better results

Out of curiosity did you buy your router new and who did you purchase from ? Patrix were on the table when I was in the market .

1/19/16       #3: Edge Quality on Plywood ...
cabinetmaker

we started running at a much higher spped to reduce tooling wear. It was such an increase that parts were moving and I have a 40hp pump Then we started return onion skinning everything. Edge is much better and the parts are coming off done and clean

I will post our speeds tomorrow.

We use Vortex 3130xp for melamine, plywood and double layed laminate

1/19/16       #4: Edge Quality on Plywood ...
daveguru

Make sure you "Power Cut" plywood as opposed to "Climb Cut".
Climb cutting will give you the furry edge finish in the pic.......

1/20/16       #5: Edge Quality on Plywood ...
jerry Member

It does look like he is climb cutting. I would do some tests cuts but cut the pieces so you have a drop and look at both sides of the cut and see what side is better. then change direction and cut again

1/20/16       #6: Edge Quality on Plywood ...
Dropout Member

If the edge needs to be decent I use chipbreaker compression spirals and if not I use roughing bits.

2 flute compression spiral chipbreaker - 600IPM climb cut full depth less 0.030, finish pass 600 IPM full depth opposite direction, slower finish pass smaller pieces.

I refuse to cut import ply.

1/20/16       #7: Edge Quality on Plywood ...
John McGinnis Member

Website: http://www.TGCabinets.com

That's pretty bad. We have the same router. We use an Onsrud 3/8" Compression bit with marathon coating for our outlines and a Vortex 3/8" Down for dados. I'll post a pic of the tool settings for both. The software should look familiar. The one with the cutter diameter of .371 is the down and the one with the cutter diameter of .375 is the compression.


View higher quality, full size image (1224 X 1632)


View higher quality, full size image (1224 X 1632)

1/21/16       #8: Edge Quality on Plywood ...
Jason Scott

Am I the only one who noticed the scorched edges at the corner and the beginning of the tenon? Make sure that you are cutting a round toolpath around your corner. I have been cutting baltic birch 1/2" thick at 22-23 Meters/minute (about 900 ipm) with an onsrude 3 flute mortise compression. Nearly perfect edges but we had to change our onion skin to 0.07 thick or it chipped really bad on the bottom edge. We run 3/4 melamine 28-30 M/Min on melamine depending on the parts.

1/23/16       #10: Edge Quality on Plywood ...
John Murphy

Website: http://www.allstaradhesives.com

You can avoid the onion skin and the reduce chatter by simply running (applying a peel-n-stick sealant) inside your tool path.
A product 1/16" thick by 1/4" wide would be perfect for your application.
If any of the CNC operators who have offered tooling and programming suggestions to resolve this issue please contact me for a free roll of this product and DIY.
Good Cutting
Captain Sticky


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Suction Cups, Vacuum Lifters, Vacuum Pumps from Anver Corporation ecabinet systems.com Thermwood Limtech Industries, Inc.