Anderson alum/phenolic grid sizing?

1/29/18       
Steve Member

I've been tasked with making pods for our new Anderson CNC (which we don't actually have yet) on my Homag but all I'm told is the table is the same. I tend not to believe that.

Does anyone know the table grid of the Anderson CNCs? The Homag is 30mm of which 7mm is the gasket groove and the depth is also 7mm.

1/29/18       #2: Anderson alum/phenolic grid sizing? ...
DannyB

A lot of these grids actually are the same.
The spacing is usually 30mm as you mention.

My recollection, however, is that Anderson is slightly off (or at least, used to be).

Honestly, i'd just bug Anderson and ask.

2/7/18       #3: Anderson alum/phenolic grid sizing? ...
Mike McClaran

Steve,
You make the wood components and I will make the Better Vacuum Cups. You could have had these in your shop by now. Also Anderson is likely going to tell you to buy the Green ones. Call us, we can help.
877 872-2821


View larger image

2/7/18       #4: Anderson alum/phenolic grid sizing? ...
Chevy

Website: http://keysoftwareservice.com

im not sure how they make these pucks,,but i can vouch for better vacuum cups,,,used them on weeke and biesse,,and they are spot on,,,acutally better than the ones from Homag,,ive even cut thought a few of them,,keep up the great work,,

hooray for the hot girls at your events

Chev

2/8/18       #5: Anderson alum/phenolic grid sizing? ...
steve Member

I have looked into the green pods and many others but I find that a two piece pod with a changeable top (for damage and size) works best for what we do.

Turns out Anderson was supposed to match our Homag table exactly (for sharing pods) and failed to do so. They are close and small pods fit but the spacing is off just enough that longer pods are too tight to fit.

2/8/18       #6: Anderson alum/phenolic grid sizing? ...
Mike McClaran

Steve,
Perhaps you have not seen our video. While you are purchasing your rubber replaceable tops, our BVC is still running for free in 30 seconds by installing the foam gasket. It's pretty safe to say our BVC lasts 20 times longer than what you are using now. Just as Chevy said he has routed into a few and still using them.

Here at BVC we manufacture over 40 different sizes of vacuum cups. A picture says a thousand words. Maybe if we could see a picture of what you are trying to accomplish, I or someone else on the boards could help.

https://www.youtube.com/watch?v=Dw1IU2Pdyco

2/8/18       #7: Anderson alum/phenolic grid sizing? ...
steve Member

I've seen your video and an impressive product it is.

However if you are skilled enough to not hit your pods nor purchase your pods in the first place it is far more economical to make them yourself. I'm using the same pods I made when we started our new line five years ago and other than pitch build up they look and work as they did new.

2/9/18       #8: Anderson alum/phenolic grid sizing? ...
Tom Flowers

Website: http://AndersonAmerica.com

The Anderson Grid is on 50mm centers. It has a 5mm x 5mm groove pattern. BVC, Schmalz, and NEMI all make standard offerings for this grid. Email me if you'd like for me to send you the part #s.

Regards,

Tom Flowers


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    ecabinet systems.com Thermwood Limtech Industries, Inc.