3/29/19       
Jeff

So weeks and months are passing and my cnc is still basically a large boat anchor.
SCM has been able to get the machine to cut but it appears that it won’t recognize the drill head. The other issue is the rail/bar on the back of the machine won’t go down when you engage the vacuum hold down.
When you try to run a program with the drill head, it moves the drill head into position and then it stops and a code comes up, plc17 Head 2 not in position.
I was wondering if anyone else has had this issue and how it was resolved.
I really need to get this working, thanks for any help or ideas.

3/30/19       #2: The SCM saga continues part 2 ...
Rob Young Member

Website: nutekmachinery.com

Jeff- you've written that the drill head moves into position, does this mean the air cylinder has lowered the drill head down to working position? If so it sounds like the reed switch in the cylinder may not be made. If the head is indeed all the way down you may need to adjust the position of the reed switch. Be cautious when making adjustments like this. When a machine is in the automatic mode providing a missing input, in some cases, will allow the machine to progress in the program. An operator died at a factory I worked at due to those circumstances.

If the cylinder is not activated you'll need to determine if the controller is sending the output to the valve to activate the head dropping.

3/30/19       #3: The SCM saga continues part 2 ...
Jeff

Rob,
Thanks for the info, the drill head moves into position on the x and y axis, but does not move on the z. It then stops and throws the plc17 code. When you hit a safety switch or step in the light barrier it lets out a huge beltch of air??
Thanks again.

3/30/19       #4: The SCM saga continues part 2 ...
cabinetmaker

Seems to me you need to reload the operating software. The “fixed cycles” maybe not fully loaded.

We went through this when we had a problem with our operating software and it had to be reloaded as the fixed cycles did not fully “take” Boring block would come to the drilling point but not descend.

4/1/19       #5: The SCM saga continues part 2 ...
Chris

Jeff,

You never said what model you have. If you go into MDI can you drop any of the boring spindles? The way the Scm machines works is all the calibrations are based of the #1 boring spindle.

4/2/19       #6: The SCM saga continues part 2 ...
Jeff

Chris,
The machine is a Pratix 48 and the individual drills can be dropped down manually through MDI.
Thanks

4/2/19       #7: The SCM saga continues part 2 ...
cabinetmaker

What are the length of the drills in relation to each other in the tool library ?

Go through the basics of calibration, sorting out lengths, diameter, symmetrical behavior

If it’s coming to the area to drill are you sure it’s not a fixed cycles issue ?

What does scmi state your error means ?

4/4/19       #8: The SCM saga continues part 2 ...
Matt

Jeff, our machine isn't even remotely the same as your SCM but we had a very similar situation happen. Our machine runs on a PC (WinCNC).

I'm sure it's not a 1:1 comparison of yours, but here is what we had happen.

Machine would do any cuts/holes in a nested sheet of cabinets up to the point that it needed to do 5mm drills. It would go pick up the 5mm bit and then abort the program with an error that said "soft limit Z".

If we ran sheets that had no 5mm drill, things cut without error.

After a few hours of head scratching, we figured out the problem was due to operator error by accidentally clicking "Calibrate Z" instead of "Calibrate Tool". He had just installed a new 5mm bit and was trying to calibrate the machine for the new bit.

On our machine, that mistake recalibrated the 5mm drill to think that the top of the spoilboard was basically the very top of the Z travel, since that's where the spindle was sitting when he hit the button and was holding tool 5.

It didn't effect any of the other tools.

4/11/19       #9: The SCM saga continues part 2 ...
CM

Jeff,

You get the cnc going yet? Your first post was a couple months ago, that is unbelievable that SCM can’t get it working.
A guy that worked for us years ago bought a SCM cnc and he had some issues as well and SCM had no clue, they were pathetic beyond words.
A tech from Homag ended up fixing his machine.

They have no idea that businesses need their equipment to STAY in business. They sit in their office collecting their hourly wage and have absolutely no concept of how the industry works. The field techs come to the shops with their briefcase full of hand tools and a multimeter and charge you north of $100 per hour to fix your machine. I just don’t get it. The shop they are working at has probably a few hundred thousand dollars of equipment, and some shops a lot more than that and they have a hourly rate less than the tech. Blows my mind.

There was another company selling Casadei machines (Another SCM company) and they had the same problem, no one has a clue how to fix them so a bunch of machines being used as dust collectors.

Anyways just my two cents worth. I feel for you.

4/15/19       #10: The SCM saga continues part 2 ...
Jeff

Cm,

Unfortunately nothing has changed, apparently no one knows how to fix it.

I will never buy anything SCM ever again.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA