Frank D. Jimenez  Member

Website: http://www.cabinetpro.com

I am enhancing our post processor for an Omnitech Selexx Pal for our software, Cabinet Pro CNC. Currently, our post looks like the following:

%
O0001 (R7X02021)
(CREATED ON July 16, 2021, at 6:22 AM)
(MATERIAL: 3/4_MAPLE PLYWOOD)
G0 G20 G91 G28 Z0 M15
G90 G40 M22
M88 B0
M89 B0
G08 P1
M25

(DRILLING TOOL: 5mm Y Axis)
(DIAMETER: 0.1969)
M88 B0
M89 B0
M23
M21
M89 B31
G90 G0 G55 X8.7146 Y1.5492 Z1.6250
G98 G81 Z0.5 R1.6250 F100.
X8.7146 Y1.5492
X8.7146 Y7.8484

(DRILLING TOOL: 5mm Y Axis)
(DIAMETER: 0.1969)
M88 B0
M89 B0
M23
M21
M89 B3
G90 G0 G55 X8.7146 Y14.1476 Z1.6250
G98 G81 Z0.5 R1.6250 F100.
X8.7146 Y14.1476

(END OF DRILLING OPERATIONS)
G80
G17 G91 G28 Z0 M95
M88 B0
M89 B0
M92

(ROUTE TOOL: 1/4 Down Shear)
(DIAMETER: 0.25)
G0 G54 G90 X0. Y0.
T16
G0 G54 G90 X10.2500 Y6.5886 M13 S17000
G43 H16 Z1.6250
G0 Z1.6250
G1 Z0.5000
X10.2500 Y19.5449 F275.

(END OF PROGRAM COMMANDS)
G0 Z1.6250
G80
M22
G91 G28 Z0 M15
G90 H0 M25
M88 B0
M89 B0
G91 G28
G0 G90 X59. Y98.5
M76
M00
G1 Y86.6 F160.
Y-2.5 F275.
M00
M77
G91 G28
G0 G90 X67. Y123.
M07
G08 P0
M30
%

------------------------------------------------------

It is the ROUTING section (showing Tool #16 above) we wish to change to the following format (Tool #12 is used in the following example):

(ROUTE TOOL: 1/2 DOWN SHEAR)
(DIAMETER: 0.499)
G0 G54 G90 X44.7825 Y51.3875
T12
G0 G54 G90 X34.0615 Y63.4144 M13 S18000
G43 H12 Z1.748
G0 Z0.998
G1 G42 D2 X35.3115 Y63.4769 Z0.373 F175.
X46.124 F352.5
Y63.2278
X24.499
Y63.4769
X35.3115
X35.8105
G40 X37.0605 Y63.4144 Z0.998
G0 Z1.748
------------------------------------------

Normally, this is an easy process because our post processor is user-defined and readily accessible. But the many X and Y values for a simple dado cut using tool comp. are a bit puzzling. My question is this: can anyone who understands the g-code for a Selexx Pal explain the meanings of the various X and Y values under "(ROUTE TOOL: 1/2 DOWN SHEAR)"? Your help would be very much appreciated.

https://www.cabinetpro.com

7/17/21       #2: Omnitech or Anderson Selexx Pal ...
Mike

X and Y values are just places in space where the tool is, so I'm not sure what you are asking, but here is a little explanation of what the code says.
G0 G54 G90 X34.0615 Y63.4144 M13 S18000 )G54 is spindle workoffset. G0 is apid move to the x, y location M13 is right hand rotation.)
G43 H12 Z1.748(H43 is height offset for Tool 12 with safe rapid of 1.748)
G0 Z0.998(Rapid movement to "rapid down to" value of Z0.998)
G1 G42 D2 X35.3115 Y63.4769 Z0.373 F175. (G1 linear feed G42 right hand cutter comp D2 is comp value for tool x,y,z are target positions)
X46.124 F352.5 (target position in X)
Y63.2278 (target position in Y)
X24.499 (target position in X)
Y63.4769 (target position in Y)
X35.3115 (target position in X)
X35.8105 (Lead out in X)
G40 X37.0605 Y63.4144 Z0.998(G40 cancels cutter comp while exiting the board)
G0 Z1.748 (Back to safe Z level)

Hope any of that helps.

7/17/21       #3: Omnitech or Anderson Selexx Pal ...
Mike

After rereading your post, maybe I didn't answer your question correctly. I will post a picture of the route when I get back to work on Monday.

7/19/21       #4: Omnitech or Anderson Selexx Pal ...
Mike

Here is a graphic of the tool path. Rectangle with lead in and out.


View higher quality, full size image (1399 X 755)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    ecabinet systems.com Thermwood Limtech Industries, Inc.
    Sponsors
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Scarlett Machinery Inc.
      New and Used CNC Routers and Used Woodworking Machinery, for Operations Ranging From Small Woodworking Shops to Large Progressive Manufacturing Plants
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Tooling on the Web
      Tooling and Tooling Accessories - Free Re-Sharpening for Qualifying Tools
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Advanced Machinery Automation
      Customized Multirip-saws, CNC drilling and milling machines; Service and Support for Cosmec machines
    • MachineryMax
      New and Used Machinery for the Professional Woodworker
    • Felder USA
      High Quality Woodworking Machines and Tools
    • W. Moore Profiles, Ltd.
      Supplying Knives and Cutters to the Woodworking Industry - Standard and Custom Profiles Available
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • Machinery Associates
      Used Woodworking Machinery marketplace
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!

    Become a Sponsor today!