Cabinet door panels

2/15/22       
Scott

I started building my own cabinet doors, mostly 5 piece, I have most of the equipment required and although the first few sets cost about $200 per door, haha. I have got a pretty good system in place.
I have a shaper cutter for running the 3/8 mdf Center panels through to get the rebate or whatever the proper term is on the back. It has a nice radius so the panels look good when you open up the cabinet.
I cut the panels on the cnc and then run them through the shaper. Is there a tool that anyone can recommend to do this rebate cut on the cnc at the same time, this would save time.
Thanks for any thoughts.

2/15/22       #2: Cabinet door panels ...
Mark B

You lost me with "or whatever the proper term is"? WTF dude? Are you trying to come up with a tool to do a back side relief? Coved? Sketch? What in the world are you doing at 200 a door and a line like "whatever the proper term is"? Holy macarolly.

2/15/22       #3: Cabinet door panels ...
Scott

MarkB,

I always look forward to your posts, I had to laugh that you were so hard on me.
Sorry I had a brain cramp, trying to do to much at once.
I am looking for tooling to make the relief cut in the panel, using the cnc.
I was joking about the $200 per door, they just cost more than buying them would have cost, but schedule and quality have been a bit of an issue since Covid started. Thanks


View higher quality, full size image (4032 X 3024)

2/15/22       #4: Cabinet door panels ...
Jared

You can do the back cut on the CNC a few ways. If you want the reverse raised panel look like your pic shows, it'll take 2 tools: your straight cutter to hog out most of the rabbet (rebate in Europe, rabbet in US, potato poTOHto), then follow up with a bullnose running a centerline cut on the edge of your rabbet to create the scallop. Or do what I do, which is to skip the bullnose and make an extra wide rabbet so it creates a 1/8" reveal and leave it at that. Spaceballs in the panel groove help center the panel so the reveal stays even.

2/16/22       #5: Cabinet door panels ...
Richard

Hello Scott,

Firstly I have to ask why you don't want to make these doors as one piece MDF? I know that the back wouldn't match a traditional 5 piece door but it seems like the savings in machine and assembly time would significantly reduce your cost which your customers may appreciate more than they value the 5 piece aesthetic.

If you are committed to producing a door that looks like a 5 piece door, you might consider making a 2 piece door. For shaker profiles similar to the photo you posted it would be very simple. You would cut a frame from 3/4" MDF. This would have a 3/8" deep rebate around the inside of the frame, "squared up" with a 1/8" or 1/16" diameter tool. Then cut your centre panel from 3/8" MDF using a ball nose tool in the way Jared explains. These panels should be cut around 0.01" smaller than the opening and have a radius in the corners that matches the radius of the tool used to cut out the rebate in the frame. I have found that these fit so snugly it's hard to tell that it's 2 pieces. This method is very simple even without costly software. You can easily draw up a template in any free CAD program and stretch to the required sizes before importing into your CAM software and assigning tools. There would be a slightly reduced yield compared to your 5 piece door and a small radius on the inside corners but your assembly and machining time should be greatly reduced.

I understand if you're set on your 5-piece concept but I figure it's always good to look at other options even if you end up rejecting them.

2/17/22       #6: Cabinet door panels ...
Scott

Thanks for all the input everyone.
Richard,
Do you have a picture or a cross section of the two pieces, thanks

2/17/22       #7: Cabinet door panels ...
Mark B

Im in the 5 piece camp and will likely never go to one piece MDF doors but Im not chasing the home center market and most of my customers are MDF averse out of the gate even though it shines where it shines. I think the doors Scott is making are far and away higher quality than a routed MDF door. We all moved away from the particle board/foil horror show in the 80's and now we are going right back. Its not to say there cant be some quality there but we all know why MDF is reigning and its not quality its price.

One knick/dent/scratch in the finish with MDF and your in the death spiral of moisture/swell/hell. The panel is a bit less susceptible to damage so its a bit more manageable but in my world a customer looking at a shaker door with wood grain telegraphing through on the rails/stiles/and panels, will choose that over a dead flat home center door all day long until you can offer the dead smooth door so cheaply they will give in.

I'd stick with your 5 piece if its what your customers appreciate.

2/18/22       #8: Cabinet door panels ...
Acctek  Member

Website: https://www.acctekgroup.com/index.html

Try to make it with a CNC engraving machine with automatic tool changer

2/21/22       #9: Cabinet door panels ...
Tyler Member

Just get this cutter. We use it all the time when making out door panels. Works perfectly.

https://www.amanatool.com/rc-2485-cnc-insert-nova-system-cove-raised
-panel-for-mdf-wood-cabinet-doors-1-11-32-dia-x-17-64-x-1-2-inch-shank.html


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Onsrud Cutter Vortex Tool Company T-Tool USA
    Sponsors
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Scarlett Machinery Inc.
      New and Used CNC Routers and Used Woodworking Machinery, for Operations Ranging From Small Woodworking Shops to Large Progressive Manufacturing Plants
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • Weinig Group-USA
      Wood Moulders and Knife Grinding Equipment
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Tooling on the Web
      Tooling and Tooling Accessories - Free Re-Sharpening for Qualifying Tools
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers

    Become a Sponsor today!