Subject: Re: High gloss with staining powder and qualosole

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

High gloss with staining powder and qualosole

10/5/16       
Michael Member

Hello,

I was touching up the edges of some worn glossy black polyester furniture with Qualasole. The result appears matte. Is there any way to bring this to a high gloss? I mixed in some black staining powder into the qualosole and this resulted in a matte mixture when it dried. If I buff it out will it become glossy? (I am still waiting for it to dry)

I've seen this done in a professional shop and I am trying to duplicate this edge touch up technique. Should I rather use Lubricite 77 or Layover or Shellac for better results?

Thank you for any advice.

10/5/16       #2: High gloss with staining powder and ...
RobertJ

Mohawk makes a rubbing compound lubricant for achieving different gloss levels.

I have used 'Level II', # M730-1016 with good results and can achieve a 40 Degree sheen....Level III may do the trick.

10/5/16       #3: High gloss with staining powder and ...
rich c.

I suggest using Mirka Abralon.

10/6/16       #4: High gloss with staining powder and ...
Michael Member

Thank you Robert and Rich for your suggestions,

Today I buffed out the qualasole and the area around it to a nice gloss - except the one worn edge where I applied the qualasole. Obviously I am missing a step somewhere with the qualasole. I would like the repaired area to be glossy like the rest of the furniture. The qualasole with the black staining powder does not buff to a gloss. I used an electric buffer as well as Meguairs hand polishes and yet it will not become any glossier.

I think the black opaque staining powder causes the result to be matte. Is there such a product as a gloss staining powder? Or should I put a clear coat of qualasole over the repaired area to make the repair glossy?

Thank you for any suggestions,

Michael

10/6/16       #5: High gloss with staining powder and ...
DanShaf Member

Lubricite is a favorite among the NYC area touch up technicians because it's sold by Industrial Finishing Supply in Brooklyn. It's similar enough to Qualosole, they're both padding lacquers.

Your issue is that your granules of pigment aren't being "wetted out" by your padding lacquer. That means that the pigment particule isn't being completely surrounded by the coating because of the lower resin content of the coating (less body).

Mohawk's Lacover comes in their #30 and their heavier body #50.

Your other issue is using a padding lacquer --any padding lacquer, including straight shellac mixes-- over polyester. You might squeeze by with an acrylic lacquer brushed on, not finger padded, but at some angles it'll still show.

Also, instead of fresco colors (Blendal powders), use a powdered dye from Lockwood. The powder dissolves in your touch up coating instead of it hanging in suspension and needing to be wetted out. Then, as had already been suggested, polish your touch up. I would use a forgiving polishing material such as Meguires Mirror Glaze #3. Use Mohawk's Trace Cloth or a microfiber cloth to polish, wrapping the cloth around your finger.

10/6/16       #6: High gloss with staining powder and ...
Michael Member

Thanks so much Dan!

This is really helpful information and seems to explain what is happening to the repair. I will give this advice a try.

(Before I read your reply, I was going to suggest that perhaps my black staining powder had matte particles mixed into it so that no matter how much I buffed out the qualasole mixed with tis black powder it would always remain matte. However your reply seems to be a much better explanation.)

Thank you!

Michael

10/6/16       #7: High gloss with staining powder and ...
Michael Member

I should add that the reason I used a powder stain pigment which is opaque (powder stain pigment mixed into the qualasole), was because I was concerned with colour fading and see-through issues with dyes. I am not sure if this is true, however I read that dyes are not as opaque and that they could fade. Is this just a myth? If dyes are just as opaque as staining powder pigment (especially black dyes) then yes, that would make sense to just use dyes because dyes naturally seem to dissolve easier into the qualasole. I just was not sure if, over time, the dye would fade, and/or the dye would not be opaque enough to cover the repair area. That is why I was reluctant to use dyes for this repair.

Would I be safe to use dyes without having to worry about fading or translucency problems? (I often have to cover worn edges on furniture)

Thank you,

Michael

10/6/16       #8: High gloss with staining powder and ...
rich c.

Have you tried a last coat or two of just the padding lacquer with no powder?

10/7/16       #9: High gloss with staining powder and ...
Michael Member

Hello Rich,

Yes I just tried this today and it works much better. The matte quality of the powder stain keeps the repair looking matte however if you apply a clear padding lacquer overtop of the repair area (not using powder stain this time) this results is more of a gloss. The trick is to be able to adjust the amount of powder for each repair area and then, as Rich mentions, to add a clear coat over the repair once complete.

I also found some older notes I took recently at another woodworking workshop that suggests the best solution is to use shellac (or Qualasole) with a black dye instead of a pigment for such repairs (along worn edges of furniture). I will give this a try in the next few days however my prediction is that it will apply much easier and certainly look glossier.

Thank you once again!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • EX-FACTORY
      Importer and Dealer of New and Used Woodworking Machinery
    • Apollo Sprayers Inc.
      High Volume Low Pressure Spray Systems
    • SAMES KREMLIN formerly EXEL North America
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Supergrit Abrasives
      Industrial Quality Abrasives Manufactured by Leading US and Foreign Companies

    Become a Sponsor today!