Subject: Re: Dyeing wood all the way through (Ebonizing)

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Dyeing wood all the way through (Ebonizing)

1/20/18       
Greg Aanes  Member

Website: chairsnw.com

The uesed to be a product based on Maple which was dyed all the way through, then there was one based on Radiata Pine, but both are no longer on the market.

We have experimented with multiday soaking of 1/4" soft maple strips in various dyes but the penetration is no more than .06".

Pressure dyeing? Is there any experience out there with accomplishing this?

The longest pieces must be 48".

1/20/18       #2: Dyeing wood all the way through (Eb ...
rich c.

I'd say you need a hard vacuum to replace the air in the cells with dye. Probably boiling hot dye at that. I've only seen this done in veneer. Are you carving it since you want full color throughout the piece?

1/20/18       #3: Dyeing wood all the way through (Eb ...
Greg Aanes

No carving, it gets sanded flush to the table top.

1/20/18       #4: Dyeing wood all the way through (Eb ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

You will have to consult with people that make UHV Chambers(ultra high vacuum)
on how to do it.
There was a guy in SanDiego that had one that pumped down to -10 atm to the 7th power.
You will not have to go to that deep of a vacuum , but you will have to pull fairly deep to get all air out of wood cells and then inject dye more than likely in a special carrier as some chemicals do weird things introduced into a UHV.
Also get your checkbook handy, my guess is 50k+.

1/21/18       #5: Dyeing wood all the way through (Eb ...
rich c.

Can you just use African blackwood or wenge?

1/21/18       #6: Dyeing wood all the way through (Eb ...
Matt Calnen

My local hardwood dealer used to carry roasted Maple, which changed the color of maple by cooking it. It wasn’t jet black, but blackish grey. My supplier said It also came in pine. I’m guessing this was the same product your looking for.

1/21/18       #7: Dyeing wood all the way through (Eb ...
TonyF

Greg Aanes:

Your description does not indicate the finished dimensions of the ebonized pieces that you need. If you can not use dyed veneer or inlay to give the effect that you need, I might suggest gluing veneer together until you reach the required thickness.

I have sourced 1.2MM nominal thickness vacuum-dyed black veneer sheets in the past; six layers of this would give you a quarter inch, if that is what you need, and the 1.2MM plies should be sufficient thickness to flush sand, such as you would not sand through and reveal a glue line.

Without knowing the specific application, it is hard to be helpful.

TonyF

1/23/18       #8: Dyeing wood all the way through (Eb ...
Greg Aanes  Member

Website: gregaanesfurniture.com

1.2 mm dyed veneer would be great! The strips we lay in are .375" wide x .1875" tall (deep). In use the .375 dim is across the face of the table, .1875 is the depth into the slot, allowing .0625 to sand off.
Does the dye in veneer affect the adhesion when gluing in to the slot?

We went through a phase of using roasted Maple and R. Birch a few years ago when one of our chair customers was making their tables with it. The roasting process affects the wood such that it splits and cracks randomly. The inlay on the table tops does get a small bend into the slot and the Roasted woods tend to pop apart with even a slight stress. Nice look though.

RE Blackwood or Wenge: Twould look great but doesn't that bring me back to the adhesion issues as with Ipe? What is needed is a temperate hardwood with its softer and more porous structure and a Dark color (Walnut isn't dark enough).

1/23/18       #9: Dyeing wood all the way through (Eb ...
Steve Juhasz  Member

Website: http://www.centrestreetmillwork.com

There are no adhesion problems with Wenge. Titebond II does a great job gluing wenge to itself or other species. Have lots of experience with this. The very porous appearance may be a problem however.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)