Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Turbine hvlp spray set up

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Turbine hvlp spray set up

12/20/18       
Dan Bloomer  Member

In the past I have had a well set-up spray rig with DeVilbiss hvlp guns, a pressure pot and a spray booth.

Time and tide find me with a much smaller shop, no spray booth or equipment, but happily not much need for it ----until, perhaps, now. I've taken on a project whereby I'll need to satin or matte finish the parts produced from about 40 sheets of 3/4" walnut - mdf core. We'll be able to finish 95% of this horizontally. The compressor I have now is incapable with keeping up with a conventional spray gun, hence I'm curious about a turbine systems. Fuji has a "semi-pro" system for about $500. (Might possibly try connecting it to a cheap Harbor Freight pressure pot) I'll be using a water-born polyurethane. My sources for finish are likely S-W, or possibly Atlantic Plywood. I've used post-cat floor finishes on stair treads (Bona)---and have been real happy with the results rolling or pad applying the finish - that is possible also.

How much slower will this be using a turbine powered hvlp set-up compared to my previous experience? These cabinets will not be getting very hard use but/and I'd appreciate any suggestions for a good fast-drying finish with good build. Any add'l comments welcomed.

12/20/18       #2: Turbine hvlp spray set up ...
kevin

Well not going to get much for $500, my experience with turbine rigs was not great, personally I would not waste any time on them again. The turbine is compact which is nice, but the sound of a jet engine in the background always made me feeling rushed. You will also be tied to a gravity cup or siphon setup making the gun very heavy with prolonged use, as all your material must be attached to the gun, also the 1" diameter hoses are like fighting a python!!

Further the turbines create heat, so your basically blowing hot/ warm air onto your project, effectively drying out the film as you move across, not the best for waterborne...

In my view I could spit on the substrate and get a better result. We currently shoot a Kremlin AAA, only my two cents.

Good luck

12/20/18       #3: Turbine hvlp spray set up ...
Stefano

I agree with Kevin about the noise, big pipe of the turbine. I used a couple but as soon I was able I switched to compressor but if you are using the turbine occasionally they are not so bad. I guess the $500 one is just 3 stages and if you can I suggest to buy the 4 stages that allow you to spray thick material like pigmented lacquer. If you just spray clear the 3stage will be ok

12/20/18       #4: Turbine hvlp spray set up ...
Ken Member

Dan, I was doing what you're suggesting, a pressure pot feeding a turbine gun. I set up a Wagner Capspray and was spraying acrylic lacquer with good results. I'd be surprised if you can find a pro gun & turbine for $500, probably $1000+. What about upgrading your compressor instead of a new setup.

12/21/18       #5: Turbine hvlp spray set up ...
robert johnston

Have somebody come in with a portable (on a cart) Kremlin and finish them in your shop.

Put an ad on Craigslist.

If you are attempting to spray a full 4 X8 sheet of Walnut with a turbine, it is not going to happen.

12/21/18       #6: Turbine hvlp spray set up ...
Adam


Dan,

Bona is for floors.

(40) sheets of 3/4" walnut will cost a couple of bucks to mess up.

If you don't have the facility to finish it properly, why not out source? I'm guessing you don't have the room for a dust free spraying area either. Nor a decent exhaust fan. There will be a ton of dust settling on a 4x8 sheet.

I feel your pain about a small shop. I started in a similar situation a long time ago.

12/22/18       #7: Turbine hvlp spray set up ...
mike j

Turbines are loud and heavy. Kremlins are the way to go if able. I would recommend using a new airless pump or a clean airless rental. Wishing you the best of luck and the happiest of holidays.

12/23/18       #8: Turbine hvlp spray set up ...
robert johnston

You may want to try (if you have a small compressor) a low CFM spray gun.
Asturo Eco SX gravity, CAT Jaguar,
or even a Binks Mach 1 with a 94 air cap.

I would only advise the use of the above guns with solvent coatings.

12/23/18       #9: Turbine hvlp spray set up ...
Dan Bloomer  Member

These responses are what I wanted. Especially the feedback on turbines. I'm not interested in plunking out much more than the 500 bucks into finishing equipment --- and that doesn't sound like it would get the job done.

Jobbing out the finishing sounds like the way to go.

5/24/19       #10: Turbine hvlp spray set up ...
Alex W Member

Is this post really old or something? Modern turbines like the Fuji 3 stage will spray water-based finishes perfectly fine.

Compressor spraying wood finishes is pretty archaic from what I read at least.

Anyone mind letting me know what I'm missing?

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)