Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: First Coat with Agualente, then a Latex Paint Topcoat?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

First Coat with Agualente, then a Latex Paint Topcoat?

4/18/19       
dan shaf Member

Can you lay down a first coat with ML Campbell Agualente to be followed up by a latex paint topcoat? Our customers final coat our cabinets with brushed on latex. We spray on the first coats in the shop.

Agualente has a much quicker setup time and it sands easier than rubbery latex.

We try to avoid hybrid systems for fear of failure down the road. Generally, we stand behind our finishing throughout the service life of the cabinet.

4/18/19       #2: First Coat with Agualente, then a L ...
Pat

I think you could get away with it, but why would anyone do this? Agualente is superior to latex in every way.

Why not just deliver them primed if they insist on the latex?

4/18/19       #3: First Coat with Agualente, then a L ...
Brewster201

Seriously why would you top coat with a latex paint? The WB Lacquer dry fast and hard compared to the latex
It's actually a joke to do that
Revise your thoughts

Bruce

4/19/19       #5: First Coat with Agualente, then a L ...
JoeW Member

It is amazing that anyone would want this. But I have seen it. I had one such customer about 18-10 years ago do exactly this.

After, getting MLC's nod of approval, the customer did a very good job using the latex. Apparently, still holding, because I have never received a call back.

Their reason was all about appearance. Had to match everything thing else in the home that was painted with latex. Seems it drove the customer crazy if it didn't.

Today I would turn these jobs away. Far too many customers want the cabinet shop fix all problems or damage, Even if it was their failure or another trades.

4/19/19       #6: First Coat with Agualente, then a L ...
dan shaf Member

Why? Our customers brush paint on their second and final coat. They use latex. They call the shots. We operate according to spec. If they are going to use latex as a final coat, my question is that I'm considering to use Aguelente because for me, going this route makes many things easier for me.

I'm going to get a gallon and shoot it, then lay down a latex topcoat. I was looking to see if anyone else does this.

What our customers like about paint is that they themselves can effect a repair if they want to. They brush on more of the rubbery coating.

4/20/19       #7: First Coat with Agualente, then a L ...
Adam

Almost every cabinet in the mansions were brushed for about 15 years. We loved it. Do a perfect prime job and let the site painters slather oil based Bennie Moore Impervo. Very profitable.

I started using Agualente the first year it came out. Awesome product. The primer is as good as any solvent product. Sands better than most and you can lay down heavy coats.

We would sand them to 240grit and install. Everybody was happy. The oil based paint sticks to that primer fine.

On one of my own big bookcase jobs I had to do a brushed finish. I sprayed the Aguelente. I had my painter use Muralo Ultra acrylic(my favourite house paint. Thankfully he started on some shelves. The Ultra did not like the Aguelente primer.

I would definitely do testing. The mlc primer is not normal. It is fancy pro stuff designed for their topcoats.

I would also stop referring to house paint as latex. It is technically waterborne acrylic. Sounds much better as well. They are more water cleanup than water based.

4/20/19       #8: First Coat with Agualente, then a L ...
Adam

The safest primer to use under any topcoat is Bin shellac primer. It works well on wood. Not the best sanding. Definitively not the best spraying. Tack coat(wait a couple of minutes)and a heavy 2nd cost for a decent thickness otherwise you can get runs or no coverage.

4/21/19       #9: First Coat with Agualente, then a L ...
Nick

I have done this many times for a variety of reasons without issue just test first to make sure there are no compatibility issues.
RE; Primer
Chemcraft Aquaprime is worth looking into. I've been a bin user for over 40 years but this stuff has cut by bin use by 90%. It will go under everything, sands great, dries fast, high build, minimal grain raise even on mdf.and water clean-up.

4/24/19       #10: First Coat with Agualente, then a L ...
mauricio poli Member

Good Morning Dan !
You can do this, there is no problem.
Just sand between coats
Have a nice day

4/25/19       #11: First Coat with Agualente, then a L ...
Wayne Weber Member

A latex is just the dispersion of a non-water soluble phase in water. Latex paint uses a dispersion of solids that are dissolved in a solvent which is then dispersed in water. As the water evaporates the droplets of the solvent coalesce into a film. If you disperse solids in water that is generally referred to as an emulsion.

5/15/19       #12: First Coat with Agualente, then a L ...
Dan Shaf  Member

Thank you all. Regarding Muralo, it's too bad that it was problematic because Muralo is an excellent paint. It's my preferred.

7/11/26       #13: First Coat with Agualente, then a L ...
irtubes  Member

Website: https://irtubes.com/

This is a common question in cabinet finishing. While using a waterborne coating like Agualente as a base coat followed by a latex topcoat can work, the most important factor is compatibility between the two coating systems. We always recommend carrying out an adhesion test before moving into full-scale production.

At I. R. Tubes Pvt. Ltd., we work with specialty chemicals and additives for coatings, rubber, plastics, and related industries. We believe that selecting compatible raw materials and following the coating manufacturer's recommendations helps achieve better adhesion, durability, and long-term performance.

If you're looking to improve sanding properties, faster drying, or overall coating performance, we'd be happy to discuss suitable specialty chemical solutions for your application. https://irtubes.com/products/latex/

Best regards,
I. R. Tubes Pvt. Ltd.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)