Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Alder Finish Too Lite

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Alder Finish Too Lite

10/3/19       
Nick Cook

This is an interesting situation, I looked at a job we're going to match the finish on. It's knotty Alder. But somehow the existing finish on the cabinets is lighter that it would be with just a clear coat of lacquer. It's in an office for an optometrist. No real way for sunlight to hit all the cabinets, that was my first thought, fading. Also wondered if they have a cleaning service constantly wiping the cabinets with something. My question, what might be another possibility for why the cabinets are so light in color? We're working with Red Alder.

Thanks,
Nick

10/3/19       #2: Alder Finish Too Lite ...
Tyler

A white/pickle stain? maybe it was bleached?

10/3/19       #3: Alder Finish Too Lite ...
Nick Cook Member

It's not the pickle stain but bleach is a possibility, I don't think the finisher bleached it but maybe the cleaning crew after finish with a chemical cleaner.

10/3/19       #4: Alder Finish Too Lite ...
Nick

It's possible it's the finish that has turned white-ish as it ages. I've notice this on a couple waterborne clear jobs l've finished. It is very noticeable on jobs finished with Valspar's WB conversion varnish.
You should be able to get a pretty good match (at least in the short term) by mixing up a very thin white or white-ish stain over a wash coat or by toning.
Good luck.

10/3/19       #5: Alder Finish Too Lite ...
Nick Cook Member

Nick I'll pursue that, thanks for the input.

10/3/19       #6: Alder Finish Too Lite ...
Mark B Member

Are you sure the material is actually Alder and not some import material that looks close enough to pass it off as Alder but isnt? Just a thought.

More and more as of late we are being asked to match a stated species that looks spon on but on closer inspection is... not.

10/3/19       #7: Alder Finish Too Lite ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

If your using red alder and you use a thin white over it to try to lighten it. Well red and white = pink. Post some photos so we can offer some real help, not just guess on what to do.

10/3/19       #8: Alder Finish Too Lite ...
rich c.

You sure it's not birch? The two species are related.

10/7/19       #9: Alder Finish Too Lite ...
Shane

very possible it's red birch and not Alder... or possibly built with a light batch of Alder... possibly bleached as well..... bleaching isn't that big of a deal either....

10/7/19       #10: Alder Finish Too Lite ...
Nick Cook Member

To give an update, I was unable to determine wood species, I'm convinced it's Alder, but we added some white tint to our lacquer and with two coats we achieved the same appearance. Another thing I'll add is that we looked at the interior of a door and it was the dead match for typical Alder with a clear coat. The light honey or amber color that car lacquer on Alder gets you. So something was going on with the exterior of these existing cabinets. Not sunlight, could be a cleaning agent, could be the original cabinets were bleached. It's in an optometrists business and I could see them regularly cleaning the cabinets with something that makes them fade.

10/7/19       #11: Alder Finish Too Lite ...
mastercabman

"Another thing I'll add is that we looked at the interior of a door and it was the dead match for typical Alder with a clear coat. The light honey or amber color that car lacquer on Alder gets you. So something was going on with the exterior of these existing cabinets. Not sunlight, could be a cleaning agent, could be the original cabinets were bleached."

Nick
It is very common for cabinets/furnitures manufacturer to only glaze/highlight just the front of doors/drawers
In a way it makes sense because the outside of the cabinet is exposed to everything but the inside is only exposed when the door is open
Glad you got it figured out
Good luck with your project

10/8/19       #12: Alder Finish Too Lite ...
rich c.

No idea how a cleaning agent gets under the clear coat and alters the color of the wood, nor alters the color of a cured clear coat. Wouldn't it need to be very even coating over the entire number of cabinets to change all the colors exactly the same? I know you like the cleaning agent theory, but I'm very skeptical.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)