Subject: Re: Hand sanding efficiency

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Hand sanding efficiency

2/4/20       
pascal stgelais

hello

Since I work on a lot of decorative furnitures and small pieces I do a lot of hand sanding (using block, sponge, hand).

I usually go as fast and press as hard on the block as possible.

recently, when sanding grain filler I begun easing off the pressure since the sandpaper had a tendency to pull the filler out. This also gave me a surface a little bit rougher (with more tooth).

This had led me to think that I may be burnishing my wood even though I don't sand past 150 grit.

I have often read to go hard when hand sanding but would I end up with better result If I use orbital sander like pressure with my block

2/4/20       #2: Hand sanding efficiency ...
scott brady

Take a look at the Surf Prep 3 x 4 sander with foam pads. Will never go back to only hand sanding, much better consistincy and easier on the body.

2/4/20       #3: Hand sanding efficiency ...
Leo G Member

Pressing as hard as you can is a good way to wear yourself out. Letting the paper do the work is what I've been told. But that doesn't work either. You have to go in between the two to make things work nicely.

Pressing hard, especially on corners wears the paper out faster but doesn't get the work done faster. As was said above the sponge sandpaper gives good pressures for most sanding, but not aggressive sanding.

Another thing I've noticed is that lower grits don't always remove wood faster. Especially if you have limited stroke such as small parts or in corners. More grit per inch sometimes is what makes the job go quicker. If you sand with 220 instead of 120 sometimes the more cutting edges will reduce your sanding time. You make have to go back with a lower grit to get the right surface for staining.

Heavy handed sanding leaves deeper scratches that may show in the finish. While lighter sanding won't and that will increase the speed of sanding in the end.

I also have the same problem as you, harder means faster. But it doesn't always work that way.

2/4/20       #4: Hand sanding efficiency ...
rich c.

Abrasives are like any other cutting tool. Let the tool do the work.

2/4/20       #5: Hand sanding efficiency ...
Adam

Imagine you are using a variable speed random orbit sander. You’ve got four variables: grit, hardness of pad, speed of the sander, and how hard you push down on it.

The grit size is typically chosen by how deep a scratch you require. Heavy removal of material 60, epoxy prep 80, joinery smoothing 100, bare wood 150, primer 240, topcoats 320.

Hardness of pad is determined mostly by the shape of or by the material/substrate

Sand faster: sharp abrasive, speed of head or head pressure.

The efficient way is to run the sander or your hand at the highest speed possible. Then apply more pressure as required.

Think about lifting weights. Would rather lift 100 lbs once or 10lbs 10 times?

2/4/20       #6: Hand sanding efficiency ...
pascal stgelais

thanks everyone. I have tried to hand sand using the same pressure when than when I use an orbital sander on some scrap pieces.

the main reason behind this thread is that I have been getting inconsistent results regarding adhesion of my vinyl sealer/cv sealer/cv. I have tried thin coats, heavy coats/ exceding the dft/ staying way below the dft and even then could not get consistent results.

lately I made a few test pieces that were already sanded 120 grit and sanded them with a 150 grit. I wanted to go fast so I just hand scuffed with a 150 grit and to my surprise got fantastic results regarding adhesion of my cv over cv sealer over vinyl toner.

I have investigated and noticed than when sanding with a lot of pressure I something get areas of matte-satin sheen wich I assume must be burnished areas. This happen more with 150+ grits where I sometime end up rubbing the wood with a layer of sawdust clogged paper rather than sandpaper itself.

I am not a wood expert but read a few time that ash can cause adhesion problem if it end up burnished. I come from a softwood background and these woods sucked the finish like a charm even when burnished.

2/8/20       #7: Hand sanding efficiency ...
dan shaf Member

Clogged sandpaper:

Clean it out by using your air gun, or by rubbing the sandpaper against a piece of carpet. You can rub the sandpaper against clean cardboard or against corrugated carboard, against the corrugation itself, but the cardboard dulls the sandpaper quicker than the compressed air or the carpet.

For surfaces that have a coating that's still o0ff-gassing, even though generally cured and ready for sanding, clean the sanded surfaces with a microfiber cloth to rag up the dust. The dust particles become sticky because as a fine particle it has more surface area exposed to off-gass whatever solvent is still part of the finish that had knitted itself together during the film-forming process.

Vinyl sealer is very, very thin. It usually only needs a scuff to create a tooth prior to coating over and not a subtractive form of abrasive removal. As long as their's no drips and as long as your VS is generally smooth, just a quick kiss with the sandpaper or Scotch-Brite is enough to give the VS surface some tooth.

2/9/20       #8: Hand sanding efficiency ...
Jim Clark  Member

Scuff pads clean sandpaper really well.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!