Subject: Re: Looking for Better stain blocking primer

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Looking for Better stain blocking primer

9/16/20       
Joe Haynes Member

Hello all! I’ve been spraying cabinetry white a lot lately. I’ve been using Sherwood Kem Aqua surfacer , a seal coat with Sherwin’s shellac primer and kem aqua plus As the finish. I typically do 2 coats of primer for good adhesive, a coat of shellac for stain killing and two top coats. This is a bulky process for my white finishes. I’m trying to find a product that combines the aspects of the surfacer and shellac. I’m looking for something with, low to medium odors, good adhesive, stain blocking and a quicker dry time. Shellac meets all of these besides the odor. Even wearing a mask with high ventilation it sometimes seems overbearing. Any thoughts?

I haven’t tried them yet but my thoughts are
-Pigmented Kem aqua plus waterborne sealer as a primer.
-kills restoration (max)

9/17/20       #2: Looking for Better stain blocking p ...
Leo G Member

Why do you need a blocking stain? Are you spraying restoration cabinetry or something else not new materials?

What about white vinyl primer. Pretty much blocks anything, pretty equivalent to shellac. Not sure if it comes in a waterborne, I know it exists in solvent. It's not exactly smell free LOL.

9/17/20       #3: Looking for Better stain blocking p ...
Shane Welch

Dude if you can't stand the smell of denatured alcohol....lol Jump into our world of acid catalyzed varnishes ,2K polyurethanes & polyesters..

9/17/20       #4: Looking for Better stain blocking p ...
rich c

Probably 1 coat of M L Campbell's Clawlock II high solids primer will replace all those primer steps. It sure would be worth a try, but you won't like the smell is my guess. Experiment on some scrap of course!

9/17/20       #5: Looking for Better stain blocking p ...
Leo G Member

Clawlock isn't a blocking primer. Take a black magic marker and write on a pc of wood and prime it. It'll keep showing through for 2 coats.

9/17/20       #6: Looking for Better stain blocking p ...
Bart

I use Bin Shellac. You can get by with one coat but two coats gives you a great primed surface especially on big end panels and refer panels etc.... Then I hit it with a 50-50 coat of GF white under coat/whatever white-ish poly I have laying around and then two top coats. Finish product is bullet prood and plush.

Don't hit the first coats of shellac or WB primer hard. Basically a wet spit coat. Knock it down with 320 and then a semi wet coat. Nice thing is the Bin drys super quick and sands easily.

my 2cts

9/17/20       #7: Looking for Better stain blocking p ...
Adam

There are only two staining issues we ever consider. Soft maple and poplar. Some of the dark veins in the soft maple and those green/purple pieces of poplar will leach into the primer coat. We’ve been using MLC Aguelente wb primer and MLC Polystar since the early 2000’s. Amazing product. You can see it lock-in the stains.

9/17/20       #8: Looking for Better stain blocking p ...
Nick

I use a WB finish system for pigmented/ painted jobs and l do much the same as you except l mark any stained areas with a pencil during my first sand and just spot prime those areas with pigmented shellac then spot sand. It won't be a huge time/ material savings, but it will be some.
Also, l'm a fan of chemcraft Aquaprime, get your hands on some and give it a try, you won't be disappointed. And, quit using SW's pigmented shellac and switch to Zinnser's, the better quality will make your work day easier.
I've discovered WB finish systems take more time, effort and (IMHO) skill to get professional results with that yes, aren't as durable as CV or 2k poly finishes but they do make the shop environment a lot more livable.

9/17/20       #9: Looking for Better stain blocking p ...
Nick

PS; ML Campbell makes a WB stain blocking primer called "Arroyo" l haven't used it but it sounds like what you're looking for.

9/18/20       #10: Looking for Better stain blocking p ...
MarkB Member

Why not talk to your tech's at your SW industrial division? They will give you a combo that will meet SW spec's and likely trim down the bulk. If your pulling KemAqua from a local branch just ask them for the contact at industrial and bypass the branch. You'd get far better information.

At least in my area the local branches are useless as **** on a ****. Thankfully we cant even pull KemAqua from them and all must go through industrial and they know the product(s) inside and out.

9/18/20       #11: Looking for Better stain blocking p ...
Terry V Member

Website: woodshoponshilling.com

Try General Finishes "Stain Blocker Primer". Developed for exactly the application you're describing. I have used it on new cabinets under white finishes and it works great. Not cheap, but it works.

General Finishes Stain Blocker

9/18/20       #12: Looking for Better stain blocking p ...
MarkB Member

At almost $40 a quart for a stain blocking primer thats insanity. We are right at 100 for 2K clear. Primer, no way.

9/18/20       #13: Looking for Better stain blocking p ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

both chemcraft aquaprime and mlc agualente plus primer will do this in two strong coats by themselves. I had an issue with the agualente primer for a while, with cratering on the second coat. turns out my solution was to not sand between the coats and shoot back to back. I dont like doing this with the aquaprime because its more tough and doesnd sand as easily. The euro brands of waterbased have gone to a two part to solve tannin bleed ect... I agree that the general primer is too expensive for use on cabinetry and millwork.

9/18/20       #14: Looking for Better stain blocking p ...
Terry V Member

Website: woodshoponshilling.com

Not sure if you're referring to my post above on cost but I assume you are. I don't pay any where near $40.00 per quart. ( for that matter who would buy it by the quart??) I must have better sources than you. It's not for everyone of course. I refinish existing kitchens and sometimes they are red oak. I would never spray white over these cabinets without using GF Stain Blocker first. It absolutely eliminates tannin bleed through.
The OP wrote: "I’m trying to find a product that combines the aspects of the surfacer and shellac. I’m looking for something with, low to medium odors, good adhesive, stain blocking and a quicker dry time". That exactly describes GF Stain Blocker. There seem to be a lot of finishing snobs on here that are "no-it- alls" and won't allow others to have an opinion without attacking. Probably why more people don't post. Who would??

9/18/20       #15: Looking for Better stain blocking p ...
Mark B Member

Even at 90-100 a gallon, forget about freight if no local stock, thats super steep for primer. Thicken up that skin bub.

10/9/20       #16: Looking for Better stain blocking p ...
Tomaszg Member

How is Aquaprime as a primer instead BIN shellac??

10/12/20       #18: Looking for Better stain blocking p ...
JaySun

MLC has a new Universal WB Primer that seems to be doing well. Tannin blocker and nice white color. Can be top coated with wide variety of products. W41259 is product code.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!