Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Spraying Conversion Varnish

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Spraying Conversion Varnish

3/19/22       
howard Member

Website: http://woodcontours.net

1) What needle should I use, I'm using a Mohawk product?

2) Spray pattern - is it the same when spraying lacquer, going first in one direction and then going at 90 degrees? Do I need to be careful with overlap?

3) How sensitive is it to temperature and humidity? I'll be able to keep the temp at around 70 degrees, humidity I can't control.

Thanks as always.

3/19/22       #2: Spraying Conversion Varnish ...
Leo G Member

What are you spraying with?

3/20/22       #3: Spraying Conversion Varnish ...
Kevin Dunphy

Website: http://www.kdunphy.com/

Your 2nd question is hard to answer it screams I don't know the basics.
Get experience the best is to get a kitchen door spraying job, having a good hand is number one skill to learn.
Mohawk has lots of videos learn and watch the hand also Youtube but find experienced guys not want a be.
I've almost finished a high gloss video showing burled elm from a 1991 MG .
Also, there is no stupid question just spend a little time first

3rd question high heat is an enemy when spraying can bubble on certain lacquers had it happen on conversion varnish

3/20/22       #4: Spraying Conversion Varnish ...
Leo G Member

Don't know about Mohawk. But ML Campbell always states 25ºC (77ºF) which of course is very warm but heat will generally not cause solvent pop. Air currents over the wet substrate are usually the culprit for solvent pop bubbles.

3/20/22       #5: Spraying Conversion Varnish ...
Mastercabman

So for your first question,we need to know more
What exactly are you using and what kind of spray equipment you're using

For the second question
Start at the edge (center of fan)
Then go back with a 50% overlap and so on

For your third question
Ideally most finish is based on 77`/ 50% humidity
Don't spray under 65`
If it gets too warm,start to use flow enhancer to slow down the drying

3/23/22       #6: Spraying Conversion Varnish ...
Kevin Dunphy

Website: http://www.kdunphy.com/

Here is the video of high gloss clear it's good to understand the process and can change the look of a furniture guy.
What I see a lot in videos is guys flicking their wrist not keeping the arm straight and understanding why that is a huge difference .
I had someone come in the shop wanting a job as a finisher that never sprayed vertical but wanted to learn at my shop at 22dollars an hr. only because where he's working there dumbing down the work making everything flat.
I was lucky enough to work a few years in aircraft executive jets doing high gloss finishes that were polished.I had a car finisher that worked there helped me a lot to learn proper spray techniques were not born with the gun in our hand.
Also, that experience taught me to be so careful with my health these chemicals are no joke

https://www.youtube.com/watch?v=OrKlWt06aZE&t=15s

3/23/22       #7: Spraying Conversion Varnish ...
Christopher Tayler Member

Use a 1.4-1.6 tip and I start thinning the CV at 10%. On humid days I add C1161 retarder. Start it at 1-2% and no more than 5%.

3/25/22       #8: Spraying Conversion Varnish ...
JeffA

So Kevin Dunphy, did you hire the kid?

3/26/22       #9: Spraying Conversion Varnish ...
Kevin Dunphy

Website: http://www.kdunphy.com/

No there was another flag he told me he didn't like the wear and tear on his vehicle I was only 10 mins away from home and where he worked was an hr. away. Plus my shop isn't geared for a full-time finisher.
I need someone that can install, prepare wood, assemble cabinets and learn the CNC. Still waiting for someone that can fit, hard because the shops in the area think it's it better to keep the workers one dimensional [example head installer, head sander, head assembler ] I think it's so boring for the workers. I don't think you can be a cabinetmaker unless you can spray, install and design.
I know the only way is to have someone that is young, green and to train.
But were in a time of great exchange of ideas thanks to the computer I learned how to run the CNC on Shopbot form 13 years ago the sign guys opened my eyes.

3/27/22       #10: Spraying Conversion Varnish ...
JeffA

The larger kitchen cabinet factories here in MN are paying at least $20.00 an hour to start and $22.00 and more if 2nd or 3rd shift. When I see a person that all they do is blow off sawdust on parts before finishing and are paid that amount I'm just flabbergasted. You can still find 1 bedroom rentals for around $500 per month that also include heat here. It's just crazy.....

3/27/22       #11: Spraying Conversion Varnish ...
Kevin Dunphy

Website: http://www.kdunphy.com/

That larger kitchen cabinet factories also has a couple of designer who talk about craftmanship.
I was hoping with CNC being affordable there would be more guys doing real custom work so you don't have an old man yelling at the sky.
I have a new video out on cabinet material basic construction hoping someone like Dave does a video
The sad thing is when someone walks out of those big factories in 10 years they have zero skills the only place they end up is at the big box stores selling kitchens.

3/30/22       #12: Spraying Conversion Varnish ...
tiptop

I'm not sure we're comparing apples to apples here. Mr Dunphy is located in Canada so I'm thinking rates of pay may not be equal. That said, you will definitely not find an experienced finisher in the mid-Atlantic states for $20-22 hr. Of course, you're not going to find any apts. at $500 month either.

I'm in agreement with Chris Tayler in his points; also taking into account that he's speaking from experience. Have a great weekend!

4/1/22       #13: Spraying Conversion Varnish ...
Kevin Dunphy

Website: http://www.kdunphy.com/

That wasn't the point the 22 an hr. The skill level is dropping in cabinet making. My son makes almost 6 figures I can't afford him he won't be running the shop and his girlfriend is looking at 6 figures teaching at the university. I'm well aware of the wages in today's world
You look on Youtube is full of people who never spent one minute in a cabinet shop giving out cabinet-making advice. The experienced shop is going the way of the dinosaurs for lots of reasons mainly so expensive to open a shop even a decent 4 man. I grew up in Toronto so I've seen crushing rents firsthand.
So there is a big hole for mini-factory shops all advice is given by salesman selling equipment. Hence all you need is min wage workers so the cycle of skilled workers is accelerated.
Sorry if I hijack this thread just wanted to make a point
Also, I have a new video on the subject

https://youtu.be/_OoGaDuMWJU

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • SAMES North America Corporation
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More

    Become a Sponsor today!