Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Stacking finished 4 x 8 panels

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Stacking finished 4 x 8 panels

9/15/22       
Jared

I'm making a batch of MDF wall panels that will be painted with a dark pigmented satin 2k poly. When it's finished, it'll be a good sized heavy stack that gets delivered a half hour away. I've not had to load and transport this many fully painted sheets before, and have concerns about the weight and truck ride causing abrasion. Panels will be cured about a week before stacking. I'm thinking about slipping a sheet of kraft paper in between each panel. Overkill, or not enough?

9/15/22       #3: Stacking finished 4 x 8 panels ...
Leo G Member

I always put something between panels. Usually I have a good stack of cheap harbor freight moving blankets for protecting most things I transport. How about the thin bubble wrap cut up into squares and put about every 2'.

9/16/22       #4: Stacking finished 4 x 8 panels ...
RichC

Kraft paper is abrasive. Some turners use it to polish the finish on parts on a lathe. As mentioned, shipping blankets should have been added to the bid.

9/16/22       #5: Stacking finished 4 x 8 panels ...
D Brown

Maybe you could stand them up ?

9/16/22       #6: Stacking finished 4 x 8 panels ...
Kevin Dunphy

Website: http://kdunphy.com

What Brown said keep it simple

9/16/22       #7: Stacking finished 4 x 8 panels ...
Leo G Member

I thought of that too but decided that while the panels are being transported the up and down movement was more likely to scratch the faces than if they were laying down.

9/16/22       #8: Stacking finished 4 x 8 panels ...
Kevin Dunphy

Website: http://www.kdunphy.com/

I think the danger is the weight once you have 4 or 5 sheets stacked acts like a press

9/16/22       #9: Stacking finished 4 x 8 panels ...
Josh Koschak

It is only being transferred a half an hour away, put them on edge with blankets in between, or make multiple trips. How many sheets are you referring to?

9/16/22       #10: Stacking finished 4 x 8 panels ...
Mark B Member

I'd agree with shipping them on edge. Even with some curing time with the weight of a stack you'll risk damaging the finish or even worse something sticking.
Not sure of your capacity or the quantity but even cutting a sheet of MDF in half and either plowing some slighty spaced dado's or some battens and screwing them to the ends of the panels so they can ride on edge spaced apart would seem simple enough.
Shipping is one of our biggest nightmares and even on short rides its amazing what the vibration/abrasion will do to finish. Sticking even with curing time is an even bigger nightmare.

9/16/22       #11: Stacking finished 4 x 8 panels ...
Leo G Member

2K poly is fully cured in 3 days.

9/16/22       #12: Stacking finished 4 x 8 panels ...
Mark B Member

Agreed on the cure time. I'd just personally still be cautious depending on the size of the stack. Add to that loading and unloading and the potential of sliding sheets stacked on top of one another and I'd be running them vertical by default. Separating them with furniture pads is fine if theres not a ton of sheets. Im even cautious loading and unloading pressed panels of HPL as one piece of grit and your scratched. With the cost of 2K finishing a quantity of 4x8 panels I'd be handling them with kid gloves to avoid any and all headaches.

9/16/22       #13: Stacking finished 4 x 8 panels ...
Jared

Thanks for the input everyone. I was hoping to load & unload in a forklift-friendly manner on an 8' pallet, as these will be ridiculously fragile. It's about 40 sheets of 3/4 MDF with curved 1/2" deep grooves going every which way. Stacked flat, the bottom sheet would have about 3700 lbs sitting on it...too risky. Final vote is hand loading on edge with blankets as spacers, 3-4 days after the last one's shot. Leo that was my understanding on cure time also. Fortunately I'm not the one that has to thread them down a spiral staircase to the final destination: that's an official SEP (Someone Else's Problem).

I've had moving blankets print on painted surfaces in the past, but it's probably because they weren't pristine, and also because that particular time we were shipping a truckload from Washington to San Francisco goes over a section of I-5 in northern CA that sets up some brutal pogo stick resonances between truck suspension and concrete.

Anyway thanks for taking the time to volunteer your ideas.

9/16/22       #14: Stacking finished 4 x 8 panels ...
Mark B Member

Ive had the imprinting issue as well but would never risk it on a 1.5 ton stack. If your wanting to fork it I would be using a large 4x8 pallet like 3Form or solid surface lands on and a couple half sheets dado'd and screwed to the ends or even just web-strapped in a pack. You could probably get 30 sheets on a single skid standing on edge that could be forked off. The effort of safely palletizing the load even for a short haul would be well worth the peace of mind. Even if one sheet gets biffed your in the hole.

9/16/22       #15: Stacking finished 4 x 8 panels ...
RichC

Any commercial glass companies near you? They get big sheets of glass coming in vertically stacked on skids all the time. I picked some up this spring for a gardening project. Well made and usually free.

9/18/22       #16: Stacking finished 4 x 8 panels ...
Quicktrim

Two pallets , 20 sheets each pallette, with foam sheet between each layer. The rolls of foam are about 300 each around here for 4' wide .

I don't remember how many feet per roll but I keep a couple rolls on hand at all times .

Depending on the pattern of the routing this may or may not work well, but would enable them to be fork loaded and off loaded which would save a good amount of time .

12/12/22       #17: Stacking finished 4 x 8 panels ...
Jon W Member

Check with warehouse packaging suppliers and get a couple rolls of 48" wide, 1/8" thick poly foam to layer in between. Then bundle or strap them down to the bed with extra cardboard corners on top to make sure they don't move when the truck bounces. We've done many large panel and steel door projects this way that are transported hundreds of miles away without ever having an issue. To save on foam, as I am assuming the panels are finished on one side only (wall panels), go back to back, face to face, with foam only between the face to face parts.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!