Subject: Re: Bleaching raw maple

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Bleaching raw maple

10/6/22       
Julie Member

We have occasional issues with our 2 part bleach where raw maple is yellowing when bleached. The wood is freshly sanded and had no ambering any ideas on how to neutralize tannins or is it something else? Thanks


View higher quality, full size image (3264 X 1836)

10/7/22       #2: Bleaching raw maple ...
chemmy Member

If your using 2 part bleach, which I surmise that you are, the mistake most people make is mixing the two together and making a single application and the neutralizing with common 5% white vinegar ( acetic acid). To rid yourself of ending up with the yellowing, which is caused by the reaction of the vinegar on the lye/ sodium hydroxide, causing the excess lye residue to turn color.!
If you instead make a two part seperate application of the lye first, letting it darken the as much as it will, then after it is surface dry, wash of the excess lye with clean water and rags, etc., and then apply the hydrogen peroxide/ bleach, and let it surface dry before neutralizing the lye with the vinegar, that should solve the problem.! If you still have the problem, after doing this, get back to me with what is happening ok.? It may be necessary to thin the vinegar or the lye, but try this first ok.?
Sincerely,
Chemmy

10/7/22       #3: Bleaching raw maple ...
Julie Member

Thanks Chemmy! Will give it a try.

12/5/22       #4: Bleaching raw maple ...
Mike

Chemmy,

I’m a bit confused by your process….

So there’s a way to remove the yellow from Maple and make it more “white”?

So is that possible by applying part one wood bleach, then part 2? If so, how long after part one?

Anything else get mixed with either part?

12/5/22       #5: Bleaching raw maple ...
chemmy Member

Hey MIKE, I thought I was pretty clear on this, but will respond anyway.!
First off, the sodium hydroxide, aka ( Caustic soda or lye,) [part 1 of the 2 part bleaching process] when applied to any common woods and most if not all uncommon woods, burns or darkens the wood it is applied to by varying degrees, depending on the tannins in the wood..ok?
Hydrogen peroxide, is actually the chemical that does the lightning/whitening, of the material it's being applied to.! It accomplishes this by an extra molecule of "nacent" oxygen, ( A litely attached molecule) being present in the chain, which when given up will lighten the area it is applied to.
Though you can achieve a good result from mixing the part 1 and part 2 chemicals together and applying them to the wood surfaces, the problem is, especially on woods that are pretty light to begin with, such as maple, birch, etc., is that all of the caustic part 1 lye, may not be fully neutralized or spent, in the process.. Which means that there is or may be tannins still present in the wood surface that are still active, and capable of showing up as a mild to medium yellowness, after the neutralizer, ( acetic acid/ white vinegar) is applied to neutralize any remaining tannins that may be present on the wood surface.! Showing up as a yellowish color, ok.??
On the otherhand, if the two components (1+2) are applied separately, and each is allowed to surface dry in between applications, the excess tannins can be removed from the part 1 lye application independently, simply by using clean water and white rags. This insures to a high degree, that when the surfaces are then surface dried again and the part 2 bleach is apllied...(hydrogen peroxide) that when it is fully dried that the vinegar will not act to leach out any unspent tannins that would exist in a one time application of the parts 1+2 being mixed together and applied simultaneously in a singular procedure.!!!
The main thing to understand in this subscribed process, is not to wait till the wood surfaces are completely or thoroughly dried, but just to where no part of the surfaces still look wet, before washing the surfaces with clear clean water and white rags, the rags are needed to see and show if any off white residue is being picked up/ removed from the surfaces...ok.? If, and when, no color is being removed from the surface, then the peroxide (part 2...can be applied and again when surface dried and the vinegar can be used without concern with it turning the wood yellow. If by chance it still turns yellow, it would only be because the concentration of the vinegar is to high.! Usually in this case I outline, if the tannins are virtually all removed, their is no need for a 5% solution of vinegar being needed, A one or two percent solution of vinegar would be more than sufficient.!!! There is also what I deemed back in the late seventies, A method I called " Hyper-Bleaching" which introduces an even whiter final product on the wood surfaces....but much caution is needed in using this method which is done with high heat.!!
I can give you little more help or understanding in this Mike, I hope this time I made myself much clearer in understanding this process, and that this can be used on virtually all woods, not just light colored woods ok.?
Sincerely
Chemmy

12/12/22       #6: Bleaching raw maple ...
Jon W Member

I have found that after bleaching/neutralizing, treating with oxalic acid should solve the problem.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!