Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Water base stain on natural cherry

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Water base stain on natural cherry

3/30/23       
Al

Anyone have a water base stain that makes natural cherry pop like a solvent finish? I have bedroom end tables and dresser that I plan on spraying 2k waterborne on cherry. I have done waterborne on cherry with Zinsser seal coat but never 2k. Chemcraft rep told me to use a water base stain. Anyone know of a stain out there that gets the look of a solvent finish on cherry?
Thanks,
Al

3/31/23       #2: Water base stain on natural cherry ...
chemmy

The requested answer as to wanting to find a water based "stain" that will give the " appearence" of a solvent based clear finish is a contradiction in and of itself.! Stains don't determine the color of the clear coat as to appearence. If you use an amber ish clear coat, it will have a final amber appearence if it's water clear, then it will have that appearence, etc.! Secondly, no matter what stain or sealers or top coats you choose to use, the cherry on it's own will naturally darken to a fairly large degree.! I think what the rep gold you was meant to steer you away from using oily or urethane type stains such as what you would buy at the big box stores.. Minwax, etc., which could possibly cause adhesion problems for the 2K.!!
If your looking for an amber type tone to your project, you would be best off by tinting your clear coat with a comparable color ant to your desired amount of amber news you desire.! Just a suggestion.

3/31/23       #3: Water base stain on natural cherry ...
nicko

You could spray a light coat of the Zinsser seal coat over the stain to give it that solvent look and then the waterborne

3/31/23       #4: Water base stain on natural cherry ...
Al

Yes cherry darkens however it is a different look with a waterborne product. I asked rep specifically about Zinsser seal coat over cherry, nothing said about Minwax or box store stuff. The rep knows I won’t be staining. I have used seal coat for over 20 years but never under 2k waterborne. When I use seal coat I mix 2 parts seal coat, 1 part denatured alcohol.

3/31/23       #5: Water base stain on natural cherry ...
chemmy

Al, to each his own.! All I am saying is if u want the same amber affect, then tint your 2K, to approximate what your getting with seal coat, no..it still won't give u the same exact appearence, but it will be close... As to staining with water base dyes, there is the chance still, over time, that the color will fade, but that's your choice.

3/31/23       #6: Water base stain on natural cherry ...
RichC

So far, I've not seen a water based stain that doesn't look like mud. Nature takes care of the most beautiful color on cherry. It would be a sacrilege to put muddy stain on cherry. If your customer insists on color, use a dye.

3/31/23       #7: Water base stain on natural cherry ...
Adam

You can also take transtint dye and add to Sealcoat to making a grain popping dye stain. It's a similar effect to a high quality solvent wiping stain.

In my experience you don't want to change the color of cherry much. If anything you are trying to even out minor differences between each piece of wood. The ability to control the extent of color change using the transtint sealcoat should give you plenty of room to even it out without too much.

If you had only one stick of cherry, it would be stupid to stain it. The natural color is beautiful. Cherry is one of my favourite woods for look, feel, smell, workability. The pain of dealing with sapwood and potential for catastrophic sun damage are its only negative attributes.

3/31/23       #8: Water base stain on natural cherry ...
mauricio poli

Hello ! You can tint you WB 2K with some drops of CHROMAFLO TRANSPARENT YELLOW IRON OXIDE 897-1752

3/31/23       #9: Water base stain on natural cherry ...
Al

I think I was misunderstood or I explained incorrectly. The house the tops are going in have cherry cabinets, cherry trim, cherry interior doors, etc. I know the house well as I made all of the cherry items. They are a long time customer and how I finish the bedroom tops is my call. I finished the kitchen cabinets with cv, the interior doors, trim and other non kitchen items I did with Zinsser seal coat and then waterborne lacquer. No stain was used. When your in the house you really can’t tell the difference between the cv cabinets and the other items I did with seal coat and waterborne. I’m tired of being around cv, the off gassing is something I hate. Plus they have to breath this stuff in their bedroom for as long as it takes to fully cure. I feel like I want to give them something as good as or close to cv because they are table tops. Chemcraft makes a single component clear waterborne that is the best wb I have ever sprayed. I tried this over the seal coat today and I don’t see any compatibility issues so this is probably what I will go with.
What I was after when I posted was to eliminate the seal coat and stain the cherry to match the seal coat and then clear coat with the 2k. In my opinion some woods need the ambering while other woods could do without the amber.
I agree with you Adam cherry is my favorite wood to work with, not real dusty and has a great smell when you cut it and finishes nice.

3/31/23       #10: Water base stain on natural cherry ...
Al

I will check that out. You must have chimed in while I was typing. Thanks

4/6/23       #11: Water base stain on natural cherry ...
Jonathan Mahnken

Website: http://www.mahnkencabinets.com

I would still seal with the seal coat, just so you don't have any tonal differences. The 2k shouldn't work any different than the previous 1k waterbased that you sprayed.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations

    Become a Sponsor today!