Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: finishing time expectations

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

finishing time expectations

3/9/24       
Quicktrim

Website: http://jkinteriorfinishllc.com

Hello finishing experts.

I have only had finishing in house for about two years.

The setup is as follows:

2500 sq ft . global finishing solutions closed face booth, foam suppression, denray downdraft for whitewood and primer / sealer sanding, dust free drying / flash off room, 3 CA tech 14 : 1 AAA pumps, 1 Kremlin eos . lots of carts and racks, air random orbits adn 3x4 square sanders.

So not the most advanced setup but what I could afford at the time.

Currently using ML products , Claw lock for primer , Klearvar for stain topcoats, woodsong for stains , stealth for color topcoats.

My question is how ling should it take for a kitchen to get sprayed start to finish ? I am talking average kitchen , shaker doors, MDF or 5 piece maple with MDF panel. Average 25 - 30 cabients so 40-50 doors and drawer fronts, a couple reffer end panels , five sticks of crown backer and five sticks of crown , five to eight toe kicks, a few fillers.

Currently my guy spraying has experience but by no means a carrer finisher. They are putting good looking product out but with two guys in there it is taking a solid week to get the finishing done for one kitchen.

Doors come in from Cal door so pretty clean to start with. Does 80 man hours seem excessive for finishing this amount ? seems to be taking quite a bit longer than I am comfortable with.

I appreciate any insight that you carrer finishers have as I want to make the finish room a profitable part of the business.

3/9/24       #2: finishing time expectations ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

The first thing I would tell you to do is work with your guys on several jobs from start to finish. Then you will have a "feel" of what it takes to get the job done.
Then sit down with them and ask them "what do you need to get things done more efficiently"
I would love to know what the outcome is. Most of the time it is help to sand and speeding up dry times.
Good luck !

3/10/24       #3: finishing time expectations ...
Antonio

That sounds like 1 day worth of priming; 2 days worth of top coating.. with other work getting done between dry times. 3 man finish shop with additional sanding help when needed. I always try to keep someone; wether myself or apprentice spraying at all times. The jobs we do are a lot bigger though 200+ doors. Your setup is similar to ours.

3/10/24       #4: finishing time expectations ...
RichC

I'll bet good money they are spending way too much time handling parts. As mentioned, put on a mask and spend a week in the booth. It's very likely not the guy unless you have him tied to the wrong kind of production spray equipment. Give him high volume spray equipment and methods of passing parts through the booth faster. Besides, finding a new finisher will really cost you and nearly impossible to find.

3/11/24       #5: finishing time expectations ...
Dave Edgerton  Member

I agree its not the person dragging their feet, its usually in setup and handling.

3/11/24       #6: finishing time expectations ...
gary

I switched to a fairly inexpensive hang line and our finishing efficiency skyrocketed.

3/11/24       #7: finishing time expectations ...
JM

I have one finisher, he will do a job like that in about 3 days. Whitewood Sanding, 1 coat primer, 2 top coats with scuff sand between all finish coats.

3/11/24       #8: finishing time expectations ...
Quicktrim

Gary ,
Did you have any probl with runs when using CV ? I see what you are saying the dry time as you do one side at a time stinks , what about sanding between coats ? Do you just remove the hinge clips and then reinstall after sand ? Also I can see benefits of not having all that open square footage for dust to set in as it's flashing off.plus no marks on backs from the dry racks .

3/11/24       #9: finishing time expectations ...
gary

We were very surprised with how short the learning curve was. We had some runs where we had to double coat when rails met stiles on doors and face frames but worked them out. It is not necessary to remove clips and other hangers but it is fast to do if you want to. Dust and rack marks are a thing of the past. I wouldn't want to go back to spraying flat...no way...not ever.

7/28/24       #10: finishing time expectations ...
Frank Garrido  Member

Website: http://www.cabinethero.com

Definitely do a job study , it’s the best thing for you take the time to ensure the job or tasks performed are structured and set by your standards . Your standards of quality and efficiency will
Really become clear to you as you see what areas require a lot more attention to detail and what areas are more productive . For example all the one sided components like Fillers , Moldings, toe kicks, panels , usually require the least amount of prep and visual inspection and time . One of primer and two coats of a top coat should see all these components out in one day . Having part of the job being completed especially parts that are necessary for installation does two things .
It demonstrates to your crew the progress and productivity which should be achieved for your business .
The other half of the job Doors and boxes ( if they are face frame) is s as mother study for you to break down for them .
Again once you see the areas of attention you will be able to understand what is important requiring more time and what is less important . Like the front of a Cab door versus the back !
Your instructions as to how they will approach the jobs will ensure the productivity to ensure profitability without compromising quality .
This structuring of how the work is to be performed is your responsibility , it’s not automatic . Taking the time to this is vital , the sooner you do it the less time you will spend retraining your guys on how get the job done. They either don’t have
A clue on the costs of running a business or more likely it’s not their responsibility and they are just doing what they think is best , which is not always what is best for your business.
Set your standards is my
Advice .

7/28/24       #11: finishing time expectations ...
Quicktrim

Frank thank you!
That is great advice. I admit the buck has to start and stop with me. It is my responsibility to set them up for success. I was a twenty five year installer before I started this shop and at times the stress of getting all the parts to come together has been debilitating. I have tremendous respect for every shop owner who has been through the first three to five years. I thought I knew a lot about how things should be done from seeing everyone's product as an installer. I thought I knew better than most.

The harsh reality was that I had no clue as to what it took to get a product out the door quickly enough and with quality enough to make a decent profit.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!