Bonehead conversion varnish mistake

7/26/15       
Andy Member

I got ready to topcoat a 3d cnc cutout that took 20 hours to cut out, and like an idiot, I used lacquer thinner to thin water white conversion varnish instead of xylene. After half a day of drying, the finish was still very tacky. I added another coat of heavily thinned varnish (this time with xylene) to try to reduce the tackiness.

After two days, the piece is still tacky, though to a lesser degree. Is there anything simple I can do to make the finish cure?

7/26/15       #2: Bonehead conversion varnish mistake ...
Jim

Call the techs for the manufacturer of that finish product. If you have to strip it there professional stripping products that you can't buy in a big box store.

Companies like Benco sales and other specialist that focus on really powerful strippers. Always follow all safety precautions!

7/27/15       #3: Bonehead conversion varnish mistake ...
Kevin

hmm... i use lacquer thinner all the time in my sherwin williams conversion varnish. Never had a problem. Sounds like you didnt add proper amount of catalyst

7/27/15       #4: Bonehead conversion varnish mistake ...
Mastercabman

I have to agree with Kevin
Usually if it does not dry is because of too little or no catalyst

7/28/15       #5: Bonehead conversion varnish mistake ...
Daniel Shafner  Member

The quick fix doesn't always work, but it did for me on a rack of doors if you didn't mix enough catalyst is to mix up another batch of topcoat and put in more than the recommended amount if catalyst.

The idea is that this new "hot" topcoat will kick your under catalyzed coating. That's the idea. You'll know if it works, everything will feel cured.

And if it doesn't work, strip or wash everything off and begin anew.

7/31/15       #6: Bonehead conversion varnish mistake ...
Shane

if you try to kick the under catalyzed coating in with over catalyzed product your customer will be calling you soon after delivery when it starts curing out. Shrinking, cracking, peeling and full of "Acid Bloom"... tuck your tail and chemically strip the piece and start over... we have all done it...

8/2/15       #7: Bonehead conversion varnish mistake ...
Sean Jackson Member

@andy - so what route did you take?

8/9/15       #8: Bonehead conversion varnish mistake ...
Ken Byrd Member

Wow. I just finished posting a new query about CV cure. (I feel like a bonehead for not searching for this thread before posting) Thanks, all sounds good. Wish me luck, going downstairs now to apply the hot coat. Just have to worry about thickness!!!

8/13/15       #9: Bonehead conversion varnish mistake ...
Ken Byrd Member

Well, last week I did the "hot coat" with almost double the catalyst (5.5%) and it did the trick. Cured enough to thoroughly sand the table top (had bugs in it anyway) then apply a proper final coat. Daniel's advice was right on! Thanks for that boost of confidence you gave me before re-coating!

8/13/15       #10: Bonehead conversion varnish mistake ...
Daniel Shafner  Member

Ken, I'm glad this worked for you. It did work for me. It's a maverick approach that will never find any official sanction, but it's a workaround that is at least possible. It has a better track fecord than, let's say, leatril has or tarot cards, lol.

In retrospect I would also add to my suggestion to mix in some "hot solvent" (something to vive your fresh over-catalyzed application some extra solvency, also). My tbinking is that you want to increase or insure a good melt-in of the application so that everything vets catalyzed.

Who doesn't like a good crosslink, said no undercatalyzed coating ever.

8/18/15       #11: Bonehead conversion varnish mistake ...
Andy Member

Thanks everyone for the suggestions.

I ended up coming to the conclusion that my catalyst was too old. I let the cutout sit and cure in my shop for about 5 days to see what would happen. It eventually got dry enough to sand. It was still somewhat tacky, but hard. I got some fresh catalyst and sprayed a light coat on. That did the trick.

  • Post a Response to this thread
  • notify me of responses to this topic
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)