Wood finish that keeps wood as natural looking as possible

12/1/15       
Jason Yeager Member

Hi all,

I have a job in rift sawn white oak in which the client is looking for a finish that leaves the wood looking as if its unfinished - as natural as possible. They have selected a wood floor finish - Bona Naturale - and are asking that I match it. I have tried various flat and super flat conversion coatings, and nothing I am working with is getting me there (specifically ML campbell magnamax in super flat, and ML campbell magnaklear in a 4 degree sheen). Anyone have any ideas? How about using the Bona Naturale on the cabinets?

12/1/15       #2: Wood finish that keeps wood as natu ...
Kevin

i was going to suggest using the bona naturale.. i have done a couple very large commercial projects that spec'd it and found it to be pretty simple stuff. even sprayed it.

12/1/15       #3: Wood finish that keeps wood as natu ...
Jason Yeager Member

Thanks Kevin,

Spraying worked well, what did you use to spray it? How many coats did you use?

Did you have any problems with the edges wanting to sag?

12/1/15       #4: Wood finish that keeps wood as natu ...
Kevin

was over a year ago. sprayed wit with a graco compliant cup gun with a 1.8 nozzle set. sprayed light coats to prevent any sags and maintain the low build/natural look. 2 coats was all it took.

12/1/15       #5: Wood finish that keeps wood as natu ...
RobertJ

Find an ICA Coatings dealer. Try one of their waterbornes....they are top notch and from Italy. End of Story.

12/1/15       #6: Wood finish that keeps wood as natu ...
Jason Yeager Member

Robert,

Can you recommend a specific finish based on your experience?

12/1/15       #7: Wood finish that keeps wood as natu ...
Jason Yeager Member

Kevin,

I am leaning towards using the Bona just because I know it will match perfectly - Do you think the finish would hold up in a kitchen environment? I would think so since its used on floors, but curious anyway.

What about the feel - was the finish smooth enough when you were done that it wasn't a liability / sticking point?

Thanks

12/2/15       #8: Wood finish that keeps wood as natu ...
CraigM

I second RobertJ's recomendation of ICA. I currently use their OAC360IPZ dead flat poly. Looks like nothing is on the wood.

12/2/15       #9: Wood finish that keeps wood as natu ...
monty

I agree with Graig, ICA 2k comes out aroud 2 degree gloss with multiple coats. Acrylic

12/2/15       #10: Wood finish that keeps wood as natu ...
Jason Yeager Member

Thanks guys,

I will call ICA and check it out

12/2/15       #12: Wood finish that keeps wood as natu ...
JT

Hi Jason,

Milesi Wood Coatings www.milesi.us The market share leader in wood coatings in Europe stocks two Natural finish products in the US specifically for your need. The solventborne finish is LUA118 Natural finish a 2K acrylic self sealing finish and the waterbase is HGA19 a 2K waterborne natural finish. They are readily available and will meet your project needs. Let us know how else we can help.

JT

12/2/15       #13: Wood finish that keeps wood as natu ...
JT

Hi Jason,

You can also check out the Milesi Wood coatings product on facebook or Finishing IQ by clicking on the following link. I think you'll find far more information on the Milesi product than anywhere else. http://www.woodworkingnetwork.com/product/sanding-and-finishing/acrylic-self-seali
ng-polyurethane-coating

12/3/15       #14: Wood finish that keeps wood as natu ...
Jason Yeager Member

Well - I have been trying to get in touch with ICA distributor - 2 days no call. Rep was great, helped with selection, but apparently distributor doesn't want to sell.

I am hearing the Acrylic coating are best for this as they don't change the look of the wood at all or bring out any of the woods color - which is really important, as the Bona that I need to match doesn't enhance the woods color at all. Do you guys agree that the Acrylic is the way to go?

12/3/15       #16: Wood finish that keeps wood as natu ...
JT

Hi Jason,

To answer your question yes the 2K acrylic is exactly what you need and want for this project. The Milesi LUA118 Natural look finish is a 2K acrylic coating that catalyzes at 25%. Let me know what state you are in and we will get you the product.

12/3/15       #17: Wood finish that keeps wood as natu ...
JT  Member

Website: http://www.milesi.us

Jason,

Also, I am a wood web member and sponsor.

12/3/15       #18: Wood finish that keeps wood as natu ...
Paul Snyder  Member

Website: finishing.tips

For a fast and easy solution I'd use the Bona finish Jason. It's a catalyzed waterborne polyurethane and will provide the durability you need as well as a guaranteed match. It's also formulated to have a warm, soft feel to the touch.

The ICA and Milesi finishes are top notch and worth getting a gallon of their various products for testing. That way you will be ready to choose and use one of them if you need it in the future.

Though acrylics are clear and non-yellowing, the key to achieving a good match in your case is to use a waterborne finish. Any solvent base finish, acrylic or not, will give the wood a different look and won't match.

Do some test spraying on large scrap before starting the actual project. Sometimes it helps to apply the first coat very thin to reduce raised grain.

12/3/15       #19: Wood finish that keeps wood as natu ...
JT  Member

Website: http://www.milesi.us

Hi Paul,
I'm sure the Bona product is a superior product for floors which it designed for. The Milesi product is specifically designed to be sprayed for exactly projects like the one dictated. The Milesi solvent version LUA118 will not change the appearance of the natural wood. However, if this is a concern Milesi also provides HGA19 2K WB Natural finish designed to be sprayed for this specific application. Regardless, I totally agree with Paul that whatever coating chosen should be tested.

12/4/15       #20: Wood finish that keeps wood as natu ...
Paul Snyder  Member

Website: finishing.tips

Hi JT,

You were able to post twice while I was typing so I didn't see your responses before I hit send. Sounds like you're able to get some product into Jason's hands quickly so he can do some comparison testing and get the client to sign off. Just curious - are there any concerns with shipping the waterborne product when the temperatures are below freezing?

I just read the product info sheet on the Milesi solvent based natural finish which says it contains pigments and extenders that prevent it from wetting the wood fibers like other solvent based finishes (which changes the color of the wood). I'd be interested to do some side by side testing with the waterborne version to see how closely the appearance matches. I wonder if the reduced surface wetting has any effect on adhesion?

Do you know the marketing plan behind Milesi formulating a solvent based finish to look like a waterborne finish? Is it intended to be step towards greater market acceptance of waterborne finishes?

Wood floor finishes and wood cabinet finishes are nearly identical. And the Bona finish is in the same family as the ICA and Milesi finishes so it's performance will be comparable. The main difference between them is that floor finishes contain additional additives (e.g., an anti-slip for safety and aluminum oxide for better wear). I would not use a floor finish as matter of routine for wood furniture, cabinetry, and mill work, but for a one-off project I'd be comfortable using it.

There's more than one way to get the job done.... What's important is that the client is happy and the check clears.

12/4/15       #21: Wood finish that keeps wood as natu ...
JT  Member

Website: http://www.milesi.us

Hi Paul,

Agree with your statements. We would be more than happy to send you some product for testing.

Please send me an e-mail with your contact information and we will get you a sample of the solvent base natural finish for testing. it is a very unique product. adhesion is not a concern. This product was actually submitted for an AWFS award this year and was developed specifically for the Italian furniture industry. It has an excellent track record.

Yes there is a major concern with freezing on WB products but we do have a distributor close to Jason's location.

I can have our Technical sales manager Ron Bryze provide you some additional insights regarding both the solvent and WB versions of this product.

Best Regards,,

JT

12/4/15       #22: Wood finish that keeps wood as natu ...
Jason Yeager Member

Thanks JT and Paul,

Interesting to hear how the finishes for the cabinetry and floors aren't that different. The sample of the floor finish provided by the flooring contractor definitely feels a little rough - which makes sense for a floor.
Nice to hear that there isn't any problems with using it if that is what I need to do to get
a perfect match.

Thanks everyone for your help and insights, really appreciated!

  • Post a Response to this thread
  • notify me of responses to this topic
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)