Bullet proof exterior wood coating

2/29/16       
Jeremy Member

Hey guys,

I am in need of some help sourcing hey really durable, long lasting exterior wood coating.

We're building custom white oak windows and I need a finish to the exterior that will put up with years of weather. We have a full spraying operation, about all the equipment one could need. I'm just not real savvy on exterior coatings.

Solid, transparent, that really doesn't matter. I really just need something that will really stand the test of time.

What have you guys had good luck with?

2/29/16       #2: Bullet proof exterior wood coating ...
PainterDave Member

100% acrylic latex, not a "blend"

the higher gloss the stronger and cleaner it will stay IMO

2/29/16       #3: Bullet proof exterior wood coating ...
Phil Haisley

Sherwin Williams "Duration"

I normally spec 100% acrylic, but I made an exception for Duration. Mfr. wouldn't tell me what's in it but it really does hold up. I have it on my house. My painter has it on his house. I suspect it's an acrylic polyurethane blend, but I can't confirm this.

2/29/16       #4: Bullet proof exterior wood coating ...
Jeremy Member

Thanks guys.

I am really hoping to find options outside of your standard off the shelf paints. I have used just about all the sw lines and find that blocking, and overall durability are a problem. Most cure slowly and don't work well in a assembly kind of situation.

With a window having contact points a product that sets up hard enough to handle seal contact, and rubs, though flexible enough to deal with the natural breathing of wood.

I find that chemicals in plane cans with warning labels are harder to locate, though work far better than your mainstream "pretty cans"

If you catch my drift

Thanks guys!

2/29/16       #5: Bullet proof exterior wood coating ...
Leo G

How about using a UV Cure Powder Coating.

UV Cure Powder Coating

3/1/16       #6: Bullet proof exterior wood coating ...
kevin

sherwin williams F63FH3 . this is exterior polyurethane. available at their chemical coatings division.

3/2/16       #7: Bullet proof exterior wood coating ...
Robert Chickey Member

The best product I have ever used is called
D Dur. It is a Chemcraft product. I have used this and had more than 5 years of protection. I periodically check the coating applications and am still blown away by the performance. Check it out. You won't be sorry.

D Dur coatings

3/3/16       #8: Bullet proof exterior wood coating ...
Bart

Amazing how often this comes up. You're looking for a Unicorn. There is no such thing as bullet proof unless you can make your windows aluminum clad. Wood regardless of finish flexes, breaths, swells and shrinks. Anything will eventually fail. A marine grade two part poly finish would look/wear great until it fails and then is a total cluster to strip and refinish. You could go with epoxy stabilizers or impregnators to stabilize the wood for less movement. That's a lot of work. Personally I'd go with a top quality paint. Benjamin Moore Aura 100% acrylic is good product . I've used it on raw wood and also stripped stained/varnished windows and doors and recoated with Aura with good results. The most exposed to the sun windows/doors are good for 3-4 yrs. Longterm I would think ease of maintenance.

http://www.benjaminmoore.com/en-us/for-your-home/paint-products/au
ra-waterborne-exterior-paint

http://www.ics-ilva.com/exterior-waterborne-finis
hes.php

http://www.westmarine.com/buy/awlgrip--two-part-linear-polyurethane-en
amel--P004_121_002_525

3/3/16       #9: Bullet proof exterior wood coating ...
Alessio

I've also used Chemcraft's D-dur on exterior Maple restaurant tables and 2 Mahogany entrance doors with sun exposure. Supplier told me will get easily 5 years. 3 years later both items still looks great, and i know the restaurant tables get cleaned with chemicals even thought i begged them not to.

3/3/16       #10: Bullet proof exterior wood coating ...
denny Member

I am in line with Bart on this one.......
There is no magic wand here.
UV is the real Demon for outside finishes.
I still cling to many "solvent based" products indoors, but High Gloss oil base will be eggshell after just 6 months of sun.
High-Gloss, water borne, enamel from any of the big paint companies is the way to go.
Kelly Moore
Behr
Sher Wil
Benny Moore
Dunn Edwards
etc etc etc
If it does not get sun, I would go with oil enamel.
I painted the windows (outside) of 400 California Street, San Francisco, 30 years ago with oil enamel from Roy Anderson. The paint is STILL there, but the windows are inset and get almost no sun.
good luck

3/3/16       #11: Bullet proof exterior wood coating ...
denny Member

.....clear, not enamel in your case, but the same applies for water borne clears as well.
good luck

3/4/16       #12: Bullet proof exterior wood coating ...
Paul Snyder  Member

Website: finishing.tips

Here’s another vote for a good quality exterior primer and paint. They come with a lifetime guarantee and are definitely the longest lasting option and relatively easy to maintain.

Clear finishes on wood don’t last as long as paint, though some do last much longer than others. There’s a wide selection of finish types and a wider range of performance. One good source of information on the performance of exterior finishes is the wooden boat community. They run long term tests on all kinds of exterior finishes ranging from wipe on oil finishes (e.g., Teak Oil) to catalyzed polyurethanes. Note that some of the exterior finishes contain a lot of pigment to block the UV and are called stains.

I’m attaching a test report from Classic Boat magazine showing the results from two different test sessions. The chart box on the left lists the finishes they used for the first round of tests that started 11-1/2 years ago (from date of publishing). The chart box on the right is from the third round of testing and show the results after 5-1/2 years.

The winner from the first test is Colean polyurethane. It cracked at the sharp corners of the wood, but otherwise held up exceptionally well. Rounding the corners of the wood will help prolong the life of your exterior paint/finish. The winner from the second test is Awlgrip Alwood MA. Both products are 1K moisture cure polyurethane. Either of these finishes would be a good choice for longevity.

Click the link below to download the file included with this post.

Exterior_Finishes_Comparison_Test_Classic_Boat_2015_04_April.pdf

Colean exterior catalyzed polyurethane

3/4/16       #13: Bullet proof exterior wood coating ...
Jeremy

I do appreciate all the responses guys. I would like to make clear that I understand that there will be no "Bullet Proof" Exterior coating. Mother nature is a beast and will beat wood, and finishes to death, I get that.

All in all, the contributions have been very helpful. With the vast knowledge that this forum has I was sure that some of you would have some products you used in the past with good results.

I had thought about an oil based enamel, though I have not had much experience with it. With the White Oak I would figure that a good wet coat to penetrate would work wanders.

2/27/20       #14: Bullet proof exterior wood coating ...
pat s gilbert

Does anybody have any idea what a permitted spray booth is worth in So Calif?

It's a 10' x 8' typical spray booth


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!