Color matching with various stains

9/30/16       
Eric Member

I am a professional finisher in both conmercial and residential casework and millwork..

I currently use Sherwins SB wiping stains..
But I also have a full line of Mohawk Ultra Penetrating stains, as well as Sherwins Universal Dyes..

I tend to keep Sheffield oils as well to use in tangent with certain recipes

To color match with SB stains, I use a chip to compare, look the recipie up and adj color for exact match. Pretty simple and fairly fast..
The SB stains have the Umbers and Sienna in raw and burnt..

How can I mix these colors using universal dyes. Or Mohawks Ultra Pens?

Raw umber

Burnt umber

Raw sienna

Burnt sienna

I have a horrible time hitting these colors from primaries and kicker colors

9/30/16       #3: Color matching with various stains ...
Eric Member

I know that Mohawks Ultra Pen ( Ngr ) has these colors.

I am very interested in mixing these colors from primaries

9/30/16       #4: Color matching with various stains ...
Leland Thomasset  Member

Website: http://www.cnc-cabinetparts.com

I do feel your pain. I have used all of the above. Lately I have been working with Gemini coatings to start using their stain matching system that comes complete with base, formulas, calibrating tools and chips. It is suppose to be repeatable from a couple ounces to a couple gallons. I will keep you posted.

10/2/16       #5: Color matching with various stains ...
Eric Member

I wish someone would chime in..I have a need of using some unis on an upcoming job..

Being able to hit all umbers and Sienna's with theses would help.

I know:

The yellow/ brown, red brown/ green brown and blue brown are the base colors for all the umbers and Sienna's..but there has to be more as these alone just don't make it

Please help

10/2/16       #6: Color matching with various stains ...
DanShaf Member

I'm not fully sure what you're asking but I am hopeful that this brilliant writeup by Mac Simmons will either help or fully steer you in your needed direction.

Are you trying to create colored dyes that when sprayed out on glass or a white surface are raw umber, burtnt umber, raw sienne, burnt sienne?

Make sure that your white base is not titanium white. Rather, use zinc white. Zinc white has much less tinting strength (it lacks hiding power and opacity versus titanium white). It's said to be a "transparent" white.

Why aren't the Mohawk Ultra Penetrating Stains which are dye stains mixed upo according to their coloring charts what you need?

"Tinting Toner Tips" by Mac Simmons

10/2/16       #7: Color matching with various stains ...
DanShaf Member

And this, also from Mac Simmons

"Color Matchting Tips" from Mac Simmons

10/2/16       #8: Color matching with various stains ...
Eric Member

What I am trying do is make all the umbers and Sienna's using universal days..sherwins colors only come in magenta.red, brown, black, yellow, orange and blue..

I can't ever get the recipe right to mimick these colors..

Mohawk has these premade..and I do have em..but I would like to know if anyone has ever success fully made them from primary colors..

I understand that grain color is a big modifier in how a color will look after mixed.
But let's just say a pale maple or white oak

TBH I just want to know what makes up each color..

To ask an artist..he'll give you 7 different colors in each..

I am working on my color mixing abilities and would like to be able to make these from sherwins universal dyes..

T

10/2/16       #9: Color matching with various stains ...
DanShaf Member

Mac's "Color Matching" essay is the best there is on this subject. It seems to me that he hones in on exactly that holy grail of color blending that you're looking for.

10/24/16       #10: Color matching with various stains ...
francis

the umbers are pigment! and if i understand your question, you would like to match those umber colour with dye, you can't match pigment colour with dye they are completly different. you need to get some pigment chromaflo 866 or 844 or mohak have their line of pigment as well.

Pigment

10/24/16       #11: Color matching with various stains ...
Eric

I use 844's and Phoenix colorants to mix my CVs with.

There has to be a formula that allows one to use an analine type stain and get close to the umber and Sienna's

And would never use them in a stain..

it's ok, I get close enough with all I use, just wanted to pick brain and see what's responses I get.
I mix all my own stains and pigments. And try to challenge myself as much as possible

2/17/22       #12: Color matching with various stains ...
Daniel Shafner Member

Get the book "Blue and Yellow Don't Make Green". After you read it, you'll have a better understanding of the world of coloring and pigments.

9/7/22       #13: Color matching with various stains ...
joseadam Member

Website: https://www.walgreenslistens.me/

Just bring a sample piece to customize. Please note that the stain may look different on different woods. So when trimming walgreenslistens


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products

    Become a Sponsor today!