5/11/17       
Alan  Member

I manage the finish dept. in a small shop. We spray a lot of SW hi build pre cat, sealing first with vinyl sealer. We spray other paint finishes as well, so we might use 15 gallons of sealer per week, more or less. I would like to start spraying sealer from 55 gal drums. Reasons: cut down on acetone use, less hazardous waste to dispose of, not have to change back and forth between sealer and top coat. I can leave the sealer gun set up and not have to run acetone through the line every night. A little cheaper per gallon.

My SW rep won't sell me sealer in a 55 unless I use 55 gal per week. Says it can't be under agitation for longer than a week. T67FH67 is good catalyzed for 6 months. I will probably use a drum in 4-5 weeks. I will only be agitating the drum 8 hours per day. Has anyone ever heard of this before, or is my SW rep jerking my chain? I sprayed from a 55 in another shop and it took us at least 3 weeks to go through a drum. Never had a problem .

5/11/17       #2: Spraying sealer from 55 gal drums ...
herb

here is my take, as far as agitation he is most likely concerned that most people peg out the agitator air motor and whip a lot of air into the coating, my suggestion would be to get a back geared agitator more expensive but has a lot of torque to mix the material and would be hard to whip in a bunch of air, frankly i have never heard that a material can't be mixed for a week max, especially a vinyl sealer i know i have no issues agitated ml campbell sealer but i don't peg out the air motor

good luck herb j

5/12/17       #3: Spraying sealer from 55 gal drums ...
Arthur grudko

I agree with Herb about the low speed stirrer. Is it an open head drum? If so, I would be concerned with solvent evaporation over that long a period.

5/12/17       #4: Spraying sealer from 55 gal drums ...
Shane

your TDS sheets for the Sherwin precat high build/sealer combination will show you that you should be catalyzing that vinyl sealer with V66V26 if your using a catalyzed product over the top. your tech/sales guy should have had that info to you a long time ago.

5/12/17       #5: Spraying sealer from 55 gal drums ...
Shane

ok I misread the product number. The F6 is precatalyzed vinyl and the F7 is a post cat.. nevermind I'm wrong.

5/12/17       #6: Spraying sealer from 55 gal drums ...
Alan Burton  Member

Thanks guys. It is a closed drum. Rep now says he is worried about viscosity change because of long term agitation, but will sell it to me to try anyway. I don't forsee any problems. I will monitor viscosity and add a little reducer or retarder if needed towards the end. Thank you for the comments.

5/13/17       #7: Spraying sealer from 55 gal drums ...
Jeff Austin

He has warned you and he is selling you want you want. You own it now. I would have said the same thing. If you can't use it in a weeks time, you shouldn't buy it in that container. He's just trying to look out for you and you called him a jerk. But what really stands out is what is with you saving on acetone? Your story doesn't make any sense. Why will you use less going to a drum?

5/14/17       #8: Spraying sealer from 55 gal drums ...
Nick

I only use about 5 gallons a week of post cat sealer but much like you l got tired of cleaning the pump between sealer and finish coats so l just bought a 5gal agitated pot. With a 6 month pot life on the sealer there's no need to clean it when it's empty l just pour in another 5 gallons. Plus no worry about evarporation as I have ball valves on the air lines, when done spraying just close them up and wipe off the gun. great time and solvent saver. I don't see why a 15 gallon pot wouldn't work for you.

5/15/17       #9: Spraying sealer from 55 gal drums ...
Matt

I don't know your specific setup, but unless you're getting a significant price break buying it in 55s instead of 5s, I wouldn't bother. That's a lot of flammable material sitting around, especially if it's kept inside your shop.

We spray 30-60 cabinet doors per day, so my usage probably isn't as much as yours is, but I'd have to triple or quadruple in volume before I'd consider buying anything but wash thinner in 55g drums.

I definitely have kept vinyl sealer in 5 gallon cans, agitating it only during working hours, and sipped on the same can for several weeks (lower volume shop, spraying Sherwood precat over the sealer). Didn't have any problems there as long as the sealer didn't clump on the bottom over the weekend (usually did, had to stir by hand before leaving it to the agitator).

Slow agitation is the key. Just keep that propeller fan air motor going "putt putt putt putt"


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)