mastercabman

How effective are chemical strippers on conversion varnish?
How about glazing?
I may have a refinish job that I would like to use CV but the doors and drawer faces are mitered rail and stile with a small rop molding and it is glazed
The client may want new doors but I do need to give him a quote on refinishing existing doors and drawers

4/9/19       #2: Chemical strippers ...
Bob Niemeyer  Member

Website: niemeyerrestoration.com

Commercial grade removers will take it off with no problem. The problem is that many Kitchen cabinet doors do not survive stripping very well. They tend to fall apart if they are cheaper doors.
We have found once you buy the remover, labor to strip them, resand wood to prep for finishing you are not to far away from buying new doors that just need a quick sand and are ready to finish. Wood species and shop hourly rate does play a big deciding role in this.

4/10/19       #3: Chemical strippers ...
rich c.

Don't forget the cost of a high end air supplied respirator if you are going to use methylene chloride industrial stripper in that bid. It's incredibly unhealthy stuff! Cheaper to buy new doors compared to the labor it will take to clean out that rope molding.

4/11/19       #4: Chemical strippers ...
Arthur grudko

Methylene chloride strippers are no longer available, unless you can find some old inventory. NMP based removers are, for all practical purposes, unavailable.

There are some removers (available at most Lowes stores) that are based on an NMP substitute) that take a lot longer to work, but are effective. There's Smart Strip and Smart Strip Pro that are di-basic acid based that work well but take many hours. These are applied in a thick coat and paper is wrapped on them.

Don't know if ether are effective on conversion varnish. Both rinse off with water. Rope molding shouldn't be too much of a problem if they're at all effective.

4/11/19       #5: Chemical strippers ...
dean c

My understanding is that while MC removers will/are banned from retail sales, you can still get them professionally from suppliers

4/11/19       #6: Chemical strippers ...
Arthur grudko

I stand corrected. You're right. Banned from consumer, allowed for commercial use.

4/11/19       #7: Chemical strippers ...
rescraft

Outsource and add $ for handling, transport etc. When customers find out how much time, trouble & expense it is to strip, it opens their eyes.

4/11/19       #8: Chemical strippers ...
mastercabman

Thanks for the replies
I got a ball park figure to have them stripped
For the price I can get new doors/drawers
I rather work with new wood when using CV anyway

5/16/19       #9: Chemical strippers ...
dan shaf Member

I live in the very blue and silly state of CT. Dad's is still available, no problem. It's methylene chloride and no lye. No lye means it won't darken the wood.

There is a myth as to just how dangerous methylene chloride is for you. No chemicals are good, but the science just is NOT there regarding the dangers of methylene chloride. The history of this chemical being over-regulated is that the giant furniture industry lobied for it to be over-regulated, impinging on many restoration shops to carry on with cost effective refinishing projects vs a potential customer deciding instead to buy new furniture. That's the history. Furniture industry lobbyists and the wined & dined Congress.

The toluene in Dads is worse for you than the methylene chloride.

5/16/19       #10: Chemical strippers ...
dan shaf Member

1. Brush on the mc stripper.
2. Wait.
3. Scrape off without gouging the wood.
4. Grab handfuls of wood carvings that come off the plane (wear thick rubber gloves) and use these shavings instead of rags.
5. The wood shavings are especially effective for getting the sludge out of the carvings and shapes of profiled surfaces and moldings.
6. Water rinse with a pressure washer set on low pressure so that you don't etch the wood. The water has to bounce off the wood, not soak into it. It will take the stripper with it.
7. Wipe down with half denatured alcohol/half water.
8. Wipe down with lacquer thinner.
9. Lightly sand and build your new finish schedule.

  • Post a Response to this thread
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)