Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Best Way to Achieve High Gloss Gray

10/3/23       
Michael R

What is the best way to achieve a high glossy finish using water-based finishes?
The customer wants a gray high-gloss.

I'm thinking the best way would be to stain the wood and then apply a 50-sheen clear coat rather than a 50-sheen black finish.

10/3/23       #2: Best Way to Achieve High Gloss Gray ...
RichC

Stain would not be my choice, but maybe they want a transparent color and are just worried about the gloss. The big problem with many water based finishes is the cure time. Not the dry time. A finish out of the gun is not enough for high gloss. To get a perfect gloss finish you have to wet sand and do a couple grades of polish. The finish must be fully cured before any buffing is even considered.

10/3/23       #3: Best Way to Achieve High Gloss Gray ...
Michael R

Hi RichC

That's what I thought a lot of water-based processing time and won't be cost-efficient to a customer or at least trying to explain it reasonably.

I'll just attempt to get them to pay for a sample using their selected gray paint color in a 50-sheen and see how that flies.

Thank you!

10/3/23       #4: Best Way to Achieve High Gloss Gray ...
Leo G

High gloss and a 50 sheen are miles away from each other.

Solvent 2K poly's cure in days.

10/4/23       #5: Best Way to Achieve High Gloss Gray ...
Adam

Do you understand that the sheen scale is 1-100?

Awlgrip 2k Poly has a sheen of 95. It is a true mirror read a newspaper reflection coating. That is off the gun with careful prep on the side of a boat. It's a solvent.

ML Campbell Arroyo 1k or 2k gloss white pigmented are 70+ sheen. They are waterborne and can easily be tinted at any paint shop or add your own pigment.

10/8/23       #6: Best Way to Achieve High Gloss Gray ...
Kevin Dunphy

Website: http://kdunphy.com

I've done lots of true High Gloss finishes a long time ago.

It is hard never found a residential customer willing to pay the price .I can't imagine the cost of a kitchen and you'll need skill and skill .

Leo right do your homework the fake high with expoy is not the same as a polished 2k or Polyester.I know Ikea sells fake high-gloss laminate white , could find that in a grey.

Below is a like I did car parts for an MG in high gloss

BTW there is no sheen number in high gloss

know Ikea seel

10/9/23       #7: Best Way to Achieve High Gloss Gray ...
JeffA

In my hard knocks opinion, most people would accept something in the 60+ gloss for a high gloss. But... and I mean But....you will need to do a magnificent job of prepping which includes whitewood sanding and filling along with 2 coats of primer to get a good filled surface. And that doesn't include applying the enamel. All that gloss will show everything you have missed and everything you didn't know..... Best of luck

10/10/23       #8: Best Way to Achieve High Gloss Gray ...
Adam

I’ve sprayed & buffed( 8) coats of MLC waterborne 2K clear on a qtr sawn white oak desk top.

1st day Woodsong solvent stain. Sealcoat shellac + transtint dye toner coat.
2nd day (4) coats 2K clear
3rd day (4) coats 2K clear
4th day curing
5th day buffed it to mirror.

That was back in the mid 2000’s. The waterborne stains weren’t good enough yet.

10/12/23       #9: Best Way to Achieve High Gloss Gray ...
Brian

I know this will sound crazy but it works. First stop thinking like a woodworker and more like an auto body technician. Once you have the substrate sanded and completely sealed use the same steps and materials as if you were finishing a body panel. Go to an auto paint supplier forget the woodworking.
Go through the steps and you will get a mirror finish that is durable.
The down side is that the materials are expensive and it takes a lot of time the end result is that few are willing to actually pay the price. I've done a full kitchen in mirror gloss black which is the most difficult color to make perfect. Charged 17k for the finish work, customer was very pleased but I should have and could have charged more as it takes TIME to get it perfect. Any way Auto finish materials are much, much better suited for high gloss.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • EX-FACTORY INC.
      Offering New & Used Woodworking Machinery including Auctions & Liquidations
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!