Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Technical advice for an arc cut of large radius

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Technical advice for an arc cut of large radius

5/26/20       
Jonathan Boulware Member

I’m working on a mahogany repro/homage of a Danish modern mirror. See design photo on paper. I planned to use a router
On a long arm the way you’d cut out a round table, but it turns out that the arc radius is huge, way more than 10’. Any suggestions on how to cut the arc of these rails and stiles? The mirror frame is 30”x50”. The arcs are not the same and they tighten a great deal at the mitres.

Any suggestions welcome.

Thanks.


View higher quality, full size image (640 X 480)


View higher quality, full size image (640 X 480)


View higher quality, full size image (640 X 480)

5/27/20       #2: Technical advice for an arc cut of ...
Tom Gardiner

Find someone with a cnc and go over with a sheet or scrap of baltic birch. Have them cut curve templates. Think about how you want to use the template. If you will be using a handheld router then make sure the width of the template is such that you have a stable surface for the router.

5/27/20       #3: Technical advice for an arc cut of ...
Cbww

Bandsaw the curve. Edge sander or spoke shave to clean up. That would take about 15-20 minutes to do.

5/27/20       #4: Technical advice for an arc cut of ...
Keith Newton

A couple of things I have done, is to bend a thin batten between to nails while pushing the middle to the right curve. Keep in mind that bending solid wood, about 8 times the thickness will be straight on the ends.

For much larger or longer arcs, I have found that my steel 100' rule is easy to attach to the edge guide on the router. Then out on my parking lot where there is lots of open space, I can clamp the 30' ~ 50' or whatever chosen radius is to a porch post. The steel tape doesn't stretch to swinging clockwise, the cutter will pull tight. Oh, to prevent the tape from snagging on the asphalt, I lay clean strips of hardwood across under the tape to hold it slightly above. And its easy to drive a 16d nail through the material and waste board underneath into the asphalt. For concrete you might need tapcon screws.

5/27/20       #5: Technical advice for an arc cut of ...
rich c.

Take your frame to a CNC shop and have them cut it. I've made up to 12' trammels. 1/4" plywood with 1x3 cleats on the sides. Alternate the joints in the parts. Hot glue the pivot block on the floor.

5/27/20       #6: Technical advice for an arc cut of ...
TonyF

Jonathan:

It sounds like you are making one frame and not multiples, so "jigging up" seems like a waste of time. If your frame is not glued together, take the parts to a bandsaw and cut the curves, then sand to the line. If the frame is already glued together, I would consider cutting through the opposite miters to leave two "L" pieces, bandsaw the curves, reglue the miters and sand to the line.

Sandpaper wrapped around a flat wood scraper as the "sanding block" will smooth out the larger curves without dips, and sandpaper around an appropriately sized piece of PVC pipe will smooth the corners.

Mirrors like this were done many years before CNC equipment. After all, we are talking about being able to cut to a line, which is a fundamental woodworking skill.

It will take less time than you have spent on the Woodweb chasing this down.

Hope this helps.
TonyF

5/28/20       #7: Technical advice for an arc cut of ...
Leo G Member

10' stick with a pencil sticking through for the line and then handsaw or jigsaw the cut and sand.

5/28/20       #8: Technical advice for an arc cut of ...
TonyF

LeoG:

The project frame looks like it has a layout line on it already, or I would have offered up the "three nails, two sticks" layout method for a large curve.

I must say that I am disappointed in the number of CNC suggestions for what is really a simple frame with a little bit of hand work.

TonyF

5/28/20       #9: Technical advice for an arc cut of ...
Leo G Member

I would have traced the opening on a pc of cardboard and then freehanded half a curve, cut it out and trace it, flip it over to do the other side of the curve. Cut it with a jigsaw and then smooth it off with a spindle sander and then a random orbit til it felt smooth with no bumps in the curve.

5/29/20       #10: Technical advice for an arc cut of ...
Tom Gardiner

Tony - I offered the cnc suggestion not because I have lost all of my hand skills or desire to use them but because I can program and run that frame in 15 minutes with the control and accuracy that minimizes errors, sanding and risk to fingers.
There should not be a conflict between fine furniture making skills and cnc.
I don't mean this post to be mean spirited but to support the benefits of a new machine in the field.

5/29/20       #11: Technical advice for an arc cut of ...
TonyF

Tom Gardiner:

It is not mean spirited at all. If I had a CNC, and were versed in its use, I would use it all the time, much like my shaper and table saw. I might even become dependent upon it. The machinery and methods that I use reflect the way I was trained, and have worked well for a long time.

Still, I would question the total time outlay for the CNC, from start to finish, for one mirror frame such as the one in question, versus someone skilled in producing it via other methods.

And having to be dependent upon outsourcing for CNC usage on one frame would just not sit well with me. If I were making 100 frames, I might consider it, given the expediency of the CNC, but then someone with a CNC would have already underbid me, and I wouldn't have that project to begin with. But for one frame, it would be a slap in the face towards my own professionalism, part of which is derived from being able to solve problems as they arise and utilize the tools I have available. I would not outsource a task unless it was absolutely necessary, or there was a huge financial or time advantage in doing so.

Perhaps I am just too old and set in my ways, as I have always used these methods to produce work. I just thought I would suggest what I did, figuring that he already had these tools available. To me, using a CNC for that one frame would be like driving two blocks to the post office, instead of walking. To each his own.

TonyF

6/3/20       #12: Technical advice for an arc cut of ...
Joe Calhoon  Member

Long router tramels are awkward but possible. I used this last week to cut a 235” radius on some 68mm thick door frame parts. CNC router would have been easier but don’t have one.
I used the 2 point fixed triangle to lay out the curve but have never come up with a good way to use a router with that.
See the Instagram link for the whole process.


View higher quality, full size image (1280 X 960)

https://www.instagram.com/p/CAcv9C_D86W/?igshid=17kesuw54804x

6/5/20       #13: Technical advice for an arc cut of ...
Dave Sochar Member

We have done many like Joe's setup with a router on a stick.

Heck, we had one radius that was so large, we had to account for the curvature of the earth.

6/7/20       #14: Technical advice for an arc cut of ...
TonyF

David Sochar:

So, in the spirit of Archimedes, if we give you a long enough trammel, and a place to stand, you can rout the curvature of the earth?

:^)
TonyF

6/11/20       #15: Technical advice for an arc cut of ...
Adam

I agree with TonyF. Cut with bandsaw/ jigsaw/ scrollsaw and sand. Making a jig for that would take longer and not yield better results.

6/11/20       #16: Technical advice for an arc cut of ...
BH Davis  Member

Website: http://www.bhdavis.net

As most here I've done pretty much everything discussed. My preference today would be to make a template on the CNC and then use it with a template guide in the hand held router on a frame that was pre-cut oversize on the band saw.

CNC code and prep time would be about 15 minutes max.

BH Davis

6/18/20       #17: Technical advice for an arc cut of ...
Patrick Drake

The micro adjust on the compass bar is unnecessary, rub collar on the router and drill a hole.

7/12/20       #18: Technical advice for an arc cut of ...
Bill Colligan Member

I have done similar arcs with a radius over 20'. I made and reinforced a beam attached to my router. I did not cut my good stock as I was not confident I would get the radius without any movement. Making certain everything was stable I proceeded to cut the radius out of a sheet of MDF. I then traced the radius from the MDF onto the table top and rough cut it with a jig saw. Finally I clamped the MDF to the table top and cleaned to the perfect radius with a pattern bit.


View higher quality, full size image (3264 X 2448)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • Rangate
      Woodworking Machinery, Supplies and Knowledge

    Become a Sponsor today!