Subject: Re: Tapering Small Radius Dowel

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Tapering Small Radius Dowel

3/20/21       
Drew Zembruski Member

Website: http://www.artifexhome.com

I need to taper some ~12" long dowels. I am using 5/8" dowels and I'd like to taper one end to 3/8". I'll be doing 40-60 of them. Current working plan is to use the jointer to taper one end to 3/8" square and then round with a block plane. Any advice on repeatable, somewhat efficient process would be appreciated! The size of the ends (5/8" and 3/8") is the most important part in terms of accuracy; the evenness of the tapers piece to piece is less critical.

I could certainly have them made by a specialty shop but this is going to be for a set of wedding gifts for friends (short Shaker-inspired benches) and as a result I would prefer to make all the parts myself.

3/20/21       #2: Tapering Small Radius Dowel ...
rich c

There is always this method.

Chopsticks

3/21/21       #3: Tapering Small Radius Dowel ...
Drew Z Member

Thanks Rich. Should have specified that these are spindles for a bench so they will be rounded. But this contraption has plenty of ideas worth mimicking for repeatability and efficiency. Seems like after using the jointer to get dowels that go (in section) from 5/8" circles to 3/8" squares, a cradle of some kind could increase my efficiency and accuracy in using my block plane to fair the square ends round again. At least in keeping my sizing consistent.

3/21/21       #4: Tapering Small Radius Dowel ...
rich c

That's why I gave you the link. They show how to do an 8 sided chop stick, a 16 sided gets very close with just tiny points to sand off.

3/22/21       #5: Tapering Small Radius Dowel ...
TonyF

Drew:

You could make a jig like the chopsticks jig, with more clearance on the bottom, and place a spur (nail point, etc.) such that the tapered end centers in a way that allows the finished taper to fall 1/8" below the "sled" that the plane rides on. If your dowel is longer to start with, you could mak a "knob" that fits on the outside of the jig, allowing you to turn the dowel as you plane it.

The resulting multi-faceted tapered spindle will give you the "Nakashima look" that you are probably after.

Hope this helps.
TonyF

3/24/21       #6: Tapering Small Radius Dowel ...
Gary Balcom

Sounds like a good job for a benchtop lathe, a chuck, and a skew chisel.

3/24/21       #7: Tapering Small Radius Dowel ...
Gary Balcom

Actually, you could setup a slope to ride a block plane on, on the lathe to make it more repeatable.

3/24/21       #8: Tapering Small Radius Dowel ...
Nicko Member

Chuck it in a drill and just squeeze it in your hand with some sand paper and spin it until you get the taper you want. Where gloves to protect from the heat buildup. I have done this before and it’s fast and works well. You would have to have a drill that would accept 5/8 or reduce one end to 1/2 and then cut it off when done.

Nicko

3/24/21       #9: Tapering Small Radius Dowel ...
Drew Z Member

Website: http://www.artifexhome.com

Thanks all for some very good ideas -- I'm going to play around with them and do some time trials to find my most efficient method for doing all 60. Thanks again all.

3/24/21       #10: Tapering Small Radius Dowel ...
Nicko Member

If you have a disc sander you could make some kind of jig that you could put the dowel in and spin it around for the taper.

Nicko

3/25/21       #11: Tapering Small Radius Dowel ...
Thomas

We have made angled jigs to fit the taper we need for edge sander. Once you have the correct angle or slope, then you just start turning the dowel as you feed it into the angled jig. 80 grit paper will shape it pretty quick.

3/25/21       #12: Tapering Small Radius Dowel ...
Nicko

There Are some clever ways of tapering dowels on YouTube. One guy makes a jig and does it on a table saw.

Nicko

3/25/21       #13: Tapering Small Radius Dowel ...
Drew Z Member

I spent some time at the end of the day today trying out some ideas; Thomas, the edge sander seemed to be the fastest way for a repeatable result (and I can have someone else do it while I'm working on the other parts of the pieces). I am attaching an image from Fine Woodworking that I found helpful.
Nicko - I have made some larger, tapered dowels on the TS before and plan to again, as I don't have a repeater set up in the shop since I do almost all cabinetry now and not furniture. I've found it much faster and more accurate with the table saw the few times a year I need to have a leg for something. Plus I can have my cabinetsaw set up to do that and use the slider for everything else.

3/25/21       #14: Tapering Small Radius Dowel ...
Drew Z Member

Image didn't link correctly, trying again.


View higher quality, full size image (700 X 321)

4/4/21       #15: Tapering Small Radius Dowel ...
Drew Z Member

Website: http://www.artifexhome.com

Thanks again for the all good ideas. The sander ended up not being as quick or accurate as I hoped; I ended up tapering on the jointer and fairing with a block plane. Took me about 75 minutes to do 44 spindles, and probably 25 minutes was setting up jigs and stop blocks to standardize my taper and fairing. Next time I have to do this that time should get cut down further.
If anyone would like to see, I’m including a photo of the completed benches here, pre finishing.


View higher quality, full size image (2016 X 1512)


View higher quality, full size image (2016 X 1512)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America

    Become a Sponsor today!