Furniture Making

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Table leg joint strength

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Table leg joint strength

12/1/13       
Michael Sanders Member

Website: http://www.michaelsanderswoodworks.com

An architect wants me to build a small conference table for his office. It will finish at 84" long, 33" wide, and 30" high. The material is 12/4 cypress, reclaimed from an old train depot, and has been sitting in a dry warehouse for at least 10 years. He wants to dovetail the legs into the top, giving a clean parsons table look. I don't think this is going to have enough lateral stability and will eventually break. Any bracing between the legs would completely restrict the movement of the top. Check out the images. Anyone have a good idea? Thanks!

Click the link below to download the file included with this post.

CONFERENCE_TABLE__JOINT.pdf


View higher quality, full size image (1024 X 739)

12/1/13       #2: Table leg joint strength ...
P. Hanes

I have used the joint you have depicted on several tables. It worked well and was quite strong. I tend to be like you and visualize someone dragging the table across a room on the carpet. There really is no way to protect yourself against the poor judgement of others. I believe it is a strong enough joint for any reasonable use. People can figure out a way to break almost anything. It is not idiot proof, neither is your finish.

12/1/13       #3: Table leg joint strength ...
mark

I've also had good luck with a similar joint: pegged through tenon, not a dovetail. The table's about 6 years old, but made in cherry.

12/2/13       #4: Table leg joint strength ...
David R Sochar Member

I see no problem with the joint as you have it planned. Cypress is a bit soft, and that would be my only concern.

Make a test joint and try to destroy it. I bet you will find it as strong as a 3" apron with a haunched 1/2" x 2-1/2" x 3" tenon in a 4" leg.

12/2/13       #5: Table leg joint strength ...
JeffM

Would you trust a mortise and tenon in this application? That's pretty much a through mortise and tenon without an apron.
I don't see much of a problem.

12/4/13       #6: Table leg joint strength ...
Michael Sanders Member

Thanks for your input guys. Because the top is laminated to show the edge grain, I can make the outer strips with the legs joined to them, and then glue those to the top. This will give me a chance to see how strong the joint is before I commit and lose the chance to mortise in a cross brace between the legs. I hope you all are right, and that is not necessary. I will post a pic when the table is complete.

2/14/14       #7: Table leg joint strength ...
Michael Sanders Member

Website: http://www.michaelsanderswoodworks.com

Delivered the table yesterday. The dovetail was more than adequate and the table was as sturdy as any traditional style. I also posted a picture of the console I made to go with it. I showed the client this thread and he was impressed I sought out industry advice. Thanks to all that contributed!


View higher quality, full size image (2927 X 2196)


View higher quality, full size image (1154 X 1847)


View higher quality, full size image (3000 X 4000)

3/21/23       #8: Table leg joint strength ...
TMVHM

Website: https://tmvhandyman.wixsite.com/tmvhm

Thank you for this great idea of fixing the legs to the table top. I very much like the clean look. I wanted a thinner table top so I was afraid your solution wasn't going to be strong enough. I added some beams under the table ends to mount the legs with a bridle joint. It is really solid.
If you would like to see how I did it, please check my blog post.


View higher quality, full size image (3982 X 1825)

https://tmvhandyman.wixsite.com/tmvhm/post/a-solid-14-person-table-design-and-build

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies

    Become a Sponsor today!