Subject: Re: Improving Production Process With Shaper

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Improving Production Process With Shaper

4/29/24       
Jason Loyd Member

I’m hoping to get some insight from some of you all working in production environments about how you would increase the efficiency of making these hanging hammock chairs, seen in pic 1.

Our shop created the design for these and have been making them since 1977. Our production facilities burned down recently in a wildfire (R.I.P. Oliver 299 and many others), and as we’re looking at retooling, we’re wondering if there are aspects of our production process that could be improved.

They’re made of white oak, and currently everything is assembled square, and then shaped by hand on a pedestal mounted drum sander, from 40 grit up to 120. This is a physically taxing process, so we’re hoping to move to more repeatable operations on the shaper to profile everything.

The arms just need a ¼” roundover, so I’m imagining a stack with a roundover cutter at the top and bottom, and a rub collar in the middle.

With the arms fully profiled down their length, that would mean we’d need a matching cove cutter for where the back meets the arms. This would leave a very fine point on the backs that I’m not sure would survive without splintering. Does this seem doable?

Moving on to the beveled curve along the back of the chair. Currently it’s run through a curved fixture on the bandsaw, with the table tilted. Coincidentally, the bevel on the front of the arm runs pretty much the same profile. See pics 2 and 3.

I’m thinking that with a custom cutter matching that profile, we could crosscut the ends of the arms, backed up to avoid blowing it out, and then run the backs through a curved fixture to bevel them. Is this set up feasible? Power feeder is obviously a given in this scenario, although getting the right angle on it seems confusing.

Continuing the roundover profile down the beveled end of the arm seems tricky, worried about tearout there. Could we freehand this on the first cutter mentioned with a large enough cutter diameter to avoid tearout? Maybe climb cut on the router table otherwise?

For rounding the back corner, I would make a template and follow it with a compression bit on the router table, then use the same method as above to add the roundover profile.

Then for finish sanding, is a foam backed ROS the way to go, or are there flap/mop sanders that may make this easier?

This all makes sense in my head, but I don't have any experience with a shaper or how most production shops do things. If you all could sanity check this for me or have other suggestions I’d really appreciate it, and it would make me feel better about trying to pursue it. Thanks!


View higher quality, full size image (480 X 646)


View higher quality, full size image (1273 X 955)


View higher quality, full size image (1273 X 955)

4/29/24       #2: Improving Production Process With S ...
Dustin orth

A shaper would improve what you are describing but if I was starting to retool completely, I would go the CNC route for this project. It would be able to do most of what you need in one machine without removing the part to change setups. Those who are CNC experts will be better at laying out the process. Myself, even being extremely proficient on a shaper, I know the shaper could do it but lots of work still.

4/29/24       #3: Improving Production Process With S ...
Dave Edgerton

We do alot of work like this. Shaper is not going to do it all. Looks like you need a bunch of router table setups. Let me think about it.

4/29/24       #4: Improving Production Process With S ...
Jason Loyd Member

Thank you, I really appreciate you taking the time!

4/29/24       #5: Improving Production Process With S ...
Tom Gardiner

I second a cnc approach. Side legs drill groove profile cut.
Back piece drill, maybe 3d carve with a roughing pass. I am assuming there is a groove on the bottom side for the rope. This would have to include flipping the piece on the table.
Still use the drum sander to blend and finish the 3d carve.
Round over after assembly.

4/29/24       #6: Improving Production Process With S ...
Jason Loyd Member

I could see CNC for the arms. I've only ever ran a hobby level machine, but if we were pushing things harder on a pro machine, getting all that done in one step could be big. That could replace the pin router and gang-drill. It's hard to see in the picture, but the holes are countersunk on the inside of the arm to reduce strain on the rope, so the piece would need to be flipped or added some other way.

The holes on the back are 3" deep, would that not be a problem?

The issue I was running into with rounding over with a router after assembly is that inside corner where the arm meets the back. That's what got me thinking about the cove cutter, like how it's done in rail and stile construction. Any suggestions for a solution to that?

4/30/24       #7: Improving Production Process With S ...
Mitch Suber

Website: http://www.subercustomshutters.com

I think you are hearing some good suggestions. But what is your budget for equipment? Good routers seem like a good option for a round over, shaper is even better but more expensive up front. For small or light cuts we use several routers, for more dedicated task and larger cuts we go to our shaper. They both cut well and deliver the profiles we need, but using several routers minimizes set up times when switching cuts. However, stacking cutters seems to be something I would only do on my shaper.
Could you utilize a stop and start profile, rather than profiling the full length? That way you have a square edge where your joints meet.

4/30/24       #8: Improving Production Process With S ...
Jason Loyd Member

Oh yeah, stop and start does seem like a better solution to that. Thanks!

4/30/24       #9: Improving Production Process With S ...
RichC

What is your production rate? A lower end CNC with multiple heads could really put you into quick production. Possibly outsource some of the operations to a CNC shop to get back into production faster.

4/30/24       #10: Improving Production Process With S ...
Jason Loyd Member

Oh wow, never knew multi-spindle was an option! That makes it make more sense.

At our peak we were making 1100/yr.

5/1/24       #11: Improving Production Process With S ...
Tom Gardiner

3" deep holes are possible with a cnc with a 8" plus z axis travel. I would set these parts up in multiples on a fixture table to accept accurately dimensioned parts wedged in place. Half the table jigged for on side of the operations - the other half for flipped parts. Toolpathed in 10 -20 parts per table, the process time would likely be about 2 minuts per part total to drill groove, countersink. I still would round over after assembly.
Consider have a shoulder on the side rails to ease the inner corner problems of rounding. I do this with ash with success.
I rout and drill ash components more complex than these by the hundreds per day with simple wedge clamping. I order my stock in D4S with a corner round on all four edges which has improved my production and profit in a big way.


View higher quality, full size image (2976 X 2976)

5/1/24       #12: Improving Production Process With S ...
Jason Loyd Member

This is great, you've all got me thinking bigger than when I started. If we increase our frame production time, eventually we'll start bottle necking at finishing.

We've got a spray booth where we finish these off with two coats of marine spar varnish. Is parallelization the only option to increase throughput here? Minimizing worker effort and solvent exposure would go a long ways to making this more feasible, as we've had a harder time filling the finishing position than anything else.

I also wonder about a first coat of CPES. This is outdoor furniture, so increasing it's ability to weather the elements is a big concern. We were spending a lot of time filling checks and finish sanding to a high degree so that they didn't come through in the finish. Might a first coat of epoxy reduce the need for this?

Anyone have experience with the no-VOC versions of CPES? I assume the performance characteristics of these are not as desirable, but if they're acceptable it would make a big difference.

You all are great, thanks so much for helping me think this through!

5/1/24       #13: Improving Production Process With S ...
Jamie Hughes

If you don't want to go the full CNC route, I would also recommend checking out an inline profile shaper. Not the standard spindle shaper that most think about. (I use two old onsrud inline profile shapers) They can be picked up at auction quite cheaply some times and one man could do 1100 of your back "scoops" in a ten hour shift. A double spindle profile shaper could do it even quicker. The long groove in the arms would be the exact same, just a shaped cutter in one of the spindles. Pick up a cheap Cemco or such vertical boring machine to do your holes with and you are off to the races. Both of these things can be had at factory liquidation auctions for around 10k, and I feel pretty confident you could do the wood working side (not finishing or sanding) of 1100 of these things in less than two weeks with a single employee.

5/1/24       #14: Improving Production Process With S ...
Jason Loyd Member

I'm not seeing too much online about the operation of the inline profile shaper. Is that like a planer molder without the planing function?

5/2/24       #15: Improving Production Process With S ...
Jamie Hughes

Here are some picture of mine. Some call it a hydraulic spindle shaper as well. Mine is an onsrud W-684 H. Spindle floats in and out of the piece and the 9 foot bed pushes into it. Spindle can be made with any shape or angle of cutter. On bed, a form is made and bolted down to mimic the shape you want, and a wheel on the bottom of the spindle rides against the edge of the form. when you press the foot pedal, the bed moves to the right and the shaper is forced into the form with an air cylinder.


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)

5/2/24       #16: Improving Production Process With S ...
Jamie Hughes

I realize my explanation and pictures are sub par, so heres a short video link to it in action. This is a curved top rail of a bed.

5/2/24       #17: Improving Production Process With S ...
Jamie Hughes

VIDEO HERE.
https://drive.google.com/file/d/10QZATrebFAsKoCQKUAfcWIcVr6ToSAFH/view?usp=sharing

5/3/24       #18: Improving Production Process With S ...
Jason Loyd Member

Oh wow, that's perfect! Thanks for the video, mind expanding for sure.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!