Macasser ebony

2/15/16       
CBWW

I will be pricing a set of chairs in Macassar ebony and have a few questions on its workability. I have made plenty of chairs in mahogany with mortise and tenon joinery, bandsaw the parts out rough then flush cut them on a shaper with high speed steel knives run off a bearing. So the question- can I use a hollow chisel mortise or should I expect to use a router bit? Should I expect any problems flush cutting? With the cost of this material, I don't want to experiment or make mistakes.

2/16/16       #2: Macasser ebony ...
doug mclaren  Member

suggest you obtain sample and cut 1 typical mortise and tenon. you cant compare the density of mahogany to ebony, macasser or gabon.

2/16/16       #3: Macasser ebony ...
CBWW

I understand the density is different. I have machined gabon before for inlays bandings etc. but never did any joinery type work. Macassar is $85 a board foot so before I drop some cash to "experiment"
I was hoping for some feedback.

2/16/16       #4: Macasser ebony ...
doug mclaren  Member

like i said get a small sample, before you quote. you can get 2x2 12s from most retail outlets relatively cheap. especially compared to getting stuck in a money losing job. sizing to a jig on shaper for chairs sounds like a nightmare. mortises i would drill out first then route. kinda oily, but must be mschined slowly with
new sharp tooling

2/16/16       #5: Macasser ebony ...
CBWW

Thanks Doug. I'm leaning toward ordering a small chunk to try it out. AS far as flush cutting off a shaper, I have done probably a atleast a thousand chair parts over the years that way. Bandsawn to a line very close, tack on a pattern, and cut freehand off a rub collar. no problems on mahogany. I have the potential for 12 Rhulman chairs in Macassar so the experiments will be well worth it. Just hoping for some help here first though.

2/17/16       #6: Macasser ebony ...
John Costin

Danger, Danger, Will Robinson!

When you said "Ruhlmann" you set off a warning light ;8>). I know his work pretty well and have watched a lot of it being built by colleagues (not done it myself).

Two important details:
1. Macassar Ebony is very unstable and prone to checking, etc... -- especially in the solid.
2. Most of Ruhlmann's work was veneered on every surface -- legs and all.

No offense, but if you are thinking of doing Ruhlmann repros in solid Macassar I am going to wager that you don't have sufficient understanding of his work. This is some of the most technically challenging furniture that has ever been built and not to be undertaken lightly.

2/17/16       #7: Macasser ebony ...
doug mclaren  Member

again, ebony cant be compared to mahogany. you cant just tack a pattern. better to glue.

2/17/16       #8: Macasser ebony ...
doug mclaren  Member

i agree with john. consider build with mahogany and veneer with ebony

2/17/16       #9: Macasser ebony ...
Dennis

I've never built anything as large as a chair out of ebony but I do cut quite a bit of it for smaller items (fashion accessories). It is beautiful wood, but very dense, very brittle and, as mentioned, prone to splits and checks.
Steel cutters will not last long, I only use carbide router bit, burned up a new set of steel jointer knives just recently with ebony. Can't comment on how well it glues with conventional wood glue but works well with epoxy.
I would think that predrilling any fasteners would be a necessity keeping in mind the brittle nature of this material. Square chisel mortising - probably not going to work. The dust is NASTY breathing protection is very important.
I would agree with the other commenters about using ebony veneer instead of solid.

11/25/16       #10: Macasser ebony ...
Allan Member

Building chairs with veneer? Seriously?
Outside of a very flat seat, how would you do it?

We've done a lot of work with macassar ebony (disclaimer: we also sell it), it is very, very hard, but machines reasonably well with carbide tooling. You shouldn't have any problems with pattern routing using a shaper.
That said, cutting your mortises will be challenging. The macassar will make short work of your mortiser chisels. I suggest using a router to cut mortises. You will need to take very light cuts. If the wood begins to smell burnt, you'll have to take an even lighter cut.
Also, take the above advice and have dust collection, air filtering, and masks available, the dust is very irritating.

11/27/16       #11: Macasser ebony ...
Allan Member

Went back and looked up Ruhlmann chairs; pretty amazing stuff, a lot of it is upholstered. The arms on the upholstered chairs looked reasonable to do in solid wood.
It's true that any ebony has its share of checks, but the East Asian ebonies, to which Macassar belongs, are not as unstable as gaboon ebony, which is a smaller tree. Before machining our Macassar, we fill any checks with colored matched epoxy (usually black); it becomes indistinguishable from the wood and allows the Macassar to be machined without problems. If you don't prefill with epoxy, the existing checks will blow the machined piece apart.
One last observation, the Macassar ebony Ruhlmann chairs I saw on the web are black with orange stripes; Macassar that is typically available is black with white or tan stripes. I suspect that the black with orange stripe material, which is highly prized, is only available as veneer.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies

    Become a Sponsor today!