Toying with an idea

7/26/19       
Ex-Pat Member

Without getting into too much detail because the idea is still bouncing around in my head, but I am contemplating an idea for a coffee table with a solid top - probably plain sliced walnut. The finish would end up unbalanced top and bottom - bad juju, I know. I am thinking about using a sliding dovetail to attach the cross grain skirt pieces to the top, with the channel running out about 3/4" longer than the skirt in either direction. Would this allow for expansion and contraction in width while preventing cupping due to the differential in moisture change between the top and bottom surfaces? I know rift or quartered would be better, but I am probably going to make this out of drop from another project. I am not new to the fact that wood moves and designs need to keep this in mind, but while not new to the industry, I haven't made a lot of furniture. Do you think my strategy could work or is this an inherently flawed design that I should walk away from?

7/26/19       #2: Toying with an idea ...
Mark B Member

The sliding dovetail option has been done many times. Reasonable fit (not so tight that it could lock up when the skirt expands) and waxing the joint would allow just as much movement as a breadboard.

7/26/19       #3: Toying with an idea ...
rich c.

Why insist on an unbalanced finish on the top? Just do it right so you don't have to do extra work. Sliding dovetails that would totally eliminate any bow would have to be fit perfectly. Too loose and the top will cup, too tight and you won't get it driven home.

7/29/19       #5: Toying with an idea ...
Ex-Pat Member

That's the rub Rich. We have a bunch of vintage photos that were left in a house I inherited. I was thinking it would be cool to have the photos laid out on the top with about 1/8" of clear epoxy on top of them. I am not afraid of having to fit a dovetail correctly, what I am not sure of is if the idea is flawed from inception. I am just looking for a little advice before I take the thought much further.

7/29/19       #6: Toying with an idea ...
Josh Koschak Member

Can you put an 1/8" of epoxy on the underside as well?

7/29/19       #7: Toying with an idea ...
Ex-Pat Member

I'm not certain about epoxying the bottom side. That is definitely outside of my wheelhouse, I haven't used epoxy for much more than filling knotholes.

7/29/19       #8: Toying with an idea ...
rich c.

You do know that epoxy severely yellows with age, right? But I see more and more people say "epoxy" when they refer to just about every form of catalyzed resin made. I sure wouldn't waste walnut to make a decoupage project!!!

7/29/19       #9: Toying with an idea ...
Ex-Pat Member

Good to know about the yellowing Rich, thanks, I'll try to find a more appropriate coating. I wasn't really thinking decoupage level concentration of the photos, my intent is the wood would remain the star of the show. But regardless of personal taste, I appreciate the input. I am trying to think of things I could do that I haven't seen done, but Dave Sochar hits the nail on the head when he (frequently) points out that the reason designers have never seen something before is because someone already tried it and it was a really bad idea....

1/5/20       #10: Toying with an idea ...
tanya koio

When you have your own company and work hard for its success you want all of your employees do the same. But you can’t control their actions constantly. That’s why there is a perfect tool - motivational mystery shopping. I inculcated this tool with the help of these guys - https://scheduling-europe.com/service/mystery-shopping/motivational-mystery-shoppi
ng/. After their examination I know that my employees do everything and more for our company.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies

    Become a Sponsor today!