Adjustable pilot drill press bits

6/13/20       
Glenn W Healy Member

I’ve been in woodworking for 50 years, I worked many of my early years in the furniture manufacturing industry at a number of different shops, the one thing they all had in common was the an adjustable pilot and countersink bits they used on their drill press. It basically looks like a Kreg bit, but with a movable pilot running through its center. If anyone out there knows what I’m talking about, or better yet, knows where I could find one, I would really appreciate it.

6/13/20       #2: Adjustable pilot drill press bits ...
Mark B Member

If Im thinking of what your thinking Amana sells them.

Amana Tool Face Frame Counterbore Drill

6/13/20       #3: Adjustable pilot drill press bits ...
Mark B Member

Or perhaps these:

Amana Tool Shankless Counterbore Bits

6/13/20       #4: Adjustable pilot drill press bits ...
Jim Acconcio

Website: http://designerclosets.com

The drills are made by W.L. Fuller They are made in RI.

W.L. Fuller Drill Stops

6/13/20       #5: Adjustable pilot drill press bits ...
TonyF

Glenn Healy:

As Jim Acconcio points out, these were made by Fuller, and are still available, even as made by other manufacturers. 30 years ago I was gifted a set of these in a mahogany box (hate to think what that costs now)

The ones I have came with tapered twist drill bits, so if you need them for the old style wood screws, that would be what you want. I replaced those with straight twist bits, which work better for drywall screws and other straight shank screws.

The Fuller set had plug cutters that made plugs to fit the deeper counterbore, but if all you need is the straight bits with a tapered counterbore to accommodate the screw head, you might see about the set in the link.

Hope this helps.
TonyF

Amana Countersink set

6/15/20       #6: Adjustable pilot drill press bits ...
Mark B Member

I personally cant stand the drill/counterbores/countersinks that set-screw onto the flutes of a standard or taper drill. They grip horribly (set screw), they jam/pack up miserably as well. Even the Fullers, which are great, are not so great.

When he said "Kreg bit" I didnt think of anything with regards to a drill/countersink or a simple stop collar on a drill bit.

Assumed he was looking for a piloted flat bottomed hole similar to what a Kreg bit drills but allowing you to set the pilot drill depth.

We run the adjustable face frame bits from Amana in a couple operations that allow for a clean 3/8" bore for a plug and we can set the pilot depth as needed (not possible with a Kreg bit). The fuller counterbores work for a 3/8" plug but again having to set screw on the flutes kinda stinks.

6/15/20       #7: Adjustable pilot drill press bits ...
Jim Acconcio

Fuller Page 29 Countersinks · Counterbores · · Adjustable Countersinks and Counterbores for deep hole drilling made of High Carbon Steel All sizes are 4-1/2” overall, 2-1/2” of twist, 1/2” split shank, and has one set screw.
This countersink has a Adjustable center drill

6/15/20       #8: Adjustable pilot drill press bits ...
Mark B Member

My page 29 shows a 5C option which is phenomenal for that counterbore provided you have 5C and a controlled feed where the feed cant be taken away from you. I have some piloted auger style counterbores but no different than a piloted electricians auger, hand feeding, they can just burry themselves into the work if they are not controlled feed or fed with a stop.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies

    Become a Sponsor today!