Mitered corners on solid table

12/3/20       
Nick Cook Member

Website: http://kootenaicabinets.com

I have a customer that sends me pictures of tables that appear to be solid wood. They have edge glued field area with solid wood wrapped around the whole table with mitered corners. I told her the mitered corners will crack. She doesn't believe me. Or is there a joinery method I don't understand? The corners she wants and the pictures appear to have very tight mitered seams.

12/3/20       #2: Mitered corners on solid table ...
Tom Gardiner

My first thought is how does she know it is solid wood? You could offer random matched veneer and no one would be the wiser

12/4/20       #3: Mitered corners on solid table ...
Nick Cook Member

Website: http://kootenaicabinets.com

I'm just curious if a solid wood wrapped table with mitered corners is good practice in furniture making, I've been in woodworking now for 29 years and this design slipped by me as a good design when it comes to seasonal wood movement. But I thought maybe I'd learn some new trick in woodworking. Am I wrong? I told the customer it's a bad design and I would not guarantee the tightness of the corners. She's second guessing me and showing me pictures of antique and current tables with this design.

12/4/20       #4: Mitered corners on solid table ...
Rocket

The customer has absolutely no clue what they're talking about. Zero. I can build a solid wood table with a miter border right now then take a picture showing tight joints...then the seasons happen. Sounds like the type of client I would add a PITA surcharge to any work and document EVERYTHING in writing, which is good practice regardless.

12/4/20       #5: Mitered corners on solid table ...
Nick Cook Member

Website: http://kootenaicabinets.com

Thank you, I didn't think I was going crazy or missing some new (after 6000 years of woodworking history) technique.

12/4/20       #6: Mitered corners on solid table ...
Jack Mazzuchelli  Member

Consider lock miter joints, pia but when done well they dont come apart. Basically a tongue and groove miter joint

12/4/20       #7: Mitered corners on solid table ...
Nick Cook Member

Website: http://kootenaicabinets.com

Jack,

A tongue and groove miter joint. I've refurbished these kinds of joints on wood boat windshield frames. I don't believe they can stand up to the expansion and contraction of a Quarter Sawn white oak edge glued panels that's about 16 to 18 inches wide.

12/4/20       #8: Mitered corners on solid table ...
Dave Sochar Member

If she can offer you some antique samples - examine them closely. If there are any - and a that is a great big if - then they exist by luck or exception. Not by common construction. Often the table was quartered lumber and used as a boards, with the mitered rim added later, after the table had found its equilibrium. We do not have that luxury.

Secondly, you will not see that design in antiques for one good reason - they cannot build them that way.

Remember the two Rules: 1.Solid wood will move. 2. Woodworkers will forever disagree on when, where, how much and why.

My bet is the a the table field is veneered, and the rim is also veneered. We tend to forget that any manufacturer must have two things: ease of construction, and predictability in manufacturing. Solid wood gives most manufacturers fits precisely because it does move. They will avoid it for all the reasons we would use it. They will be attracted to all veneered parts since they are predictable - or, more predictable than solid. Cores of MDF or particle board will hold a miter as well as the veneers. Sizes of components will be consistent and call backs will drop to zero.

12/4/20       #9: Mitered corners on solid table ...
Glen Harwell

Typical of a veneered top with solid edge detail. We do them all the time. You wrap a solid top with a solid edge and it will crack, period.

12/4/20       #10: Mitered corners on solid table ...
duster

I've done a lot of these type of table tops. The only way I'll do it is with a veneer center panel, then wrap it with a mitered solid wood border. I learned the hard way long ago that wrapping a solid wood top is just a disaster waiting for seasonal wood movement to occur. Either the miters will open or the panel will crack.

The tables shown were built this way with alder and oak, and have held up for years with no issues.


View higher quality, full size image (800 X 417)


View higher quality, full size image (608 X 336)

12/4/20       #11: Mitered corners on solid table ...
duster

Here are couple more in walnut and oak with the same construction method. As the others here have stated, it's the best way to achieve a long term good result.

12/4/20       #12: Mitered corners on solid table ...
duster

Here's the walnut one.

12/4/20       #13: Mitered corners on solid table ...
duster

Hmm.. the walnut photo won't load...

12/4/20       #14: Mitered corners on solid table ...
Mark B Member

Just tell her you'll gladly build to her specifications and take her money along with a signed contract that she specified the construction method and takes all responsibility for any future defect.

As awful as that concept is, rather than us makers having to reason, debate, argue, edu-ma-cate, or worse, walk away from a paying job, the misery foisted on us by the Pinterest/HGTV mob may just have to learn their lessons the hard way if they so choose.

If after a brief explanation she still balk's/argues, just ask her to put in writing how she specifies the table to be constructed and let her sign the contract.

12/4/20       #15: Mitered corners on solid table ...
rich c

You might get away with if if the center of the table is very strictly quarter sawn, and the miter frame around the outside is narrow. The major seasonal change direction with true quarter sawn is vertical. Get to rift sawn and you will start to get a little width movement too. A low movement species will also help.

12/5/20       #16: Mitered corners on solid table ...
D Brown

Even though we know it is not the best way to go, you could think of it as more of a floating center panel in a groove with a deliberate notch or type of vee groove around the edge to hide any movement.
It would be like a 4 sided breadboard end. good luck.

12/19/20       #17: Mitered corners on solid table ...
Matt Calnen

Can you provide pictures of what she wants? I have made several tables with an applied wood molding mitered around a solid wood top. As D Brown said, there are ways to put the wood in a groove or channel that allow for movement.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America

    Become a Sponsor today!