Recipe for failure

3/31/23       
Mike Barker  Member

I have been asked to build this table. The shelf at the bottom noting the grain direction and that of the stretcher looks like a recipe for failure. The widest part of the bottom is 12". Any suggestions to make this work. I suggested to use a trestled beam in place of the shelf. She isn't convinced.


View higher quality, full size image (3024 X 1451)

3/31/23       #2: Recipe for failure ...
Bill

I think there are ways around the problem. Fasten the center only hidden underneath and let the ends float so they can move with humidity.

If you feel that is not enough structure you could attach the shelf like a table top so it can move as much as it needs to.

Good luck.

4/1/23       #3: Recipe for failure ...
Tom Gardiner

It appears the designer wants to make the joint to be a visual feature with the lengthwise stretcher let into the cross braces. There will be a stress riser at the base of the tenons. I would suggest fully enclosed tenons with the outer mortises lengthened to allow some movement. Glue the central joints, peg the outer ones. To add visual interest you can do through tenons but you will have to be sneaky with the outer ones to avoid showing the oversized mortises. I would make end grain caps to imitate the through tenons.

4/1/23       #4: Recipe for failure ...
RichC

If you use quarter sawn, wood movement won't be a problem at the joint.

4/5/23       #5: Recipe for failure ...
Mike Barker  Member

Thank you all so much for your help. I think I can sell her on the through tenons. I feel more comfortable allowing for wood movement. I will have to get a little crafty with small tenons on the end grain caps.

5/2/23       #6: Recipe for failure ...
Chippy1987 Member

Love to see the end product there @MarkBaker!

6/8/23       #7: Recipe for failure ...
Mike Barker  Member

Website: http://wooddimensionsky.com

The table is finally complete. The lumber was sourced from a downed tree on the client's property. Quarter sawn and dried to 6-8%MC. I decided I would try something a little different, using relief cuts to address my concerns about movement in the bottom stretcher. Honestly I'm kinda keeping my fingers crossed.


View higher quality, full size image (2412 X 1908)


View higher quality, full size image (2868 X 1908)

6/13/23       #8: Recipe for failure ...
Dave Sochar Member

Website: http://www.acornwoodworks.com

Nice work. Your decision to make relief cuts in the stretcher is a good one. It is not hard to find precedent on the detail. Three small cross sections will have negligible movement compared to one larger joint.

8/29/23       #9: Recipe for failure ...
David William  Member

Website: http://www.bergenfurniturenj.com/

Building the table with the shelf as designed might indeed pose a challenge due to potential wood movement issues. To ensure stability, consider using breadboard ends on the shelf and stretcher. This allows for wood expansion while maintaining structural integrity. If your client prefers the original design, using a stable wood species and accounting for seasonal wood movement with proper joinery could help. However, a trestled beam could provide a more reliable solution, offering support without compromising aesthetics. It's important to discuss these options and their implications with your client to find a suitable compromise.

11/15/23       #10: Recipe for failure ...
Mohammad Sheikh Foyjul Islam  Member

Website: https://elegantinterior.com.au

The design in the image and the final work look so different... You make the work so beautiful and awesome.. Nice work..


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Shop Gear Inc.
      Distributor of Co-matic Power Feeders, Le-matic Portable Edgebanders, and Supplier of Woodworking Machinery, Tooling and Accessories in North America

    Become a Sponsor today!