Cherry Supplier
12/20/23
Website: http://woodcontours.net
I need a new supplier for cherry. Anyone in the NJ ,lower hudson valley NY, or CT area that has a recommendation at reasonable prices. Usually get 200 bf at a time. My supplier in white plains NY sent me a load with honeycomb and was not very apologetic. Thanks
12/21/23 #2: Cherry Supplier ...
Howard, I’ve had good luck with Rex Lumber out of South Windsor CT. Never had to send anything back.
12/21/23 #3: Cherry Supplier ...
What do you consider a reasonable price?
12/23/23 #4: Cherry Supplier ...
Website: http://woodcontours.net
I've been paying around $5 per bf for 4/4
12/23/23 #5: Cherry Supplier ...
For FAS? No wonder you need a new supplier. That guy has to be cutting corners someplace.
12/23/23 #6: Cherry Supplier ...
Rich, Cherry has been dirt cheap for several years now. $5 a board foot seem quite high to me.
View higher quality, full size image (750 X 1334)
12/24/23 #7: Cherry Supplier ...
$2.50 a board foot for 4/4 in the rough. Western PA
1/14/24 #8: Cherry Supplier ...
Cherry is not very hot right now, so I haven't bought any recently. About a year ago however, I bought a load of FAS 4/4 cherry cheaper than what I was paying for paint grade soft maple. It was around 2.00/bdft if I remember correctly. I'm in eastern PA, but I cant imagine you should be paying anywhere near $5 in your area unless you're going to a mom & pop where they let you dig thru their stacks to buy 3 boards.
4/13/24 #9: Cherry Supplier ...
Rex lumber is good. Steve H wall out of NC does 100bf packs motor freight and can be trusted.