Laminating and Solid Surfacing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 1/4" Corian over plywood

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

1/4" Corian over plywood

12/18/12       
Leland Thomasset

Website: http://www.cnc-cabinetparts.com

I am doing a desk or 5 with 1/4" corian laminated to a substrate of which I can choose. I will be mitering all corners, front,sides,top and back edges. Miter fold actually. The units are 5'x3'x2.5'. I would like to use contact cement to adhere to the substrate. This could be plywood arch. Choice or mdf my thought as it is more stable and consistent. Any thoughts on this. I was thinking contact would have a little flexibility. I will be seaming miters with seam kit.

12/18/12       #2: 1/4" Corian over plywood ...
Marty Member

G'day Mate
I'd glue up all the corian first then drop over my substrate using silicone. Over time the contact glue will harden up more than you expect.

Merry Christmas

Marty

12/18/12       #3: 1/4" Corian over plywood ...
Dave Edgerton  Member

No contact cement for corian. You have to use either the 2 part epoxy for seaming or silicone. The silicone would give you a bond only where it contacts and will not be structural if this is what you are looking for. I would get some documentation on how to do this from the manufacturer.

12/19/12       #4: 1/4" Corian over plywood ...
Snaglpuss

I second the idea by Marty.
Have done lots of similar stuff using silicone.

12/19/12       #5: 1/4" Corian over plywood ...
Leland Thomasset

Marty,

So you would build the structure and then fit the mitered corian then set silicone bead then corian seam kit the miters. Ok this is something I considered but I was thinking the silicone would be too thick and it would not allow the proper fit.

12/19/12       #6: 1/4" Corian over plywood ...
Ken Dolph  Member

Website: sites.google.com/site/coriartinc

Leland

I would not do it at all. There are reasons that the back side of 1/4" Corian says "Vertical Use Only". In the 90s the motor home industry tried this and had many failures over the years.

The wood substrate will expand/contract with humidity changes. The Corian will expand/contract with temperatures. On any given day the total of the changes will be twice as great as those you need to take into account with wood construction alone. The Corian alone can change 1/16" over 6' in normal home temperature changes.

1/4" Corian is, in most cases, no less expensive than 1/2" and it does not need a substrate. In fact, it is not recommended. So you would be going through more work and expense to have an inferior product.

12/19/12       #8: 1/4" Corian over plywood ...
Marty Member

G'day,
Cut, glue and fold your corian using their correct adhesive. Use your finger to smooth the adhesive around the inside but leaving a nice "cove" as a backing and added strength.
Under cut your substrate about 1.5mm all sides and chamfer where required to clear your "cove". Seal your subtrate (MDF) both sides and all edges.
When applying your silicone to the flat surface do so in blobs, so as not to create "air locks" or sealed sections.
Now carefully caulk the under side again leaving small sections clear so as not to trap any air.

Cheers Marty

12/19/12       #9: 1/4" Corian over plywood ...
Leland Thomasset  Member

Website: http://www.cnc-cabinetparts.com

Thank you Marty,

This makes sense to me

12/19/12       #10: 1/4" Corian over plywood ...
Marty Member

Not a problem mate.
Just remember lots of smaller blobs are better than a few bigger ones and don't create any air pockets.

You'll be fine.

Cheers Marty

12/23/12       #11: 1/4" Corian over plywood ...
Mike

Just use 1/2" corian. I don't think your saving any money by using 1/4" material. I just took a look at my price list, and the 1/2" glacier white actually costs less, than the 1/4" material.

Gluing solid surface to plywood with contact cement is a no go. Backing with plywood, is not entirely recommended either. If you do go this route use coin sized dabs of silicone. This will allow movement in the substrate, and or solid surface material.

By the nature of your question, I would recommend that you take a look at the corian fab guide. There is allot of information that would answer your question.

http://www2.dupont.com/Surfaces/en_US/assets/pdf/Fab-Manual-for-print
ing.pdf

If your getting the corian on the "grey" market, you can generally get the corian adhesives, and guns via ebay.

12/23/12       #12: 1/4" Corian over plywood ...
Leland Thomasset  Member

Website: http://www.cnc-cabinetparts.com

No grey market corian, this is all above board it is at the design of architect that we are going this route. I know 1/2 is the same or less expesive. The weight would be out of control on these units. Site fabrication would be a bad idea. So I want to see what others have done and get the great feed back that you and all the other contributers have provided.

Thanks

12/29/12       #14: 1/4" Corian over plywood ...
mike

just a note- If you are expecting to get the corian 10yr warranty then just about everything you are doing is a no-no. Correct way would be 1/2" corian over perimeter only support w/ dabs of silicone.

1/13/13       #15: 1/4" Corian over plywood ...
Terry LaFond Member

Website: terrylafond2709@gmail.com

No need to miter solid surface. A good joint is invisible or very near that.

2/3/13       #16: 1/4" Corian over plywood ...
Erlewine

What was your reason for using the 1/4 inch would be my question. Personally I found it to be quite brittle and not easy to work with like the 1/2..

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)