Subject: Re: How to clamp V-Grooved Solid Surface C-Tops

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

How to clamp V-Grooved Solid Surface C-Tops

10/8/15       
David Smith  Member

Website: http://www.crowescabinets.com

We are looking for feedback on clamping the front edge of solid surface tops that are V-Grooved and then folded over. We use a profilematic V-grooving machine and have been having issues with how the seam looks after we apply glue, fold it over, then sand and polish. Most of the time we can see a seam line as well voids (sometimes large) within that seam where glue should be. Our clamping method is just to apply a thin bead of adhesive, fold the edge over, then just use tape to hold it in place.

This has been driving us nuts for a very long time now. We have tried changing the angle on our cutters, played with how much glue we put into the seam, used different tapes, etc...

Since we got machine i have felt that we got better results and seams that you can barely see by doing it the old fashion way which is the build up method. With the right color and pattern and if fabricated properly, it should be very difficult for someone to locate the seam. But with using this machine it is just so obvious that there is a seam and it drives me nuts.

So, is there anyone out there that also uses the V-groove method to fab solid surface tops and what method of clamping are you using to get successful results? Any feedback or recommendations would be great.

Also, we typically fabricate tops that are 25" wide with a 1 1/2" fron edge.

Thank you!

Dave

10/8/15       #2: How to clamp V-Grooved Solid Surfac ...
rich c.

Are you running a full strip of tape centered on the seam as a hinge before folding?

10/9/15       #3: How to clamp V-Grooved Solid Surfac ...
David Smith  Member

Website: http://www.crowescabinets.com

Im sorry,yes we are.

10/20/15       #4: How to clamp V-Grooved Solid Surfac ...
Dave Edgerton  Member

hot glue a beveled strip of wood on each length and use spring clamps. You are not getting the pressure you need by folding the edge over and you will see the seam. make the strip triangluar so that when you glue the strip the pressure from the clamp is perpendicular to the joint.

10/21/15       #5: How to clamp V-Grooved Solid Surfac ...
Dave Edgerton  Member

Like this


View higher quality, full size image (840 X 718)

10/21/15       #6: How to clamp V-Grooved Solid Surfac ...
David Smith

Dave, thanks you for the tip! I will try this the next time we run solid surface throught the shop, which will be soon. The only problem with that method is how much labor is added when your doing 20 tops...

10/28/15       #7: How to clamp V-Grooved Solid Surfac ...
Matt

David,
Something you might check...on our Profilematic, the aluminum anvil roller was poorly machined. The bearing pockets were not even remotely concentric to the outside diameter. This caused the v-groove to vary in depth for every revolution of the roller. A local machine shop trued it up for us and the results were much better.

10/29/15       #8: How to clamp V-Grooved Solid Surfac ...
David Smith

Matt, Thank you for your response. I WILL look into this. I just looked at that part and it does seem to have some damage to it already. And it makes sense that if it's off, so will the depth of your cut.. Great response..

10/29/15       #9: How to clamp V-Grooved Solid Surfac ...
Matt

David, Glad to help.

Regarding your original question on how to clamp the miter-folded edge; please see the attached sketch. I have a couple benches configured this way. Fast, easy and perfect edges every time. 1-5/8" tall curb w/ 1/4" foam. A 4-5/8" curb is used for folded back splash.

Good luck to you.

Matt

Click the link below to download the file included with this post.

Folding_curb_2.pdf

10/29/15       #10: How to clamp V-Grooved Solid Surfac ...
David Smith

Matt, do you clamp the top in place?

So, you just fold the edge over and then push it up against the curb?

10/29/15       #11: How to clamp V-Grooved Solid Surfac ...
Matt

Large (i.e. heavy) tops just push in place. Sometimes a small one needs a clamp.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Today's Sponsors
    • J&P Machines
      Design and Production of Custom Equipment for the Manufacturing Industry
    • Template Services
      Professional Moulding Design and Template Making Service
    • WOODWEB, Inc.
      The Information Resource for the Woodworking Industries
    • Wood Doctor's Rx, LLC
      Wood Processing Seminars, Kiln Operators Seminar & Training, and Advanced Drying Evaluation & Training
    • Biesse America
      Woodworking Machinery - Machining Centers, Edge Banders, Feeders/Stackers, Panel Sizing Centers
    • EX-FACTORY
      Importer and Dealer of New and Used Woodworking Machinery
    • SAMES KREMLIN formerly EXEL North America
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Elias Woodwork & Manufacturing
      Solid Wood Cabinet Doors, Furniture, Dovetail Drawers, Mouldings, and Related Items
    • Original Saw Company
      Industrial Radial Arm Saws
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • RT Machine Co.
      Stocking Distributor of New and Used Woodworking Machinery
    • EnRoute Software
      CAD CAM Software by SAi Featuring 2D/3D Design and Toolpath Functions, Nesting, Rapid Texture and More, with Low-Cost Monthly Subscriptions Available

    Become a Sponsor today!