Subject: Re: CNC through protective film

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

CNC through protective film

10/16/19       
Mark B Member

Do any of you cut solid surface on the CNC leaving the protective film on the sheets? Have one coming up with a lot of 4x8 and 5x8 panels and some machining would be easier done on the CNC but I'd like to leave the film on for shipping. The concern that flashed into my head was a loose corner of film or a small hole cutout and the film grabbing hold of the bit and balling up under the spindle and all heck breaks loose. I can stand there and tend but Im sure if it would happen it'd be the instant my attention lapses.

10/16/19       #2: CNC through protective film ...
Nathan W Member

Hi Mark,

Ive never done it with solid surface, we dont touch the stuff, but we have done lots of acrylic panels and laminate panels with film on them. As long as the film hasnt rolled or started peeling near where you want to machine you should be fine. We have two machine centres, one rail and pod, and one vertical machine. I would suggeste to not run anything with a film on a vertical machine, as it will roll as it slides back and forth, that causes all sorts of problems, but a table or pod machine shouldnt be an issue.

10/16/19       #3: CNC through protective film ...
Mark B Member

Thanks Nathan,
We are opting to run face down with the film. That should give a bit more peace of mind as well with the film pinched between the spoilboard and the material.

10/16/19       #4: CNC through protective film ...
Jared

I always cut with film on and most of the time facing up, and have never had it tangle. Mostly downshear cutters also.

10/12/21       #5: CNC through protective film ...
John Member

When the solid surface does have the protective film on it we always leave it on when cutting. We cut it face down(film side down) and we don't cut through the film.

When doing miter fold front edges this film still being in place is great. Most of the time we can fold the front edge using the film in place instead of tape

10/12/21       #6: CNC through protective film ...
Mark B

Thanks John,
I had always been more concerned with film side up which I not too long ago concluded is a bad idea unless the film is very well adhered and fully intact. We often get sheets where the film is loose on the corners or a pretty low adhesion film. When I initially asked about this we had some sheets like that and I opted to cut them face down for that reason.

Several months ago though we were running some sheets that had some loose corners and needed to cut them face side up and it was a terrible idea. One of those loose tags wrapped the spindle and stripped a large corner off the sheet and started whipping like a fan. Knocked the dust shoe off before someone got to the Estop lucky it wasnt worse or a spindle.

Ive always consdered using the film for folding but again it seems a lot of the material we get it has been slid onto a load out of the stack and the film is knicked or even small tears. Not saying we never get nice film but its not the norm for us.

Thanks

1/20/24       #7: CNC through protective film ...
z Member

i have found that it is the air blast that causes it more than anything.
We cut a lot lot of acrylic, laminate, solid surface and we leave the cover plastic on everything. For acrylic, hdpe, solid surface cut face up and we run the 64-000 & 65-000. try moving your air blast nozzle and see if that helps

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Today's Sponsors
    • Centex Automation
      New and Used Machinery sales and service
    • Professional Machinery Group
      New and Used Machinery Serving the Needs of the Professional Woodworker
    • Elias Woodwork & Manufacturing
      Solid Wood Cabinet Doors, Furniture, Dovetail Drawers, Mouldings, and Related Items
    • MachineryMax
      New and Used Machinery for the Professional Woodworker
    • W. Moore Profiles, Ltd.
      Supplying Knives and Cutters to the Woodworking Industry - Standard and Custom Profiles Available
    • Industrial CNC
      Affordable, Easy, Industrial Grade CNC Routers for Woodworking and Cabinetmaking - Free Lifetime Support
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • J&P Machines
      Design and Production of Custom Equipment for the Manufacturing Industry
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • CabMaster Software
      The Easiest Custom Cabinetry Software
    • Lignomat
      Moisture Meters and Monitoring Systems

    Become a Sponsor today!