Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Wood Boring Insect Larva Prevention

5/8/15       
Charles Hanna

Does anyone have any suggestions or recomendations for the prevention of PPB and other wood borer larva from hatching

We built a 12' X 24' Log Cabin using air dried 6" X 8" SYP dovetail logs
The logs wear sticker stacked under cover for 2 years
I was unable to get the logs to the dry kiln
The current logs shell MC is averaging
8 percent
What would be the best way protect this structure from wood borers and the exterior from weather ?
This cabin was built to be sold and ship out on a truck ,
All recomendations are welocome !
Thanks Y'all
Charles Hanna

5/8/15       #2: Wood Boring Insect Larva Prevention ...
Charles Hanna

This is the a photo of the portable cabin in under construction being built o sale


View higher quality, full size image (1200 X 1600)

5/8/15       #3: Wood Boring Insect Larva Prevention ...
John S  Member

I am far from an expert on the topic, but I used to own and live in a log house. Every two or three years I had to spray on some sort of sealer/stain/protectant which was supposed to guard against insect damage. It was NASTY stuff, I had to wear a full head to toe protective suit and if you got a drop on your skin, it burned like crazy. But it did work.

I don't remember the brand name anymore, but I got it from one of the local log house builders in my area.

5/8/15       #4: Wood Boring Insect Larva Prevention ...
Charles Hanna

Thank You For your input
John S

5/9/15       #5: Wood Boring Insect Larva Prevention ...
Gene Wengert-Wood Doc

The risk of PPB with SYP is close to zero. The lyctid PPB prefers grainy hardwoods, so softwoods are not at risk. The low MC eliminates damage from most other insects. However, because you need a chemical on the inside of the house that is safe for humans, does not smell, lasts a long time, penetrates to wood a little bit, does not color the wood, does not add water back, and maybe a few more, you have no chemical that you can use. You could fumigate the house (expensive and not long lasting) to kill any existing insects if you do find some activity in the future.

On the outside, the requirements change, so there are some chemicals that can be used. Unfortunately, borates can easily leach out from rain wetting or other water sources. Even so, repeated applications to you get reasonable penetration so the chemical retention is high enough to work well, is probably your best option to avoid new insects from entering. Any insects in the wood now would be hard to reach with any chemical, so fumigation is probably the only choice. On the other hand, some insects do so little damage and will not likely ever mate, that they are ignored. In addition, we know that almost all insects find wet wood is easier to eat, so you will help matters if you keep the exterior wall as dry as possible, including no plants near the wall (allowing the wall to dry quickly if wetted) and a water repellant coating on the wood, including the end grain. With a new design, we also want to keep the wood away from the soil at least a foot and, if using a crawl space, use a soil blanket and foundation venting- - standard construction techniques.

5/9/15       #6: Wood Boring Insect Larva Prevention ...
Charles

Thank You Very Much
Dr Gene !

5/13/15       #7: Wood Boring Insect Larva Prevention ...
ChicagoGangsta

I assume there is neither snow nor wind load where that structure is - that roof would fold up in a stiff breeze, from the looks of that truss system, if I can use those words loosely enough.

Next time, hire an engineer to design the roof. That thing will not last long in the real world.

5/13/15       #8: Wood Boring Insect Larva Prevention ...
Charles

The log cabin doesn't have a roof on it
What are you talking about ?

5/19/15       #9: Wood Boring Insect Larva Prevention ...
Bugsy

One sure-fire way to get rid of the bugs is to burn that thing down now.

I'll provide the gasoline and a match.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)