Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Mini Kiln questions

7/19/21       
Dan Wolf Member

Website: http://dwolfwooddesigns.com

I just built a mini version of a VA tech solar kiln (4’ x 2.5’ by 2.5’ ). I did it completely out of scrap material! I only had to buy screws and two small fans! I am “turning it on” tomorrow. I gather 2 to 4 feet long local logs from neighbors and arborists and make bowls, boxes, vases, puzzles, pepper mills, and whatever looks interesting. I work with many local woods.

Three questions at this point:
1. Since this is a small kiln with a roof angle of 33 degrees (I live in North Texas) – it is a good idea to tilt it 10 or 15 degrees back in May June, July and 10 or 15 degrees forward in Nov, Dec, Jan? Is it worth putting the kiln on a large lazy susan to track the sun? I realize that this would not work for a full size kiln, but mine is small/light enough that I think I can figure it out, but is it worth it?

2. I want to dry fairly thick wood blanks. Like 3” x 3” x 7” for pepper mills, 4”x4”x12” for turning projects and 7”x5”x4” for boxes (I use the bark edge as the top, these can’t be made from store bought 4/4 lumber). I don’t care how warped or cracked the get during the drying process – I will joint/plane them into rectangular blocks and cracks get enhanced with colored epoxy later. But they must be dry all the way through (or they warp when they are worked). Any advice on drying thick, but small, blocks of wood? I will be mixing these thick blanks with 4/4 boards – any issues with mixing different thickness woods in a mini kiln? Any issues with mixing different types of wood in a mini kiln (beside the issues with mulberry, osage orange and black locust mentioned in another post). I use pecan, walnut, mesquite, lace bark elm, ash, hackberry, bradford pear, chinaberry, post oak, cottonwood and sycamore. Note: I turn all my bowls green and will not be using the kiln to dry bowls.

3. Any other issues I may run into with a mini kiln?

Thanks in advance for any advice.

7/21/21       #3: Mini Kiln questions ...
rich c

You'll need a super slow cycle at the beginning. A solar kiln in Texas in the summer can make a lot of firewood out of thick stock in a couple of days. Osage will need to take at least 4 times longer than ash. So mixing species will definitely be an issue. I would definitely not cut the blanks to length and put them in the kiln. With more end grain exposure your degrade will certainly go up.

7/24/21       #4: Mini Kiln questions ...
Gene wengert-wood Doctor

Do not worry about the roof angle. Thirty degrees or whatever you have is fine.

Consult DRYING HARDWOOD LUMBER to learn more about drying. As the kiln was designed for 1” oak, drying thicker stock of hardwoods will likely require slowing it down by covering part of the collector.

9/15/21       #5: Mini Kiln update ...
Dan Wolf

Website: dwolfwooddesigns.com

Thanks for the advice. Update: I put about 80 board feet of a mix of 4/4, 6/4, 8/4 and 16/4 mesquite, walnut, lace bark elm, bradford pear and pecan. It works!!! Drying speeds vary greatly. The bradford pear and lace bark elm are the fastest followed by pecan and walnut. Mesquite is the slowest. Almost no cracking so far, bradford pear warps alot and lace bark elm warps a little, all others are fine. Mixing woods and thicknesses seems to be OK (at least so far). Every two weeks I go through it to pull out dry wood. I am weighing every piece rather than relying on a moisture meter. I don't trust mm especially on 4" thick wood. 4/4 and 6/4 are mostly dry. I expect the 16/4 to take 10-14 weeks to fully dry. The kiln opens up a great source for what is effectively "free" local wood for my craft business. And I can dry really thick wood for crafts. This website was key in helping me build a successful mini kiln, Thanks!! I'll update again in a few months. In the mean time I need to find some more logs....

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery

    Become a Sponsor today!