Drying kiln using a reefer body and Nyle dehumidifier

9/6/14       
Ed Schmidt Member

I'd like to know who has experience utilizing a reefer truck body with a Nyle. I've found a 22' aluminum composite reefer with diamond plate floor and insulated roll up door for a good price. I'd like to match it with a Nyle l-53. Is this advisable, what questions should I be asking.

I'm limited in space and this size would work well.

9/7/14       #2: Drying kiln using a reefer body and ...
Jerry

I have a 53' reefer trailer with hinged doors. And use the nyle L200M works good but A witch to load and unload.

9/14/14       #3: Drying kiln using a reefer body and ...
Bill Stuewe Member

I have a 40' with a Nyle L200 and a track system to load?unload. Works pretty good


View higher quality, full size image (640 X 480)


View higher quality, full size image (480 X 640)


View higher quality, full size image (480 X 640)

9/15/14       #4: Drying kiln using a reefer body and ...
al

Hey Bill that looks awesome! Where does the dehumidifier unit go? Also are those fans in that unit hanging from ceiling? I have had trouble finding info on how DH kilns are set up.
Thanks,
Al

9/15/14       #5: Drying kiln using a reefer body and ...
Bill Stuewe Member

If you look about half way down on the left in the top picture there is a cut out that the Nyle sits in.The first picture below is a picture of the kiln at its original location showing the outside addition that houses the unit. There is an access door to the controller on the left outside of the buildout and it is isolated/insulated from the inside of the kiln so that it does not get too hot.

Screw a 2x4 to the top of the kiln and fir down with a baffle that houses the fans--mine has 7 fans that I can individually control I also have a partition that I can add to block/divide the kiln in half that I use when I do not have a full load. This one will hold about 6000bf and that is too much for the Nyle L200 It was designed to dry only mesquite and it works for that purpose. I partition it for other woods.


View higher quality, full size image (640 X 480)


View higher quality, full size image (480 X 640)


View higher quality, full size image (640 X 480)

9/15/14       #6: Drying kiln using a reefer body and ...
al

I wonder if you could help me with another question. Ebac brand DH kilns come in a smaller
size than the Nyle and would probably be better for the amounts I want to dry. They say unit cannot go more than 113 degrees. If you need to get wood to 130 degrees to kill bugs how would this be accomplished?

Thanks again I'm really interested in a DH kiln and trying to learn.

9/15/14       #7: Drying kiln using a reefer body and ...
Tennessee Tim

Website: http://www.tsmfarms.com

I didn't go with the reefer body but something wider. The reefer body is awful tight with the air flow. I went with a 12' x 20' insulated metal inside and out building. I started out with DH and loading AND unloading by hand (LONG DAYS). At that time it only had double doors (6'w). After load/unload 3x......I modified and made triple 3' (9') doorway, added a track and carriage system...Added a 3'x9' knockout mechanical room for DH, fans and heat.

My circulation is set up different due to my carriage hieght (ex-farmwagon frame), the initial air flows longways under the lumber and then up through the lumber and escapes out the sides. This lets my have and use FULL advantage of my heat never having hot and cool spots (heat always rises). I have insulated panels that I place around the carriage that creates a plenum (air balancer in hvac systems) forcing balanced air up through lumber. This is a little slower for my drying due to I cut wider boards than usual and creates fewer slots...but most of mine are live edge flitches leaving larger single gaps.

Here's a few pics, enjoy and maybe it will be helpful. Have a Blessed day.

10/1/14       #8: Drying kiln using a reefer body and ...
Jason S Member

I have a Nyle L 200 in a 22 ft cold plate body with a trifold rear door and a track system for loading. The "kiln cart" is made from an old school bus frame. The whole system works awesome and I am very satisfied. When setting pitch in pine at 170 degrees, I have climbed on the roof and felt for warm spots. The whole outer surface is cool to the touch. Amazing insulation in a cold plate body. The whole thing holds 2000 bd ft and that is a prefect match to the L 200 in soft woods.
I don't check here often so if you have questions please email me.
Jason

10/2/14       #9: Drying kiln using a reefer body and ...
Mike Born

We had Nyle build a kiln just like this a year ago. It has 9 fans in it lengthwise and 2 DH compressors. We don't dry much from green lumber down to 8% but a lot of reconditioning of wood just before use. We had 2 drop down plenums also put in to be able to direct air flow. It works so well that we normally just use the heat from the fans for additional drying, but have also heat treated lumber up to 165 F for insects. Highly recommend it, and we have 5 other Nyle custom units that we use.

10/3/14       #10: Drying kiln using a reefer body and ...
Sherwood Member

If you are going to do this, you can put a big dent in your operating costs by orienting the box east-west, and building a solar preheater box on the south side.

This can be as simple as a layer of tarpaper, firring strips, and a layer of clear plastic, with the air pulled from a plenum (gaps in the firring) at the top.

Bunches of clever solar ideas.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)