Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

drying spalted pine mantle

12/7/18       
Bryan "doc" Henderson  Member

I had not milled in awhile, and had a friend who wanted some junk wood for his fireplace. Meaning not nice mulberry or oak for a wood stove that could actually put out some heat. I still had the upper half of a pine tree, the lower half of which is now 2x4 lumber. I was cutting and saw spaltting, and the wood was solid despite sitting for a year. I put a chunck on the mill and made a massive mantle, left live edge on a surface. 10 x 14 inches by 7 feet long. I have a container with a dehumidifier, and a shop that is heated all winter. I know soft wood is supposed to dry fast but this is a thick beam. I could heat it in a small container in my shop and let the extra heat migrate into the shop. Any hobby home made ideas to help dry this mantle. It is big enough I can re-saw surfaces if needed for warp or twist. also big enough I do not want to move it more than needed. Just wanted to get a new sawing and drying thread going for the holidays. What do you think! Pic to follow. Thanks

12/7/18       #2: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

the wood


View higher quality, full size image (4032 X 3024)

12/7/18       #3: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

the log that was destined for firewood.


View higher quality, full size image (1280 X 960)

12/15/18       #4: drying spalted pine mantle ...
Gene Wengert-WoodDoc

That is going to,look awesome when done. The only concern is insects, so heating it up to 133 F for a day would be prudent.

Drying needs to be done somewhat slowly...if 8/4 can safely dry in 10 days, then 16/4 requires 25 days and 8” around 70 days.

Figure than if this chunk of wood weighs 150 pounds, it could contain 75 pounds of water when fresh, but probably has lost a few pounds while waiting to be sawn. So, a pint of water is around one pound, so you have about 48 pounds of water to come out or 6 gallons. Will this moisture affect your shop by increasing the humidity?

12/21/18       #5: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

Gene, thanks for the response. My shop has radiant floor heat and it is topped off with a wood stove. the shop is currently 74 degrees F and 30% humidity. The boiler is set at 58 degrees as backup for when I am not home to stoke the stove with wood. The shop is 4500 sq. feet so I do not think that this chunk will overall effect the rel. humidity and therefore other wood in the shop much. It is now outside under a tarp at night. For fun, I will try to get a weight. I am sure it is more than 150#. I have a finished bit of this wood from the lower trunk of the tree finished and it is neat. I'll try to add a picture.

12/21/18       #6: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

Here are pictures of the wood with several coats of a spar varnish, but otherwise the natural color of the wood. Same tree, but the trunk that I processed more expediently.


View higher quality, full size image (2048 X 1536)


View higher quality, full size image (1536 X 2048)

12/22/18       #7: drying spalted pine mantle ...
Gene Wengert-WoodDoc

From a technical point of view, the fungi you have in the picture is the common blue stain (or sap stain) fungus. These fungi are not the fungi associated with spalting ...white rot and brown rot.

Blue stain fungi, as well as mold and mildew fungi, are not spalting fungi, as their hyphae do not colonize the wood internally and they do not produce the enzymes necessary to digest the wood cell wall components.

12/22/18       #8: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

Very Interesting. I assumed any color change after a period on the ground and from fungi would be generically called spalting. I like the look, and these will be outdoor BSA camp out benches. Thanks for the info. Merry Christmas! I will look forward to any further info or reference you wish to provide. Please let me know if you speaking anywhere in the area.

12/25/18       #9: drying spalted pine mantle ...
Gene Wengert-WoodDoc

I am giving a Talk here in Athens, GA in March...about understanding your DNA results from Ancestry.com. Nothing on drying scheduled, but in May in central GA WE MAY HAVE AN ADVANCED 1-DAY CLASS ON DH, hopefully with YellowHammer...still planning.

12/27/18       #10: drying spalted pine mantle ...
Bryan "doc" Henderson  Member

Thanks. Maybe post the essentials here for ancestry. Keep me in the loop, I will check in after this spring. may just have to come to your town and get tutored. Hope to hear back after the holidays from our forester. Thanks again. For this mantle and given the weather, I may try to make the one from clear plastic at some point. Like info put out by Timbergreen farms. Any thoughts?

  • Post a Response to this thread
  • notify me of responses to this topic
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Rose Machinery
      Horizontal Band Re-rips, Standard & Custom Designed Machinery
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • Baker Products
      Industrial Woodworking Machines, Wooden Pallet Manufacturing Machines, & Portable Sawmills

    Become a Sponsor today!