Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Advice on Planer Purchase

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Advice on Planer Purchase

12/30/22       
Jon Member

I am looking to upgrade from my old 18" Rockwell 22-201 wedge planer.
We are a currently a 6 person shop with more cabinetry work than we can handle. I currently outsource my drawer box material and my standard 2.25" door stiles and rails material to a local mill shop which eliminates a 90% of the need for a thickness planer. However, I would be open to processing that material in house in the future.
The delta had been upgraded to a Bryde helical head but after the first rotation of the blades we have never been able to eliminate streaking from the inserts not being perfectly aligned. This experience scarred me and has me wanting to go with the Tersa head vs. the "Xylent" (from SCM)
I am leaning toward the SCM Nova s 520 and the runner up is the Ironwood p500.
1. What are your thoughts on the two machines as they are relatively the same price.
https://www.youtube.com/watch?v=gaWpcIcIzsI
https://amldata.stilesmachinery.com/assets/files/2hy/98-965-00227.pdf
2. Tersa vs Xylent. My number one concern being insert alignment.

12/30/22       #2: Advice on Planer Purchase ...
Bill Stanisci

I assume you don't have a wide belt or you would not care as much about "insert alignment". Most insert heads have insert with a slight radius so material coming out of it needs to be sanded anyway.

If you have more work than you can handle making drawer box material and door stiles would be a false economy. Both are made more efficiently on a molder.

Inserts as you know are quiet and a straight knife is not. You also will get significantly more tear out from a straight knife. I am a fan of inserts.

12/31/22       #3: Advice on Planer Purchase ...
Allen Chalifoux

If your getting a streaking on the surface that you weren't getting before rotating the knives it's because there not seated properly.
We've been using Byrd heads for close to 20 years in both my molder and planer and will tell you that the knife seat has to be absolutely clean when installing the inserts.
Bill is correct about the mill marks sanding out with normal surface sanding.
If your looking for a machine to increase productivity I suggest you think about a 4 side molder, no other machine in my shop has has had as big of an impact on productively and opened up new markets. Allen

12/31/22       #4: Advice on Planer Purchase ...
Pete

I went from a 20" powermatic(high end hobby) with straight knives to a used scm 520 with a tersa head. I love the tersa head. No experience with inserts.

12/31/22       #5: Advice on Planer Purchase ...
Bruce H

If you have a Bryde helical head in your current planer, that is pretty much at the top of the food chain. A new planer isn't going to help you as much as learning to tune the planer you have. Those pockets need to be absolutely clean when you install the knife. One at a time, clean the pocket with a tooth brush, oil the screw before installing it. We do one row before the torque sequence and then move on to the next row. I have a 24" planer with six rows of cutters, takes about one day to change the head. For that, I get one and half to two years before needing to turn.

12/31/22       #6: Advice on Planer Purchase ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I'm a fan of Tersa heads. Super easy to change knives.

Neither Tersa or Inserts allow big cuts. Hogging material, get a Northfield.
Different knife options for Tersa

I can tell you to skip Felder. I hate mine. I wish I would've bought a used Kolle or Panhans. If only going new, Martin or a L'invincibile.

12/31/22       #7: Advice on Planer Purchase ...
Jason

The carbide inserts that are on a new head 15x15 or 14X14 are always perfect but as soon as you rotate them you will get the lines. Clean as clean can be and I have never been able to get it back to a no line finish so I only use them on the first bottom. Seems to do really good there.

1/3/23       #8: Advice on Planer Purchase ...
Jon Member

I do have a very old Timesaver wide belt sander...that is a problem for another thread. It doesn't run like I wish it would and, in all honesty, it would maybe make more sense to upgrade my sander. However, that is a significantly larger purchase.

@ Bill - You're not wrong on the false economy.

The inserts were just changed a couple weeks ago. We tooth brushed each "seat" and each insert as clean as possible, still have the lines. Do they need torqued all exactly the same with a torque screwdriver?

1/3/23       #9: Advice on Planer Purchase ...
gary

Maybe look into a planer/sander. Kill two birds with one stone. The sander will remove all planer marks and you can raise it out of the way when rough planning only plus you have conveyor feed.

1/3/23       #10: Advice on Planer Purchase ...
Hen Bob Member

I would also recommend just upgrading your sander, yes more of an investment but will save you labor in the long run. How are you sanding your doors now? But if you do go the planer route heed Karl's advice ... I just watched a nice panhans sell for 4.5K

1/3/23       #11: Advice on Planer Purchase ...
Jon

I will definitely keep panhans in mind.
All cabinet doors are sanded individually with a palm sander.
The joints are usually very close to perfectly flush off the shapers so it doesnt take “too” long. It would be nice to be able to simply run them through our widebelt though.
Any sander recommendations?

1/5/23       #12: Advice on Planer Purchase ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I have an Apex and have been happy with it.

I agree with others. A better widebelt would be money well spent.

1/7/23       #13: Advice on Planer Purchase ...
Dave Edgerton  Member

In all honesty if you are doing that kind of work get a 4 head planer. We did and we should have done it sooner. We bought ours used and have it on a 4 year lease.

1/9/23       #14: Advice on Planer Purchase ...
David R Sochar Member

Website: http://www.acornwoodworks.com

I agree with Dave E. - Get a four head planer with digital readouts, process (control) all your material needs and you will not regret it.

We had a Weinig Quattromax that was fast, accurate and worked like a charm. Quick change knives could be done on the machine. Similar to Tersa. SCMI also made/makes o similar machine. A long infeed table will work like a jointer, so all the stock come out straight, unlike most molders.

1/17/23       #15: Advice on Planer Purchase ...
Allen Chalifoux

Jon, back to your original question.
I just finished rotating the inserts on my molder and remembered the 1st time I rotated them I broke a couple of knives. The problem was garbage on the underside of the knives. Since then I drop them in a bowl of lacquer thinner and clean them as well as the pockets in the head as well. Hope this helps, Allen

2/8/23       #16: Advice on Planer Purchase ...
Ian

On a side note, make sure there are enough rollers on the bed so you don't get that entry snipe. Our powermatic has two, not enough when their on either side of the cutterhead.

2/27/26       #17: Advice on Planer Purchase ...
sarahwilson1 Member

If your current volumes are still moderate and you’re outsourcing most of the thicknessing, I’d focus first on reliability and local service support.

Between the two, SCM generally has the edge in build quality and overall fit and finish, and it tends to hold value better long term. Ironwood is a solid, workhorse option, but a bit more utilitarian.

As for Tersa vs. Xylent: if your previous experience with a helical head left you frustrated due to streaking and insert alignment issues, Tersa will likely feel more straightforward and predictable — fast knife changes and minimal adjustment. Xylent runs quieter and can give excellent surface quality, especially on figured material, but it does require careful maintenance and clean insert seating.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!