Building a gang rip saw up-to 15 blades

12/5/19       
Prangige

We are an entry door and engineered flooring manufacturing company.

We are trying to build a gang rip saw for speeding up ripping of engineered panels.

Typical panel dimensions are 2-1/2" thick x 32" wide x 96" long and saw needs to cut material 2-1/2 deep".

Would like to check on a suitable blade for setting up a gang rip saw up-to 15 blades maximum.

I am thinking of using a 8 feet long 40mm stainless steel arbor with two keyways for this.

I am thinking of using 15 blades from Frued gang rip saw thin kerf (1.7mm) blade LM0814 model for this set up.

Motor is a 10hp motor.

Is 40mm stainless steel arbor with two keyways OK for this set up?

Thanks

12/5/19       #2: Building a gang rip saw up-to 15 bl ...
duster

I'm not a mechanical engineer, but a 10 hp motor seems vastly underpowered for 15 blades cutting 2.5" deep.

12/6/19       #3: Building a gang rip saw up-to 15 bl ...
BH Davis  Member

Website: http://www.bhdavis.net

I'm afraid I can see all kinds of problems here.

1) 10 hp as mentioned above is probably woefully inadequate. I good 10" table saw will have a 5 hp motor and even that is going to be pressed hard on a 2-1/2" single-pass cut.

2) 8' long arbor ?? It that really what you meant? I'd think at 8' long a 1-1/2" (40mm) shaft would have significant whiplash.....and that's without the blades cutting 2-1/2" thick material. I'm not a mechanical engineer either but I'd think you would need something more on the order of 3" to 4" diameter, and perhaps hollow (think pipe) as vs. a solid arbor due to the weight.

3) Stainless steel arbor......why? Extremely difficult to machine to needed specs vs. steel.

I'd like to know if you actually end up building this as described so I can make sure I'm not in the same state when it is started up for the first time....chuckle. In all seriousness though I think you need to have this designed by a professional. Or, better yet, purchase a machine made for the job.

Good luck,
BH Davis

12/6/19       #4: Building a gang rip saw up-to 15 bl ...
David R Sochar Member

Why stop at 8'? 24' would cut 3 times as much material. A few carrier bearings and you are good to go. Of course, you will need a hoist or small army to push those 24' wide panels thru the saw.

A typical Straight line Diehl or equal will have a 20hp motor, up to 30 hp. The gang rips like Merreen Johnson have 60 hp direct drive motors.

12/6/19       #5: Building a gang rip saw up-to 15 bl ...
Jared E

I would very much like to see this built. It sounds entertaining. Please post the youtube link, and be sure to update your will and life insurance policy.

Where's my popcorn?

12/6/19       #6: Building a gang rip saw up-to 15 bl ...
Dom

60+ hp. Minimum 3"dia. shaft with outer carrier bearing. Hydrolic feed. No chains. This is a dangerous machine to build if you dont know what youre building.

12/6/19       #7: Building a gang rip saw up-to 15 bl ...
Rob Young  Member

Website: nutekmachinery.com

I would recommend against trying to "design and build" your own. This is a job for a mechanical engineer. You put your life, your employees lives, and your entire business at risk. If OSHA walks into your plant and sees something that is obviously not engineered by experts, without all the proper safeties in place, you can expect heavy fines.

12/8/19       #8: Building a gang rip saw up-to 15 bl ...
rich c.

A 40mm x 8' arbor will sag under it's own weight. Let alone handle blades under that kind or load.

12/9/19       #9: Building a gang rip saw up-to 15 bl ...
Mark Elliott Member

A 12" Mereen Johnson has a 3 1/8" arbor w/ a 50hp direct drive motor.

A 24" MJ still has a 3 1/8" arbor but has an outboard bearing to support it.

I have seen a 60" MJ come up on the used market that was set up to rip particle board into strips.

12/9/19       #10: Building a gang rip saw up-to 15 bl ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Just here stop jump on the "this is a terrible idea" bandwagon.

12/11/19       #11: Building a gang rip saw up-to 15 bl ...
Steve

Paul makes a panel gang rip saw for this very purpose. They have models that will rip close to 3" thick.

They can be had used if you watch the auctions.

I don't think it is practical to make a machine like you are talking about. First off what happens when the material binds on the blades? What kind of kick back safety is that going to lead to? There is a lot more to think about other then just getting an arbor and put a motor to it. You are better off in the long run to just purchase one of these machines used. The machine will have some resale value later, the one you make won't. Not to mention what happens to you when someone at your place gets hurt.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)